Corrosion of the crystalline phases of matte glazes in aqueous solutions
Source abstract
Abstract
Chemical durability was determined for fast and conventionally fired matte raw glazes in acidic to alkaline aqueous solutions. According to XRD, the main crystalline phases in the glazes were diopside, plagioclase, anorthite, wollastonite, and pseudowollastonite. SEM-EDXA and whitelight confocal microscopy were used to analyze the surfaces after immersion in the aqueous solutions. The ionic concentrations in selected solutions after immersion were determined by ICP-AES. Diopside was not attacked by the test solutions. Plagioclase started to corrode along the crystal interfaces in the most acidic environments. Wollastonite crystals with different crystal habitus and slightly different chemical composition formed depending on firing cycle and composition of the glaze. In fast firing, tiny columnar wollastonite crystals were formed. These crystals were attacked in acidic to slightly alkaline environments. In conventionally fired glazes the wollastonite crystals were dendritic. These crystals were attacked only by acidic solutions. Pseudowollastonite with poor chemical resistance formed only in magnesia-free glazes.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Pigment Synthesis and Properties · Recycling and utilization of industrial and municipal waste in materials production · Cultural Heritage Materials Analysis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (15)
Show source-provided references
1. Corrosion of glazes and enamels
2. Kingery · 1976
3. Preparation and properties of CaO–MgO–Al2O3–SiO2 glass–ceramics from kaolin clay refining waste (kira) and dolomite10.1016/j.ceramint.2003.11.005 ↗
4. Glass–ceramics prepared from sludge generated by a water purification plant10.1016/j.ceramint.2005.11.009 ↗
5. Effect of additional materials on the properties of glass–ceramic produced from increnator fly ashes10.1016/j.chemosphere.2004.02.009 ↗
6. Durability of mat glazes in hydrochloric acid solution10.4028/www.scientific.net/KEM.264-268.1565 ↗
7. Chemical resistance of fast-fired raw glazes in solutions containing cleaning agents, acids or bases
8. Chemical resistance and cleanability of glazed surfaces10.1016/j.susc.2004.11.048 ↗
9. Plasma-sprayed glass–ceramic coatings on ceramic tiles: microstructure, chemical resistance and mechanical properties10.1016/j.jeurceramsoc.2004.06.018 ↗
10. Thermal and chemical properties of diopside–wollastonite glass–ceramics in the SiO2–CaO–MgO system from raw materials10.1016/S0272-8842(02)00114-1 ↗
11. Theory of corrosion of glass and ceramics
12. Corrosion of glazes coated with functional films in detergent solutions10.4028/www.scientific.net/AST.45.156 ↗
13. Chemical durability of glazed surfaces10.1016/j.jeurceramsoc.2006.04.162 ↗
14. Surface composition and topography of fast-fired raw glazes
15. Influence of firing parameters on phase composition of raw glazes10.1016/j.jeurceramsoc.2006.05.012 ↗