Influence of structural parameters and transition interface on the fracture property of Al 2 O 3 /Mo laminated composites
Source abstract
Abstract
Abstract This paper proposes a set of new structural parameters to quantify the fracture behavior of Al 2 O 3 /Mo laminated composites. The relationships between the relevant structural parameters and mechanical properties of the materials were analyzed. Results show that the variation of structural parameters causes significant changes in the effective proportion of Mo phase and the contribution to the crack propagation energy of the materials, thus realizing the optimization of the materials. Based on these analyses, we formulated a set of principles and theoretical models to design Al 2 O 3 /Mo laminated composites. Furthermore, the performance of the Al 2 O 3 /Mo laminated composites can be improved further by introducing a transition interface with appropriate Mo content. We demonstrated that the toughness and work of fracture of Al 2 O 3 /Mo laminated composites could reach 7.3 MPa m 1/2 and 8757 J m −2 , respectively.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Metal and Thin Film Mechanics · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (37)
Show source-provided references
1. Lubrication behavior of Y-TZP/Al2O3/Mo nanocomposites at high temperature10.1016/j.wear.2010.01.009 ↗
2. Design and preparation of high-performance alumina functional graded self-lubricated ceramic composites
3. Design and fabrication of laminated-graded zirconia self-lubricating composites10.1016/j.matdes.2013.01.040 ↗
4. High-performance ceramic lubricating materials
5. High-temperature self-lubricated properties of Al2O3/Mo laminated composites10.1016/j.wear.2012.01.010 ↗
6. Influence of structural parameters on the tribological properties of Al2O3/Mo laminated nanocomposites10.1016/j.wear.2014.09.003 ↗
7. R-curve behaviour in weak interface-toughened SiC–C laminates by discrete element modelling10.1016/j.jeurceramsoc.2013.08.021 ↗
8. Control of composition and structure in laminated silicon nitride/boron nitride composites10.1111/j.1151-2916.2002.tb00480.x ↗
9. Fracture of metal/ceramic laminates-II crack growth resistance and toughness10.1016/S1359-6454(98)00358-9 ↗
10. A novel method to make tough Ti2AlC/Al2O3- and Ti3AlC2/Al2O3-laminated composites10.1111/j.1551-2916.2010.03989.x ↗
11. Biomimetic structure design-a possible approach to change the brittleness of ceramics in nature10.1016/S0928-4931(00)00133-8 ↗
12. The mechanical and dielectric properties of Si3N4-based sandwich ceramics10.1016/j.matdes.2011.09.019 ↗
13. Control of strength and toughness of ceramic/metal laminates using interface design10.1557/JMR.1993.2362 ↗
14. Toughening by metallic lamina in nickel/alumina composites10.1111/j.1151-2916.1993.tb03750.x ↗
15. A simple way to make tough ceramics10.1038/347455a0 ↗
16. Huang · 2008
17. Preparation of alumina/W laminated composites
18. The influence of plasticity on mixed mode interface toughness10.1016/0022-5096(93)90057-M ↗
19. The fracture toughness of Ni/Al2O3 laminates by digital image correlation I: Experimental crack opening displacement and R-curves10.1016/j.engfracmech.2005.09.005 ↗
20. Mechanics and mechanisms of crack growth at or near ceramic–metal interfaces: interface engineering strategies for promoting toughness10.1016/0921-5093(93)90325-9 ↗
21. Toughness of an interface along a thin ductile layer joining elastic solids10.1080/01418619408242253 ↗
22. Metal thickness effect on the calibration of stress intensity factors for Si3N4/Fe and Al2O3/Au joints10.1016/S0013-7944(98)00012-5 ↗
23. Influence of ceramic–metal interface adhesion on crack growth resistance of ZrO2–Nb ceramic matrix composites10.1016/j.actamat.2008.03.021 ↗
24. Mechanics and mechanisms of crack growth at or near ceramic–metal interfaces: interface engineering strategies for promoting toughness10.1016/0921-5093(93)90325-9 ↗
25. A numerical analysis of failure characteristics of ductile layers in laminated composites10.1023/A:1004644728764 ↗
26. Improving the mechanical properties of Al2O3/Ni laminated composites by adding Ni particles in the layers10.1016/j.msea.2006.09.055 ↗
27. Preparation and properties optimization of Al2O3/Al2O3–ZrO2 (3Y) laminated nanocomposites
28. Toughening of layered ceramic composites with residual surface compression: effects of layer thickness10.1016/S0013-7944(00)00096-5 ↗
29. Effects of dislocation shielding on interface crack initiation and growth in metal/ceramic layered materials10.1016/S0022-5096(99)00015-0 ↗
30. On crack extension in ductile/brittle laminates10.1016/0956-7151(91)90032-V ↗
31. Multilayer Al2O3/SiC ceramics with improved mechanical behavior10.1016/S0955-2219(00)00048-0 ↗
32. Damage resistance and R-curve behavior of multilayer Al2O3/SiC ceramics10.1016/S0272-8842(00)00020-1 ↗
33. The fabrication and failure of laminar ceramic composites10.1016/0956-7151(92)90471-P ↗
34. Fracture behavior of multilayer silicon nitride/boron nitride ceramics10.1111/j.1151-2916.1996.tb08996.x ↗
35. Crack deflection and propagation in layered silicon/boron nitride ceramics10.1111/j.1151-2916.1998.tb02438.x ↗
36. High toughness silicon carbide/graphite laminar composite by slip casting10.1016/0167-8442(95)00027-C ↗
37. Laminar ceramic copmposities10.1016/0955-2219(95)93055-8 ↗