Abstract

Abstract Process-tolerant SiC ceramics were prepared by pressureless sintering at 1850–1950 °C for 2 h in an argon atmosphere with a new quaternary additive (Al2O3-Y2O3-CaO-SrO). The SiC ceramics can be sintered to a > 94% theoretical density at 1800–1950 °C by pressureless sintering. Toughened microstructures consisting of relatively large platelet grains and small equiaxed grains were obtained when SiC ceramics were sintered at 1850–1950 °C. The presently fabricated SiC ceramics showed little variability of the microstructure and mechanical properties with sintering within the temperature range of 1850–1950 °C, demonstrating process-tolerant behavior. The thermal conductivity of the SiC ceramics increased with increasing sintering temperature from 1800 °C to 1900 °C due to decreases of the lattice oxygen content of the SiC grains and residual porosity. The flexural strength, fracture toughness, and thermal conductivity of the SiC ceramics sintered at 1850–1950 °C were in the ranges of 444–457 MPa, 4.9–5.0 MPa m1/2, and 76–82 Wm−1 K−1, respectively.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (53)

Show source-provided references
1. Development of a roadmap for advanced ceramics: 2010–202510.1016/j.jeurceramsoc.2008.10.015 ↗
2. Commercialization of advanced structural ceramics: Patience is a necessity
3. Reed · 1995 · 407
4. Fracture properties of SiC ceramics with oxynitride additives10.1016/S0955-2219(02)00132-2 ↗
5. Microstructural design of sliding-wear-resistant liquid-phase-sintered SiC: an overview10.1016/j.jeurceramsoc.2007.02.190 ↗
6. Effect of sintering conditions on microstructure in α-SiC prepared by slip casting in a strong magnetic field10.1016/j.jeurceramsoc.2010.04.022 ↗
7. Oxidation resistance of SiC ceramics prepared by different processing routes10.1016/j.jeurceramsoc.2016.03.016 ↗
8. Tribological behavior of silicon carbide ceramics-a review10.4191/kcers.2016.53.6.581 ↗
9. Process-tolerant manufacturing: an optimization strategy for improving manufacturing yields
10. Electrochemical corrosion of silicon carbide ceramics in H2SO410.1016/j.jeurceramsoc.2013.08.024 ↗
11. Additive-free hot-pressed silicon carbide ceramics-a material with exceptional mechanical properties10.1016/j.jeurceramsoc.2015.12.013 ↗
12. High-temperature strength of a thermally conductive silicon carbide ceramic sintered with yttria and scandia10.1016/j.jeurceramsoc.2016.02.028 ↗
13. Pressureless sintered silicon carbide with enhanced mechanical properties obtained by the two-step sintering method10.1016/j.ceramint.2013.07.075 ↗
14. The effect of in situ synthesized AlN on densification of SiC ceramics by pressureless sintering10.1016/j.ceramint.2015.07.040 ↗
15. Effect of liquid phase sintering on microstructure and mechanical properties of Yb2O3-AlN containing SiC-based ceramics10.1111/j.1551-2916.2005.00212.x ↗
16. Properties of liquid phase pressureless sintered silicon carbide obtained without sintering bed10.1016/j.jeurceramsoc.2004.05.014 ↗
17. The effect of rare earth oxides on the pressureless liquid phase sintering of α-SiC10.1016/j.jeurceramsoc.2014.03.029 ↗
18. Microstructure and mechanical properties of silicon carbide pressureless sintered with oxide additives10.1016/j.jeurceramsoc.2006.04.009 ↗
19. In situ toughening of pressureless liquid phase sintered α-SiC by using TiO210.1016/j.ceramint.2014.03.055 ↗
20. Effect of additive composition on mechanical properties of pressureless sintered silicon carbide ceramics sintered with alumina, aluminum nitride and yttria10.1007/s12540-015-4383-0 ↗
21. Mechanical and thermal properties of pressureless sintered silicon carbide ceramics with alumina-yttria-calcia10.1111/jace.14114 ↗
22. Thermal, electrical, and mechanical properties of pressureless sintered silicon carbide ceramics with yttria-scandia-aluminum nitride10.1016/j.jeurceramsoc.2016.04.014 ↗
23. Microstructural development of silicon carbide containing large seed grains10.1111/j.1151-2916.1997.tb02796.x ↗
24. Microstructural development of liquid-phase-sintered silicon carbide during annealing with uniaxial pressure10.1016/S0955-2219(01)00408-3 ↗
25. Relationship between microstructure and fracture toughness of toughened silicon carbide ceramics10.1111/j.1151-2916.2001.tb00840.x ↗
26. Grain growth during gas-pressure sintering of β-silicon nitride10.1111/j.1151-2916.1990.tb07610.x ↗
27. Standard test method for flexural strength of advanced ceramics at ambient temperature
28. Standard test methods for determination of fracture toughness of advanced ceramics at ambient temperature
29. Microstructure and thermal conductivity of silicon carbide with yttria and scandia10.1111/jace.12737 ↗
30. Thermochemical analysis of the silicon carbide-alumina reaction with reference to liquid-phase sintering of silicon carbide10.1111/j.1151-2916.1991.tb06885.x ↗
31. Effect of annealing treatments on microstructure and mechanical properties of liquid-phase-sintered silicon carbide10.1016/S0955-2219(00)00254-5 ↗
32. Microstructural evolution in liquid-phase-sintered SiC: part I effect of starting powder10.1111/j.1151-2916.2001.tb00880.x ↗
33. Effect of initial α-phase content on microstructure and mechanical properties of sintered silicon carbide10.1111/j.1151-2916.1998.tb02748.x ↗
34. Keppeler · J. Eur. Ceram. Soc. · 1998 · 18 · 52110.1016/S0955-2219(97)00163-5 ↗
35. Ye · Acta Mater. · 1999 · 47 · 48110.1016/S1359-6454(98)00371-1 ↗
36. Core/rim structure of liquid-phase-sintered silicon carbide10.1111/j.1151-2916.1993.tb03677.x ↗
37. Effect of grain growth on electrical properties of silicon carbide ceramics sintered with gadolinia and yttria10.1016/j.jeurceramsoc.2015.08.006 ↗
38. Process-tolerant SiC-TiC composites10.1023/A:1015722612151 ↗
39. Microstructural evolution during sintering with control of the interface structure10.1111/j.1551-2916.2009.03106.x ↗
40. Solid-state conversion of single crystals: the principle and the state-of-the-art10.1111/jace.13420 ↗
41. Effect of microstructure and grain boundary chemistry on slow crack growth in silicon carbide at ambient conditions10.1016/j.jeurceramsoc.2015.02.020 ↗
42. Heat-resistant silicon carbide with aluminum nitride and scandium oxide10.1016/j.actamat.2005.07.002 ↗
43. Solid-state pressureless sintering of silicon carbide below 2000°C10.1016/j.jeurceramsoc.2014.06.006 ↗
44. Properties of silicon carbide ceramics from gelcasting and pressureless sintering10.1016/j.matdes.2014.08.034 ↗
45. Preparation of pressureless-sintered SiC-Y2O3-Al2O310.1007/BF00540522 ↗
46. Flexural strength and toughness of liquid phase sintered silicon carbide10.1016/S0272-8842(99)00084-X ↗
47. Effect of grain growth on the thermal conductivity of liquid-phase sintered silicon carbide ceramics10.1016/j.jeurceramsoc.2017.04.050 ↗
48. Effects of Y2O3-RE2O3 (RE=Sm, Gd Lu) additives on electrical and thermal properties of silicon carbide ceramics10.1111/jace.13958 ↗
49. Electrical and thermal properties of SiC-AlN ceramics without sintering additives10.1016/j.jeurceramsoc.2015.04.010 ↗
50. Effects of rare-earth oxide and alumina additives on thermal conductivity of liquid-phase-sintered silicon carbide10.1557/JMR.2003.0259 ↗
51. Electrical and thermal conductivity of liquid phase sintered SiC10.1016/S0955-2219(01)00178-9 ↗
52. Thermal conductivity of liquid phase sintered silicon carbide10.1016/S0955-2219(02)00271-6 ↗
53. The effects of nanoparticle addition on the densification and properties of SiC10.1016/j.ceramint.2012.03.049 ↗