journal article·2019-08

Design and optimization of the coating thickness on chopped carbon fibers and sintering temperature for ZrB2-SiC-Cf composites prepared by hot pressing

Cheng Fang, Ping Hu, Shun Dong, Ping Xie, Kaiyang Wang, Xinghong Zhang

Publisher page

Abstract

Abstract Interface designation and low-temperature densifying were expected to inhibit the performance attenuation of fiber in the preparation of ceramic matrix composites. Nevertheless, the optimization of interface thickness and sintering temperature were still rarely investigated systematically. Herein, the performance of carbon fiber varied with coating thickness and the heat-treat temperatures were investigated by quantitatively. The tensile strength of carbon fibers degraded dramatically (≥30%) when coating thickness above a critical value. A larger dimension and ordered graphite crystallite structure resulted in the severe performance deterioration of carbon fibers as the sintering temperature exceeding 1500 ℃. The PyC coatings with an appropriate thickness acted as a critical role of changing the fracture mode of the ZrB2-SiC-Cf and noticeably increased the fracture strain of the composite. The regular trend provided a general design strategy in construction of ZrB2-SiC-Cf composite with optimal properties and could be extended to other ceramic matrix composites.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · MXene and MAX Phase Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (41)

Show source-provided references
1. Arc-jet wind tunnel characterization of ultra-high-temperature ceramic matrix composites10.1016/j.corsci.2018.12.039 ↗
2. Preparation and characterization of high-performance ZrB2-SiC-Cf composites sintered at 1450 ° C10.1007/s40145-017-0223-7 ↗
3. Effect of graphite flake on microstructure as well as mechanical properties and thermal shock resistance of ZrB2-SiC matrix ultrahigh temperature ceramics10.1016/j.jallcom.2009.04.109 ↗
4. Beneficial effects of an ultra-fine α-SiC incorporation on the sinterability and mechanical properties of ZrB210.1007/s00339-005-3327-9 ↗
5. Toughened ZrB2-based ceramics through SiC whisker or SiC chopped fiber additions10.1016/j.jeurceramsoc.2009.11.012 ↗
6. Processing, sintering and oxidation behavior of SiC fibers reinforced ZrB2 composites10.1016/j.jeurceramsoc.2011.10.032 ↗
7. Design, preparation and properties of carbon fiber reinforced ultra-high temperature ceramic composites for aerospace applications: a review10.1016/j.jmst.2016.08.004 ↗
8. Introduction to H2020 project C3HARME–next generation ceramic composites for combustion harsh environment and space10.1080/17436753.2018.1509822 ↗
9. Krenkel · 2008
10. Surface temperature jump beyond active oxidation of carbon/silicon carbide composites in extreme aerothermal conditions10.1016/j.carbon.2014.01.018 ↗
11. Unified tensile model for unidirectional ceramic matrix composites with degraded fibers and interface10.1016/j.jeurceramsoc.2018.09.006 ↗
12. Relationships between carbon fiber type and interfacial domain in ZrB2-based ceramics10.1016/j.jeurceramsoc.2015.09.026 ↗
13. Rapid spark plasma sintering to produce dense UHTCs reinforced with undamaged carbon fibres10.1016/j.matdes.2017.05.029 ↗
14. A novel vibration-assisted slurry impregnation to fabricate Cf/ZrB2-SiC composite with enhanced mechanical properties10.1016/j.jeurceramsoc.2018.10.029 ↗
15. Additive manufacturing of ceramics enabled by flash pyrolysis of polymer precursors with nanoscale layers10.1111/jace.13946 ↗
16. Tough salami-inspired Cf/ZrB2 UHTCMCs produced by electrophoretic deposition10.1016/j.jeurceramsoc.2017.09.047 ↗
17. Influence of fiber coating thickness on microstructure and mechanical properties of carbon fiber-reinforced zirconium diboride based composites10.1016/j.ceramint.2013.07.040 ↗
18. High-performance ZrB2-SiC-Cf composite prepared by low-temperature hot pressing using nanosized ZrB2 powder10.1016/j.jeurceramsoc.2017.02.008 ↗
19. Toughening effect of non-periodic fiber distribution on crack propagation energy of UHTC composites10.1016/j.jallcom.2018.11.043 ↗
20. On the thermal shock resistance and mechanical properties of novel unidirectional UHTCMCs for extreme environments10.1038/s41598-018-27328-x ↗
21. Oxidation behaviour of a continuous carbon fibre reinforced ZrB2–SiC composite10.1016/j.corsci.2017.04.012 ↗
22. Effect of pyrolytic carbon coating on the microstructure and fracture behavior of the Cf/ZrB2-SiC composite10.1016/j.ceramint.2018.07.210 ↗
23. Evaluation of the effect of PyC coating thickness on the mechanical properties of T700 carbon fiber tows10.1016/j.apsusc.2018.08.195 ↗
24. The study on low temperature sintering of nano-tungsten powders10.1016/j.ijrmhm.2016.10.003 ↗
25. Coating of carbon fibers-the strength of the fibers10.1111/j.1151-2916.1995.tb08372.x ↗
26. Interpretation of infrared and Raman spectra of amorphous carbon nitrides10.1103/PhysRevB.67.155306 ↗
27. Interpretation of Raman spectra of disordered and amorphous carbon10.1103/PhysRevB.61.14095 ↗
28. Tensile strength of fiber-reinforced composites: III. Beyond the traditional Weibull model for fiber strengths10.1177/002199830003401503 ↗
29. The effect of thermal exposure on the strength distribution of B4C coated carbon fibers10.1016/S0008-6223(98)00197-3 ↗
30. The influence of graphitization on the mechanical properties of carbon fibers10.1007/BF01584920 ↗
31. Kinetic studies on hot-stretching of polyacrylonitrile-based carbon fibres by using internal resistance heating part II changes in structure and mechanical properties10.1023/A:1004664611696 ↗
32. Gradient distribution of radial structure of PAN-based carbon fiber treated by high temperature10.1016/j.pnsc.2014.01.009 ↗
33. Effect of microstructure on the modulus of PAN-based carbon fibers during high temperature treatment and hot stretching graphitization10.1007/s10853-006-0519-4 ↗
34. Effect of carbon fiber crystallite size on the formation of hafnium carbide coating and the mechanism of the reaction of hafnium with carbon fibers10.1016/j.carbon.2017.01.059 ↗
35. Elastic moduli of nanocrystallites in carbon fibers measured by in-situ X-ray microbeam diffraction10.1016/S0008-6223(02)00359-7 ↗
36. A comparison of the effect of graphitization on microstructures and properties of polyacrylonitrile and mesophase pitch-based carbon fibers10.1016/j.carbon.2012.05.024 ↗
37. The fracture mechanics of finite crack extension10.1016/j.engfracmech.2004.07.001 ↗
38. Microstructure, mechanical properties and thermal shock resistance of ZrB2-SiC-Cf composite with inhibited degradation of carbon fibers10.1016/j.jallcom.2017.02.227 ↗
39. Preparation and characterization of high-performance ZrB2-SiC-Cf composites sintered at 1450 ℃10.1007/s40145-017-0223-7 ↗
40. High-performance ZrB2-SiC-Cf composite prepared by low-temperature hot pressing using nanosized ZrB2 powder10.1016/j.jeurceramsoc.2017.02.008 ↗
41. An integrated composite with a porous Cf/C-ZrB2-SiC core between two compact outer layers of Cf/C-ZrB2-SiC and Cf/C-SiC10.1016/j.jeurceramsoc.2014.10.005 ↗