journal article·2015-03

Fast synthesis of B4C–TiB2 composite powders by pulsed electric current heating TiC–B mixture

Dewen Wang, Songlin Ran, Lu Shen, Huifeng Sun, Qing Huang

Publisher page

Abstract

Abstract Synthesis of B4C–TiB2 composite powders via a carbide boronizing process was performed in a pulsed electric current sintering furnace with a specially designed graphite die/punch set-up. Pure B4C–TiB2 powders could be obtained at 1200 °C for 0 min or 1000 °C for 15 min with a total thermal cycle time of only 12–25 min. In the as-prepared B4C–TiB2 composite powders, submicrometer B4C particles were surrounded by nano-TiB2 particles with an average particle of less than 50 nm. The bulk B4C–TiB2 ceramic sintered from the as-prepared composite powders had a relative density of 96% with ultrafine microstructures.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Boron and Carbon Nanomaterials Research · Advanced materials and composites · Advanced ceramic materials synthesis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (20)

Show source-provided references
1. Boron carbide – a comprehensive review10.1016/0955-2219(90)90048-K ↗
2. Spark plasma sintering of B4C ceramics: the effects of milling medium and TiB2 addition10.1016/j.ijrmhm.2011.07.016 ↗
3. Low pressure hot pressing of B4C matrix ceramic composites improved by Al2O3 and tic additives10.1016/j.msea.2009.06.016 ↗
4. Effect of Al addition on pressureless sintering of B4C10.1016/j.ceramint.2008.03.003 ↗
5. Wear resistance of silicon infiltrated B4C/BN composites10.1016/j.matlet.2008.08.037 ↗
6. Microstructure and mechanical properties of hot-pressed B4C/TiC/Mo ceramic composites10.1016/j.ceramint.2008.02.014 ↗
7. Effect of fiber type on mechanical properties of short carbon fiber reinforced B4C composites10.1016/j.ceramint.2008.07.023 ↗
8. Microcracking in B4C–TiB2 composites10.1111/j.1151-2916.1995.tb08671.x ↗
9. In situ synthesis and densification of submicrometer-grained B4C–TiB2 composites by pulsed electric current sintering10.1016/j.jeurceramsoc.2010.10.028 ↗
10. Microstructure and mechanical properties of pulsed electric current sintered B4C–TiB2 composites10.1016/j.msea.2010.10.022 ↗
11. Electrical discharge machining of B4C–TiB2 composites10.1016/j.jeurceramsoc.2011.04.024 ↗
12. Synthesis and properties of hot pressed B4C–TiB2 ceramic composite10.1016/j.msea.2010.07.101 ↗
13. Synthesis and sinterability of composite powder of the B4C–TiB2 system10.1016/0925-8388(93)90063-S ↗
14. Synthesis of pure YB4 powder via the reaction of Y2O3 with B4C10.1111/j.1551-2916.2012.05272.x ↗
15. Ultra-low temperature synthesis of Al4SiC4 powder using spark plasma sintering10.1016/j.scriptamat.2013.02.042 ↗
16. Synthesis of ultrafine hafnium diboride powders using solution-based processing and spark plasma sintering10.1111/ijac.12016 ↗
17. Spark plasma sintering of superhard B4C–ZrB2 ceramics by carbide boronizing10.1111/jace.12284 ↗
18. Synthesis of B4C–TiB2 composite powders by carbide boronizing process10.1016/j.ceramint.2014.06.103 ↗
19. Hexagonal BN-encapsulated ZrB2 particle by nitride boronizing10.1016/j.actamat.2014.03.054 ↗
20. TiB2 powders synthesis by borothermal reduction in TiO2 under vacuum10.1111/jace.12908 ↗