Effect of ZnO level in secondary copper smelting slags on slag/magnesia-chromite refractory interactions
Source abstract
Abstract
Abstract To determine the effect of ZnO in ZnO-containing fayalite (ZFS) slags on the degradation of magnesia-chromite refractories, the corrosion behaviour of a direct-bonded magnesia-chromite refractory was studied by rotating refractory finger tests at 1200 °C under reducing atmosphere. In addition, MgO crucible tests at these conditions were performed to investigate in particular the effect of ZnO on the slag/MgO interaction. The dissolution of MgO from periclase into the ZFS slags is not enhanced by increasing the ZnO content in the slags. (Fe,Mg,Zn)2SiO4 olivine and (Fe,Mg,Zn)O solid solution are the only two products in the slag/MgO interfacial reactions, even when the ZnO content in the ZFS slag reaches 16.7 wt%. The diffusion of ZnO into the chromite grains to form the (Fe,Mg,Zn)(Fe,Al,Cr)2O4 spinel was favoured with increasing the ZnO content in ZFS slags.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metallurgical Processes and Thermodynamics · Metal Extraction and Bioleaching · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (14)
Show source-provided references
1. Degradation mechanisms and use of refractory linings in copper production processes: a critical review10.1016/j.jeurceramsoc.2013.10.005 ↗
2. The influence of ZnO in fayalite slag on the degradation of magnesia-chromite refractories during secondary Cu smelting10.1016/j.jeurceramsoc.2015.03.013 ↗
3. Modeling the viscosity of silicate melts containing zinc oxide10.1016/j.calphad.2011.09.005 ↗
4. Viscosity and electrical-conductivity of Na2O–SiO2–ZnO and CaO–SiO2–ZnO10.2320/jinstmet1952.46.3_280 ↗
5. Petkov V., Degradation mechanisms of copper anode furnace refractory linings, KU Leuven—Faculteit Ingenieurswetenschappen—Dept., MTM, 2007, PhD thesis.
6. Influence of FeO/SiO2 ratio of ZnO-rich fayalite slags on the degradation of magnesia-chromite refractories under reducing atmosphere
7. The system MgO–ZnO–SiO210.1111/j.1151-2916.1965.tb14778.x ↗
8. Experimental study of phase equilibria in the systems Fe-Zn-O and Fe-Zn-Si-O at metallic iron saturation10.1007/s11663-000-0006-2 ↗
9. Fukuyama · 1996 · 109
10. Wetting behavior between fayalite-type slags and solid magnesia10.1111/j.1151-2916.1997.tb03112.x ↗
11. Influence of MgO precursors on mechanically activated forsterite synthesis10.1016/j.ceramint.2015.06.096 ↗
12. Low temperature synthesis of forsterite from hydromagnesite and fumed silica mixture10.1016/j.ceramint.2014.10.025 ↗
13. Effect of MgO on liquidus temperatures in the ZnO–FeO–Al2O3–CaO–SiO2–MgO system in equilibrium with metallic iron10.1007/s11663-011-9498-1 ↗
14. FactSage thermochemical software and databases—recent developments10.1016/j.calphad.2008.09.009 ↗