Pressureless sintering and mechanical properties of mica glass–ceramic/Y-PSZ composite
Source abstract
Abstract
Abstract Mica glass–ceramic composites toughened by 5, 10 and 15 wt.% partially stabilized zirconia (Y-PSZ) were prepared via pressureless sintering. Sinterability of composites was investigated in the temperature range of 1060–1170 °C using soaking time of 240 min. The sintered specimens were characterized by scanning electron microscopy (SEM) and X-ray diffraction (XRD) methods. The results revealed that during sintering, the dissolution of Y-PSZ occurred in the residual glass which caused the formation of zircon and transformation of tetragonal to monoclinic zirconia. Mechanical properties of the sintered samples such as bending strength, Vickers micro-hardness and fracture toughness were also investigated. Measurements showed that addition of 15 wt.% ZrO 2 to the mica glass–ceramic matrix increased the bending strength from 50.91 ± 10.50 to 132.47 ± 13.80 MPa. Fracture toughness was also improved up to 1.37 ± 0.14 MPa m 1/2 .
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Nuclear materials and radiation effects · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (23)
Show source-provided references
1. Höland · 2002
2. Microstructures & mechanical properties of mica glass–ceramics
3. High-strength mica-containing glass–ceramics10.1111/j.1151-2916.1991.tb04314.x ↗
4. Hot-pressed mica glass–ceramics with high strength and toughness10.1111/j.1151-2916.1999.tb01977.x ↗
5. Enhanced mechanical properties of orientated mica glass–ceramics10.1016/S0167-577X(99)00033-6 ↗
6. Processing, microstructure and mechanical properties of extruded mica glass–ceramics10.1016/S0921-5093(00)01968-7 ↗
7. Microstructure of mica-based nanocomposite glass–ceramics10.1111/j.1151-2916.1993.tb03821.x ↗
8. Study on machinable glass–ceramic containing fluorophlogopite for dental CAD/CAM system10.1007/s10856-006-0540-9 ↗
9. The effect of B2O3, PbO and P2O5 on the sintering and machinability of fluoromica glass–ceramics10.1016/j.jeurceramsoc.2004.04.019 ↗
10. Influence of TiO2, Cr2O3 and ZrO2 on sintering and machinability of fluorophlogopite glass–ceramics10.1179/096797804X938 ↗
11. Khatib Zadeh, S., Samedani, M., Eftekhari Yekta, B. and Hashemi Nia, S., Effect of sintering and melt casting methods on properties of a machinable fluor-phlogopite glass–ceramic. J. Mater. Proc. Tech., in press.
12. Monoclinic-tetragonal transition of zirconia10.1111/j.1151-2916.1961.tb13732.x ↗
13. Transformation toughening in zirconia-containing ceramics10.1111/j.1151-2916.2000.tb01221.x ↗
14. Richerson · 1992
15. Phase analysis in zirconia system10.1111/j.1151-2916.1972.tb11290.x ↗
16. Phase transformation of zirconia by ball-milling10.1111/j.1151-2916.1979.tb19121.x ↗
17. Viscous sintering and mechanical properties of 3Y-TZP-reinforced LAS glass–ceramic composites10.1111/j.1151-2916.1997.tb03223.x ↗
18. Microstructure and properties of a composite system for dental applications composed of glass–ceramics in the SiO2–LiO2–ZrO2–P2O5 system and ZrO2-ceramic (TZP)10.1023/A:1004661911158 ↗
19. Microstructural design of zirconia-toughened ceramics (ZTC)
20. Viscous flow sintering of bioactive glass–ceramic composites toughened by zirconia particles10.1016/S0955-2219(02)00164-4 ↗
21. Optimisation of the synthesis of glass–ceramic matrix biocomposites by the “response surface methodology”10.1016/S0955-2219(02)00264-9 ↗
22. Sintering behavior of composite materials borosilicate glass–ZrO2 fibre composite materials10.1016/S0955-2219(01)00479-4 ↗
23. Sintering with rigid inclusions10.1111/j.1151-2916.1987.tb04870.x ↗