Preparation and hydrothermal corrosion behavior of Cf/SiCN and Cf/SiHfBCN ceramic matrix composites

Jia Yuan, Xingang Luan, Ralf Riedel, Emanuel Ionescu

Publisher page

Abstract

Cf/SiCN and Cf/SiHfBCN-based ceramic matrix composites (CMC) were fabricated using the precursor infiltration and pyrolysis technique (PIP). Their behavior in subcritical hydrothermal conditions was investigated at 150–250 °C using exposition times of 48, 96 and 240 h and shown to rely on active corrosion. The data of the mass loss as a function of the corrosion time and temperature at S/V of 0.075 were used to rationalize the corrosion kinetics of the CMCs. Both materials have been shown to exhibit excellent stability in subcritical hydrothermal conditions. The corrosion rates of Cf/SiHfBCN were lower than those determined for Cf/SiCN; furthermore, SEM investigation indicates that spallation occurred in the Cf/SiCN samples; whereas the ceramic matrix was still attached on the individual carbon fibers in Cf/SiHfBCN. The results indicate that the incorporation of Hf and B into SiCN matrix leads to a significant improvement of its hydrothermal corrosion performance.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Concrete and Cement Materials Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (36)

Show source-provided references
1. Krenkel · 2008
2. Theory of mechanical properties of ceramic–matrix composites10.1111/j.1151-2916.1991.tb06852.x ↗
3. Carbon fiber reinforced CMC for high-performance structures10.1111/j.1744-7402.2004.tb00169.x ↗
4. The CVI-processing of ceramic matrix composites10.1051/jphyscol:1989526 ↗
5. Design, preparation and properties of non-oxide CMCs for application in engines and nuclear reactors: an overview10.1016/S0266-3538(03)00230-6 ↗
6. Carbon fibre-reinforced CMCs by PCS infiltration10.1023/A:1017990709819 ↗
7. Fiber-reinforced composites with polymer-derived matrix: processing, matrix formation and properties10.1016/S1359-835X(98)00128-6 ↗
8. Processing and properties of C/SiBCN fiber–reinforced ceramic matrix composites prepared by precursor impregnation and pyrolysis10.1016/j.actamat.2007.12.001 ↗
9. Oxidation and corrosion of ceramics and ceramic matrix composites10.1016/S1359-0286(01)00009-2 ↗
10. Kinetics and mechanisms of oxidation of 2D woven C/SiC composites: I, experimental approach10.1111/j.1151-2916.1994.tb07096.x ↗
11. Kinetics and mechanisms of oxidation of 2D woven C/SiC composites: II, theoretical approach10.1111/j.1151-2916.1994.tb07097.x ↗
12. Accelerated oxidation of SiC CMC's by water vapor and protection via environmental barrier coating approach10.1016/S0955-2219(02)00141-3 ↗
13. Current status of environmental barrier coatings for Si-based ceramics
14. Polymer-derived yttrium silicate coatings on 2D C/SiC composites10.1016/j.jeurceramsoc.2012.08.032 ↗
15. Corrosion of a SiC-C/PyC/SiC composite by sodium sulfate vapor at high temperatures10.1515/SECM.2002.10.2.157 ↗
16. Corrosion of a 3D-C/SiC composite in salt vapor environments10.1016/S0008-6223(01)00203-2 ↗
17. Effects of water vapor on corrosion behaviors of c/sic in oxidizing atmosphere containing Na2SO4 vapor10.1016/j.compositesb.2012.05.047 ↗
18. Low-temperature oxidation, hydrothermal corrosion, and their effects on properties of sic (tyranno) fibers10.1111/j.1151-2916.1995.tb08835.x ↗
19. Hydrothermal degradation of chemical vapour deposited SiC fibres10.1023/A:1004480814477 ↗
20. Ceramic and metal matrix composites: routes and properties10.1016/j.jmatprotec.2005.04.038 ↗
21. Single-source-precursor synthesis of hafnium-containing ultrahigh-temperature ceramic nanocomposites (UHTC-NCs)10.1021/ic501512p ↗
22. Active-filler-controlled pyrolysis of preceramic polymers10.1111/j.1151-2916.1995.tb08404.x ↗
23. Pressureless fabrication of dense monolithic SiC ceramics from a polycarbosilane10.1016/j.jeurceramsoc.2014.05.002 ↗
24. The design of the fibre-matrix interfacial zone in ceramic matrix composites10.1016/S1359-835X(97)00128-0 ↗
25. Hydrothermal corrosion of pure, hot isostatically pressed silicon nitride10.1111/j.1151-2916.1993.tb03768.x ↗
26. Corrosion of silicon nitride ceramics under hydrothermal conditions10.1007/BF00543597 ↗
27. Corrosion of silicon nitride materials in acidic and basic solutions and under hydrothermal conditions10.1016/S0955-2219(02)00303-5 ↗
28. Corrosion of silicon nitride in sulphuric acid aqueous solution10.1016/S0010-938X(00)00193-1 ↗
29. Corrosion of silicon nitride materials in aqueous solutions10.1111/jace.12509 ↗
30. Hydrothermal corrosion of nitride and carbide of silicon10.1016/S0254-0584(00)00434-X ↗
31. Corrosion behavior of silicon oxycarbide-based ceramic nanocomposites under hydrothermal conditions10.3139/146.110625 ↗
32. Oxidation/corrosion of polymer-derived SiAlCN ceramics in water vapor10.1111/j.1551-2916.2005.00791.x ↗
33. Approaches to standardisation: high temperature oxidation and hydrothermal corrosion of silica forming ceramics10.4028/www.scientific.net/KEM.113.15 ↗
34. Corrosion behavior of silicon carbide in 290°C water10.1111/j.1151-2916.1989.tb06029.x ↗
35. Diffusion of water into silica glass at low temperature10.1111/j.1151-2916.1989.tb05990.x ↗
36. Hydroxo and chloro complexes/ion interactions of Hf4+ and the solubility product of HfO2(am)10.1023/A:1013337925441 ↗