Degradation mechanisms of a self-healing SiC(f)/BN(i)/[SiC-B4C](m) composite at high temperature under different oxidizing atmospheres
Source abstract
Abstract
Abstract Chemical vapor-infiltrated self-healing SiC(f)/BN(i)/[SiC-B4C](m) composite specimens were exposed at 1300 °C for 300 h at atmospheric pressure under two different oxidizing atmospheres (i.e., wet (12%H2O:8%O2:80%Ar) and dry (0.01%O2:99.99%Ar)) representative of rich and poor oxidizing conditions, respectively. Mechanical testing, microstructural observations, and element analyses were performed on the treated specimens. The flexural strength retentions of the specimens were 47.9 and 39.4% under wet and dry oxygen conditions, respectively. The SiC and B4C matrices were severely oxidized under wet oxygen conditions, whereas the BN interphase remained intact. The BN interphase and the B4C layered phase were both partially oxidized under dry oxygen conditions. Thus, the SiC(f)/BN(i)/[SiC-B4C](m) composites exhibited improved oxidation resistance under wet oxygen atmospheres as compared to dry oxygen conditions as a result of the formation of borosilicate glasses. In addition, two different degradation mechanisms for the composites during the oxidation process were discussed.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Concrete and Cement Materials Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (49)
Show source-provided references
1. Design, preparation and properties of non-oxide CMCs for application in engines and nuclear reactors: an overview10.1016/S0266-3538(03)00230-6 ↗
2. SiC-matrix composites: nonbrittle ceramics for thermo-structural application10.1111/j.1744-7402.2005.02009.x ↗
3. HSR/EPM combustor materials development program10.1016/S0921-5093(98)01079-X ↗
4. Ceramic matrix composite combustor liners: a summary of field evaluations10.1115/1.2181182 ↗
5. Performance benefit assessment of ceramic components in an MS9001FA gas turbine10.1115/1.1335476 ↗
6. Rebillat · 2010 · 151
7. Thermal expansion and oxidation of 3D C/SiC composites with different coatings from room temperature to 1400 °C10.1515/SECM.2002.10.5.377 ↗
8. Thermal expansion behavior of carbon fiber reinforced chemical-vapor-infiltrated silicon carbide composites from room temperature to 1400 °C10.1016/j.matlet.2006.02.088 ↗
9. Oxidation behavior of SiC fiber reinforced SiC10.1016/0022-3115(95)00133-6 ↗
10. Self-healing mechanisms of a SiC fiber reinforced multi-layered ceramic matrix composite in high pressure steam environments10.1016/j.jeurceramsoc.2006.06.007 ↗
11. Degradation mechanisms of a SiC fiber reinforced self-sealing matrix composite in simulated combustor environments10.1016/j.jeurceramsoc.2006.02.042 ↗
12. The mechanical behavior of ceramic matrix composites10.1016/0001-6160(89)90291-5 ↗
13. A multi-scale approach of degradation mechanisms inside a SiC(f)/Si–B–C(m) based self-healing matrix composite in a dry oxidizing environment10.1007/s11085-013-9385-z ↗
14. Oxidation behavior and protection of carbon/carbon composites10.1016/0008-6223(87)90197-7 ↗
15. High-temperature oxidation of boron nitride: I, monolithic boron nitride10.1111/j.1551-2916.1999.tb20075.x ↗
16. Chase · 1986
17. Formation and oxidation resistance of the coating formed on carbon material composed of B4C-SiC powders10.1016/0008-6223(94)00164-U ↗
18. Development of oxide scale microstructure on single-crystal SiC10.1007/BF02402838 ↗
19. High-temperature passive oxidation of chemically vapor deposited silicon carbide10.1111/j.1151-2916.1989.tb07658.x ↗
20. Corrosion of silicon-based ceramics in combustion environments10.1111/j.1151-2916.1993.tb03684.x ↗
21. Oxidation kinetics of chemically vapor-deposited silicon carbide in wet oxygen10.1111/j.1151-2916.1994.tb05357.x ↗
22. Degradation of silicon carbide in combustion gas flow at high-temperature and speed10.1299/jsmea.44.520 ↗
23. SiC recession caused by SiO2 scale volatility under combustion conditions: I, experimental results and empirical model10.1111/j.1151-2916.1999.tb02004.x ↗
24. SiC recession caused by SiO2 scale volatility under combustion conditions: II, thermodynamics and gaseous-diffusion model10.1111/j.1151-2916.1999.tb02005.x ↗
25. Oxidation of SiC fiber-reinforced SiC matrix composites with a BN interphase10.4028/www.scientific.net/MSF.696.342 ↗
26. Borosilicate glass-induced fiber degradation of SiC/BN/SiC composites exposed in combustion environments10.1111/ijac.12499 ↗
27. Oxidation mechanisms and kinetics of 1D-SiC/C/SiC composite materials: I, an experimental approach10.1111/j.1151-2916.1994.tb07015.x ↗
28. Oxidation-resistant carbon-fiber-reinforced ceramic-matrix composites10.1016/S0266-3538(98)00146-8 ↗
29. Relationship between oxidation resistance and structure of B4C–SiC/C composites with self-healing properties10.1016/S0008-6223(98)00184-5 ↗
30. New route for preparation of SiC-B4C/C composite with excellent oxidation resistance up to 1400 °C10.1023/A:1022210328332 ↗
31. Oxidation behavior of C/SiC composite with CVD SiC-B4C coating in a wet oxygen environment10.1007/s10443-008-9077-z ↗
32. Oxidation behavior of two-dimensional C/SiC modified with self-healing Si-B-C coating in static air10.1016/j.corsci.2012.08.003 ↗
33. Effect of temperature on stress oxidation behaviors of 2D C/SiC-BCx composite in wet oxygen atmosphere10.1007/s11661-014-2500-1 ↗
34. Oxidation behavior of SiBC matrix modified C/SiC composites with different PyC interphase thicknesses10.1016/j.ceramint.2014.09.111 ↗
35. Active-to-passive transition in the oxidation of silicon carbide and silicon nitride in air10.1111/j.1151-2916.1990.tb09793.x ↗
36. General relationship for the thermal oxidation of silicon10.1063/1.1713945 ↗
37. A pervasive mode of oxidative degradation in a SiC/SiC composite10.1111/j.1151-2916.1998.tb02696.x ↗
38. The ZrB2 volatility diagram10.1111/j.1551-2916.2005.00599.x ↗
39. Active oxidation of SiC10.1007/s11085-010-9216-4 ↗
40. Expression for effect of porosity on elastic modulus of polycrystalline refractory materials, particularly aluminum oxide10.1111/j.1151-2916.1961.tb11671.x ↗
41. High-temperature flexural properties of SiBC modified C/SiC composites10.1016/j.ceramint.2013.11.072 ↗
42. Properties of multilayered interphases in SiC/SiC chemical-vapor-infiltrated composites with “weak” and “strong” interfaces10.1111/j.1151-2916.1998.tb02627.x ↗
43. Interfacial bond strength in SiC/C/SiC composite materials, as studied by single-fiber push-out tests10.1111/j.1151-2916.1998.tb02434.x ↗
44. The concept of a strong interface applied to SiC/SiC composites with a BN interphase10.1016/S1359-6454(00)00247-0 ↗
45. Development of damage in a 2D woven C/SiC composite under mechanical loading: I. mechanical characterization10.1016/S0266-3538(96)00094-2 ↗
46. Effect of carbon and boron on the high-temperature oxidation of silicon carbide10.1111/j.1151-2916.1995.tb08918.x ↗
47. High temperature crack sealant based on SiO2-B2O3 for SiC coating on carbon/carbon composites10.1163/156855103772658498 ↗
48. Phase relations in the system boron oxide–silica10.1111/j.1151-2916.1965.tb11803.x ↗
49. Oxidation behavior of boron carbide powder10.1016/j.msea.2006.08.068 ↗