Formation and leachability of hexavalent chromium in the Al 2 O 3 -CaO-MgO-Cr 2 O 3 system
Source abstract
Abstract
Abstract The Al2O3-CaO-MgO-Cr2O3 system has immense potential for refractory castables applications. However, Cr(III) can potentially be oxidized to carcinogenic Cr(VI) during the usage, which can cause subsequent problems with disposal. Equilibrium experiments on the Al2O3-CaO-MgO-4wt%Cr2O3 system were performed at 1500 °C in air. The effect of MgO addition (0 and 20 wt%) on the formation and leachability of hexavalent chromium was investigated using XPS, XRD, SEM-EDS, the TRGS 613 standard Cr(VI) leaching test and multiple leaching tests. A Cr(VI)-containing phase Ca4Al6CrO16 predominantly formed in the samples with 0 and 5 wt% MgO, while the Cr(III)-containing Mg(Al, Cr)2O4 spinel phase formed in the samples with 10 and 20 wt% MgO. Addition of MgO suppressed the formation of Cr(VI) while favored the formation of spinel phase. Concentrations of Cr(VI) in the leachates from TRGS 613 tests exceeded the European limit of 0.0002 wt% in all samples, although decreased significantly with 20 wt% MgO addition.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metallurgical Processes and Thermodynamics · Advanced ceramic materials synthesis · Bauxite Residue and Utilization
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (37)
Show source-provided references
1. Hot corrosion behaviour of Al2O3–Cr2O3 refractory by molten glass at 1200 °C under static condition10.1016/j.corsci.2015.10.004 ↗
2. Thermo-mechanical behaviour and microstructure of Al2O3–Cr2O3 refractories: effect of TiO210.1016/j.ceramint.2014.10.155 ↗
3. Chromium speciation in coal and biomass co-combustion products10.1021/es103361g ↗
4. Thermogravimetric studies of high temperature reactions between potassium salts and chromium10.1016/j.corsci.2012.02.013 ↗
5. Development of a new cleaner production process for producing chromic oxide from chromite ore10.1016/j.jclepro.2004.09.001 ↗
6. Cr(VI)/Cr(III) and As(V)/As(III) ratio assessments in Jordanian spent oil shale produced by aerobic combustion and anaerobic pyrolysis10.1021/es200695e ↗
7. Chromium behaviour during thermal treatment of MSW fly ash10.1016/S0304-3894(01)00328-4 ↗
8. Mechanisms of chromium toxicity, carcinogenicity and allergenicity: review of the literature from 1985 to 200010.1191/096032701682693062 ↗
9. Leachability and fractionation of heavy metals in stainless steel plant dust
10. Multi-element pollution in soil, ground and surface water from abandoned chromate chemical plants: a case study in Hangzhou10.1007/s12665-015-4310-1 ↗
11. Fishbein · 1987 · 295
12. Cockerham · 1994 · 121
13. Corrosion behaviour of chromium-free ceramics for liquid slag removal in pressurized pulverized coal combustion10.1016/j.jeurceramsoc.2009.03.019 ↗
14. New development of spinel bonded chrome-free basic brick10.5897/JCEMS12.030 ↗
15. Fundamental study on the formation mechanism of hexavalent chromium compounds from refractories including chromium trioxide for waste melting furnace
16. Corrosion of glass contact refractories for the vitrification of radioactive wastes: a review10.1179/1743280410Y.0000000005 ↗
17. Matte – tap-hole clay – refractory brick interaction in a PGM smelter
18. Luz · 2015
19. Equilibrium phase relations in the Al2O3-CaO-Cr2O3 system in air
20. Formation, leachability and encapsulation of hexavalent chromium in the Al2O3–CaO–Fe2O3–Cr2O3 system10.1016/j.jeurceramsoc.2015.12.036 ↗
21. Effect of FeO on the formation of spinel phase and chromium distribution in the CaO-SiO2-MgO-Al2O3-Cr2O3 system10.1007/s12613-013-0720-9 ↗
22. Immobilization of chromium in slags using MgO and Al2O310.1002/srin.200806135 ↗
23. Effect of low oxygen partial pressure on the chromium partition in CaO–MgO–SiO2–Cr2O3–Al2O3 synthetic slag at elevated temperatures10.1002/srin.201200214 ↗
24. New spinel-containing refractory cements10.1016/S0955-2219(02)00166-8 ↗
25. Improved spinel-containing refractory castables for slagging gasifiers10.1016/j.jeurceramsoc.2012.11.011 ↗
26. Refractory aluminous cements
27. Aluminous cements containing magnesium aluminate spinel from Egyptian dolomite10.1016/S0272-8842(01)00042-6 ↗
28. 2002
29. FactSage Software (FactSage 7.0), Thermfact Ltd and GTT-technologies, Montreal, Canada, Aachen, Germany.
30. Chinese EPA, Solid Waste-Extraction Procedure for Leaching Toxicity-Sulphur Acid & Nitric Acid Method, HJ/T 299-2007.
31. Oxidation of metals at the chromium oxide interface10.1063/1.1506942 ↗
32. 1989
33. 1992
34. 2003
35. Release dynamic process identification for a cement based material in various leaching conditions. Part II. modelling the release dynamics for different leaching conditions10.1016/j.jenvman.2004.06.015 ↗
36. Leaching test conditions for Cr(VI) in cement, fly ash and cement solidified fly ash and their influencing factors
37. Solubility of chromate hydrocalumite (3CaO.Al2O3.CaCrO4.nH2O) 5-75 °C10.1016/S0008-8846(01)00507-5 ↗