journal article·2020-11

Tensile creep properties and damage mechanisms of 2D-SiCf/SiC composites reinforced with low-oxygen high-carbon type SiC fiber

Xi Wang, Zhuolin Song, Zanlin Cheng, Dong Han, Mei Li, Chengyu Zhang

Publisher page

Abstract

Abstract Tensile creep properties of 2D-SiCf/SiC composites reinforced with low-oxygen high-carbon type SiC fibers were studied in vacuum at 1300°C∼1430°C. The fracture morphology was observed by scanning electron microscopy and the damage of fiber in 2D-SiCf/SiC composites was characterized by nanoindentation. Moreover, the microstructure of the composite was investigated by high-resolution transmission electron microscopy. The results show that rupture time is much shortened and steady-state creep rate increase three orders of magnitude when creep temperature is higher than 1400°C. There are two different creep damage mechanisms due to the decrease of interfacial bonding strength at high temperature. The amorphous SiOxCy phase in the fibers can crystallize into SiC and C and the SiC grain grows in the fiber. The microstructural changes lead to the decrease of fiber strength and degrade the creep properties of the composite above 1400°C.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (29)

Show source-provided references
1. Beyer · 2013
2. Sauder · 2015
3. TEM observations of SiC-SiC materials with a carbon interphase after tests at high temperature10.1051/mmm:019910020107500 ↗
4. Creep and fatigue behavior of SiC fiber reinforced SiC composite at high temperatures10.1016/S0921-5093(96)10872-8 ↗
5. Creep and fatigue behavior in an enhanced SiC/SiC composite at high temperature10.1111/j.1151-2916.1998.tb02621.x ↗
6. Tensile creep and creep fracture of a fibre-reinforced SiC/SiC composite10.1016/S1359-6462(98)00181-X ↗
7. Creep and fatigue behavior in Hi-Nicalon (TM)-fiber-reinforced silicon carbide composites at high temperatures10.1111/j.1151-2916.1999.tb01731.x ↗
8. The creep mechanism of ceramic matrix composites at low temperature and stress, by a material science approach10.1016/S0955-2219(02)00103-6 ↗
9. Creep behaviour of a SiC/Si-B-C composite with a self-healing multilayered matrix10.1016/S0955-2219(02)00273-X ↗
10. Fracture mechanisms for SiC fibers and SiC/SiC composites under stress-rupture conditions at high temperatures
11. DiCarlo · 2005 · 77
12. Creep and stress-strain behavior after creep for SiC fiber reinforced, melt-infiltrated SiC matrix composites10.1111/j.1551-2916.2006.00939.x ↗
13. Tensile creep and rupture of 2D-woven SiC/SiC composites for high temperature applications10.1016/j.jeurceramsoc.2010.01.030 ↗
14. Creep in vacuum of woven Sylramic-iBN melt-infiltrated composites10.1016/j.compscitech.2010.10.003 ↗
15. Tensile creep of melt-infiltrated SiC/SiC composites with unbalanced Sylramic-iBN fiber architectures10.1111/j.1744-7402.2010.02524.x ↗
16. Monotonic tension, fatigue and creep behavior of SiC-fiber-reinforced SiC-matrix composites: a review10.1016/S0266-3538(99)00014-7 ↗
17. Tensile creep behaviour of a silicon carbide-based fibre with a low oxygen content10.1007/BF00356326 ↗
18. Tensile creep behavior of SiC-Based Fibers with a low oxygen content10.1111/j.1551-2916.2007.01535.x ↗
19. In-plane mechanical behavior and failure mode of a 2D-SiC/SiC composite under uniaxial dynamic compression10.1016/j.ceramint.2018.07.280 ↗
20. The surface properties of low oxgyen high carbon type silicon carbide fiber
21. Creep properties of single crystal oxides evaluated by a Larson-Miller procedure10.1016/0955-2219(95)00017-O ↗
22. Fine diameter ceramic fibres10.1016/S0955-2219(00)00090-X ↗
23. Crack deflection process-I theory10.1016/0001-6160(83)90046-9 ↗
24. Effects of temperature of temperature on microstructure evolution and mechanical properties of Hi-Nicalon SiC fibers10.1002/jccs.200500039 ↗
25. A theoretical and experimental approach to the active-to-passive transition in the oxidation of silicon carbide10.1023/A:1004313022769 ↗
26. Oxidation behavior of Si-M-C-O fibers under wide range of oxygen partial pressures10.1023/A:1020608704120 ↗
27. Microstructural characterization and fracture properties of SiC-based fibers annealed at elevated temperatures10.1007/s10853-006-0579-5 ↗
28. Effect of heat treatment on the tensile strength and creep resistance of advanced SiC fibers10.1016/j.jnucmat.2004.04.123 ↗
29. Creep properties and damage mechanisms of 2D-SiCf/SiC composites prepared by CVI