journal article·2021-02

Long-term oxidation behavior of C/SiC-SiBCN composites in wet oxygen environment

Xin’gang Luan, Xinming Xu, Lei Wang, Yun Zou, Ralf Riedel, Laifei Cheng

Publisher page

Abstract

Abstract Polymer derived SiBCN ceramic was introduced into carbon fiber reinforced SiC composites to prepare C/SiC-SiBCN composites. Weight change and flexural strength of the samples after oxidation at different temperatures and in different atmospheres were tested up to 100 h to investigate their wet oxidation behavior. It was found that the stable silicoboron glassy self-healing phase formed from the oxidation of SiBCN had favorable oxidation resistance in wet oxygen atmosphere. And the SiC-SiBCN matrix can provide about 50 h of protection for carbon fiber in wet oxygen. Besides, the influence of temperature on the oxidation behavior of C/SiC-SiBCN composites were much related to the release speed of gas products (B2O3, HBO2 and Si(OH)4). And the oxidation mechanism of SiC/SiC-SiBCN composites were further explained by the comparation with C/SiC-SiBCN composites.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Concrete and Cement Materials Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (29)

Show source-provided references
1. Design, preparation and properties of carbon fiber reinforced ultra-high temperature ceramic composites for aerospace applications: a review10.1016/j.jmst.2016.08.004 ↗
2. Advanced structural ceramics in aerospace propulsion10.1038/nmat4687 ↗
3. High-temperature properties and interface evolution of C/SiBCN composites prepared by precursor infiltration and pyrolysis
4. Carbon fibre reinforced silicon carbide composites (C/SiC, C/C-SiC)
5. An approach to the mechanical behaviour of SiC/SiC and C/SiC ceramic matrix composites10.1007/BF02403938 ↗
6. SiC-matrix composites: nonbrittle ceramics for thermo-structural application10.1111/j.1744-7402.2005.02009.x ↗
7. A review of the application of C/SiC composite in thermal protection system10.1163/157361109787959903 ↗
8. Phenomena encountered by the thermal protection materials during Hermes reentry
9. The application study status of spacecraft structural materials10.4028/www.scientific.net/AMR.904.126 ↗
10. Oxidation behavior of 3D C/SiC composites in two oxidizing environments10.1016/S0266-3538(00)00190-1 ↗
11. Paralinear oxidation of CVD SiC in water vapor10.1111/j.1151-2916.1997.tb02810.x ↗
12. Variation of the oxidation rate of silicon carbide with water‐vapor pressure10.1111/j.1151-2916.1999.tb01810.x ↗
13. Oxidation of carbon fiber-reinforced silicon carbide matrix composites at reduced oxygen partial pressures10.1111/j.1551-2916.2010.04376.x ↗
14. SiC recession caused by SiO2 scale volatility under combustion conditions. Part 2; thermodynamics and gaseous-diffusion model10.1111/j.1151-2916.1999.tb02005.x ↗
15. Measurement and simulation of the oxidation of carbon fibers and C/SiC ceramic10.4028/www.scientific.net/AST.45.1489 ↗
16. Oxidation-resistant carbon-fiber-reinforced ceramic-matrix composites10.1016/S0266-3538(98)00146-8 ↗
17. Oxidation behavior of SiBC matrix modified C/SiC composites with different PyC interphase thicknesses10.1016/j.ceramint.2014.09.111 ↗
18. Effect of SiC particle size on anti-oxidation behavior of C/B4C/SiC composite10.4028/www.scientific.net/MSF.658.308 ↗
19. Boron-bearing species in ceramic matrix composites for long-term aerospace applications10.1016/j.jssc.2003.03.005 ↗
20. Microstructure and thermal shock behavior of sol-gel introduced ZrB2 reinforced SiBCN matrix10.1007/s10971-018-4648-4 ↗
21. In-situ preparation and mechanical property analysis of SiC/SiBCN(O) nanocomposites10.1016/j.ceramint.2020.03.291 ↗
22. Precursor-derived Si-B-C-N ceramics: oxidation kinetics10.1111/j.1151-2916.2001.tb00985.x ↗
23. Characterization of oxidized polymer-derived SiBCN fibers10.1111/j.1151-2916.2001.tb00987.x ↗
24. Oxidation behavior of C/SiC-SiBCN composites at high temperature10.1016/j.jeurceramsoc.2019.04.025 ↗
25. Wet oxidation behavior of SiC/SiC-SiBCN composites prepared by CVI combined with PIOP process10.1111/jace.16497 ↗
26. Polyborosilazane‐derived high temperature resistant SiBCNO10.1002/adem.201801295 ↗
27. Oxidation behavior of 3D-C/SiC composites fabricated by PIP process at low temperatures10.2991/icmse-18.2018.41 ↗
28. Effect of oxidation treatment on the mechanical properties of C/SiBCN composites10.1016/j.ceramint.2019.07.269 ↗
29. Oxidation behavior and protection of carbon/carbon composites10.1016/0008-6223(87)90197-7 ↗