Contact damage of silicon carbide ceramics with different grain structures measured by Hertzian and Vickers indentation
Source abstract
Abstract
We have used Hertzian and Vickers indentation to investigate contact damage in sintered SiC ceramics, one consisting of uniform, fine-grains and the other a coarse, elongated grain structure. Cracking-resistance measured by Hertzian indentation, showed no discernible difference, nor did the Vickers hardness. However, numerical analysis of the Vickers indentation size effect, performed using the proportional specimen resistance model, indicates 77.3% greater surface energy, mostly realised through cracking, is experienced by heterogeneous SiC per unit area of indentation impression. This is typified by an observable increase in the number of radial cracks generated around Vickers impressions, which has been found to artificially increase the KIC determined by Vickers indentation fracture. Quantitative measurements of pre-existing flaws by Hertzian indentation show that heterogeneous SiC retains a higher density of larger flaws. Relationships between the differences in cracking around Vickers indents and the pre-existing flaw populations of these two SiC ceramics are discussed.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Metal and Thin Film Mechanics · MXene and MAX Phase Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (27)
Show source-provided references
1. Effect of α-SiC versus β-SiC starting powders on the microstructure and fracture toughness of SiC sintered with Al2O3–Y2O3 additives10.1111/j.1151-2916.1994.tb09771.x ↗
2. In situ-toughened silicon carbide10.1111/j.1151-2916.1994.tb07024.x ↗
3. Grain growth and fracture toughness of fine-grained silicon carbide ceramics10.1111/j.1151-2916.1995.tb09100.x ↗
4. Pressureless sintering of SiC
5. Liquid phase sintered silicon carbide
6. The effect of indentation-induced cracking on the apparent microhardness10.1007/BF00352908 ↗
7. Cracking and the indentation size effect for Knoop hardness of glasses10.1111/j.1151-2916.2003.tb03319.x ↗
8. The indentation load/size effect and the measurement of the hardness of vitreous silica10.1016/S0022-3093(05)80492-2 ↗
9. Hardness-grain-size relations in ceramics10.1111/j.1151-2916.1994.tb04641.x ↗
10. Statistical determination of surface flaw distributions in brittle materials10.1016/0955-2219(95)00005-F ↗
11. Silicon carbide-based ceramics for ballistic protection
12. Influence of the α/β-SiC phase transformation on microstructural development and mechanical properties of liquid phase sintered silicon carbide10.1023/A:1004552704872 ↗
13. Fracture toughness testing for advanced technical ceramics: internationally agreed good practice
14. On the Vickers indentation fracture toughness test10.1111/j.1551-2916.2006.01482.x ↗
15. Determining the fracture toughness of brittle materials by Hertzian indentation10.1016/0955-2219(95)93941-U ↗
16. Untersuchungen über Harteprufung und Harte
17. Swain · 1996 · 379
18. Indentation brittleness of ceramics: a fresh approach10.1023/A:1018671823059 ↗
19. A critical evaluation of indentation techniques for measuring fracture toughness. I. Direct crack measurements10.1111/j.1151-2916.1981.tb10320.x ↗
20. Crack-growth resistance-curve behavior in silicon carbide small versus long cracks10.1111/j.1151-2916.1997.tb03115.x ↗
21. Toughness properties of a silicon carbide with an in situ induced heterogeneous grain structure10.1111/j.1151-2916.1994.tb04637.x ↗
22. High-toughness silicon carbide as armor10.1111/j.1551-2916.2005.00415.x ↗
23. Mechanical properties of β-SiC pressureless sintered with Al2O3 additions10.1016/0956-7151(94)90072-8 ↗
24. Characterization of surface damage via contact probes10.1088/0957-4484/7/3/019 ↗
25. Determination of surface residual stresses in brittle materials by Hertzian indentation: theory and experiment10.1111/j.1151-2916.1999.tb02003.x ↗
26. A model for crack initiation in elastic/plastic indentation fields10.1007/BF00552240 ↗
27. Depths of cracks produced by abrasion of brittle materials10.1016/S1359-6462(98)00403-5 ↗