Hot corrosion and protection of Ti2AlC against Na2SO4 salt in air
Source abstract
Abstract
The hot corrosion behavior of Na2SO4-coated Ti2AlC was investigated by means of thermogravimetric analysis, X-ray diffraction, and scanning electron microscopy/energy dispersive spectroscopy. This carbide displays good hot corrosion resistance below the melting point of Na2SO4 while the corrosion attacks become virulent when the salt is molten. A protectively continuous Al2O3 layer forms and imparts good corrosion resistance, and consequently, the corrosion kinetics is generally parabolic at 850 degrees C. However, porous oxide scales fail to protect the Ti2AlC substrate at 900 and 1000 degrees C. The segregation of sulfur at the corrosion scale/substrate interface accelerates the corrosion of Ti2AlC. Furthermore, a convenient and efficient pre-oxidation method is proposed to improve the high-temperature hot corrosion resistance of Ti2AlC. An Al2O3 scale formed during pre-oxidation treatment can remarkably restrain the infiltration of the molten salt into the substrate and prevent the substrate from severe corrosion attacks. (c) 2005 Elsevier Ltd. All rights reserved.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: MXene and MAX Phase Materials · Advanced materials and composites · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (25)
Show source-provided references
1. Kohlenstoffhaltige ternare verbindungen (H-phase)10.1007/BF00913068 ↗
2. Electronic structure and bonding properties of layered machinable Ti2AlC and Ti2AlN ceramic10.1103/PhysRevB.61.12570 ↗
3. Summary of constitutional data on the aluminium–carbon–titanium system10.1007/BF02647559 ↗
4. Solid–liquid reaction synthesis and simultaneous densification of polycrystalline Ti2AlC10.3139/146.020066 ↗
5. Synthesis of ternary titanium aluminum carbides using self-propagating high-temperature synthesis technique10.1111/j.1151-2916.2001.tb01138.x ↗
6. Processing and characterization of Ti2AlC, Ti2AlN and TiAlC0.5N0.510.1007/s11661-006-0243-3 ↗
7. Deformation of polycrystalline Ti2AlC under compression10.1007/s100190100132 ↗
8. High-temperature oxidation of Ti2AlC in air10.1023/A:1023092027697 ↗
9. Dependence of elastic stiffness on electronic band structure of nanolaminate M2AlC (M=Ti, V, Nb, and Cr) ceramics10.1103/PhysRevB.69.214111 ↗
10. Deposition of Ti2AlC and Ti3AlC2 epitaxial films by magnetron sputtering10.1063/1.1780597 ↗
11. Raman active phonon modes and heat capacities of Ti2AlC and Cr2AlC ceramics: first-principles and experimental investigations10.1063/1.1873057 ↗
12. Vibrational behavior of the Mn+1AXn phases from first-order Raman scattering (M=Ti, V, Cr, A=Si, X=C, N)10.1103/PhysRevB.71.012103 ↗
13. Lin, Z. J., Zhuo, M. J., Zhou, Y. C., Li, M. S. and Wang, J. Y., Microstructural characterization of layered-ternary Ti2AlC. Acta Mater., 2006, 54, in press.10.1016/j.actamat.2005.10.028 ↗
14. Alloy design of intermetallics for protective scale formation and for use as precursors for complex ceramic phase surfaces10.1016/j.intermet.2004.02.019 ↗
15. The improvement of high-temperature oxidation of Ti–50Al by anodic coating in the phosphoric acid10.1016/S1359-6454(01)00390-1 ↗
16. Oxidation behavior of Ti3AlC2 at 1000–1400°C in air10.1016/S0010-938X(02)00177-4 ↗
17. Kofstad · 1988
18. Hot corrosion of Na2SO4-coated Ti3AlC2 in air at 700–1000°C10.1149/1.1778171 ↗
19. Studies on the interactions of transition metal oxides and sodium sulfate in the temperature range 900–1200K in oxygen10.1016/0925-8388(95)02125-6 ↗
20. Hot corrosion of alumina10.1557/JMR.1993.1964 ↗
21. Hot-corrosion behaviour of silica and silica-formers: external versus internal control10.1016/S0955-2219(98)00243-X ↗
22. Hot corrosion of sintered α-SiC at 1000°C10.1111/j.1151-2916.1985.tb10170.x ↗
23. Oxidation-resistant multilayer coatings using an anodic alumina layer as a diffusion barrier on γ-TiAl substrates10.1016/j.surfcoat.2004.08.211 ↗
24. Effect of pre-oxidation on the corrosion behavior of Fe–40Al sheet in a N2–11.2O2–7.5CO2–500ppm SO2 atmosphere at 1273K10.1016/S0966-9795(02)00192-9 ↗
25. High-temperature interactions of transition-metal carbides with Na2SO410.1016/0022-5088(91)90325-X ↗