Effect of CuO on self-lubricating properties of ZrO2(Y2O3)–Mo composites at high temperatures
Source abstract
Abstract
Abstract In this paper, ZrO2 matrix high-temperature self-lubricating composites with addition of CuO as lubricant were prepared using a hot-pressing method by tailoring the content of CuO. The wear and friction behaviour of the composites were investigated from 700 °C to 1000 °C. The composites sliding against an Al2O3 ceramic ball exhibited excellent self-lubricating and anti-wear properties at high temperatures. The low friction and wear mechanisms were investigated in detail.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced materials and composites · Advanced ceramic materials synthesis · Tribology and Wear Analysis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (35)
Show source-provided references
1. Low-pressure plasma-sprayed ZrO2–CaF2 composite coating for high temperature tribological applications10.1016/S0257-8972(00)00918-X ↗
2. Wear of plasma-sprayed nanostructured zirconia coatings against stainless steel under distilled-water conditions10.1016/S0257-8972(03)00311-6 ↗
3. Friction and wear of Al2O3, ZrO2 and SiO2 rubbed against pure metals10.1016/0043-1648(92)90176-9 ↗
4. Influence of porosity on friction and wear of tetragonal zirconia polycrystal10.1111/j.1151-2916.1997.tb02841.x ↗
5. Unlubricated friction and wear behavior of low-pressure plasma-sprayed ZrO2 coating at elevated temperatures10.1016/S0272-8842(00)00072-9 ↗
6. Microstructure and tribological characteristics of ZrO2–Y2O3 ceramic coatings deposited by laser-assisted plasma hybrid spraying10.1016/S0301-679X(02)00005-1 ↗
7. Microstructure–toughness–wear relationship of tetragonal zirconia ceramics10.1016/S0955-2219(03)00355-8 ↗
8. The synergistic effects of CaF2 and Au lubricants on tribological properties of spark-plasma-sintered ZrO2(Y2O3) matrix composites10.1016/S0921-5093(04)00965-7 ↗
9. Tribological properties of ZrO2(Y2O3)–Mo–BaF2/CaF2 composites at high temperatures10.1016/j.triboint.2011.09.008 ↗
10. Microstructure–mechanical–tribological property correlation of multistage spark plasma sintered tetragonal ZrO210.1016/j.jeurceramsoc.2010.08.005 ↗
11. Friction reduction by adding copper oxide into alumina and zirconia ceramics10.1016/S0043-1648(03)00267-9 ↗
12. Friction behaviour of solid oxide lubricants as second phase in α-Al2O3 and stabilised ZrO2 composites10.1016/S0043-1648(03)00388-0 ↗
13. Dry sliding wear of zirconia-toughened alumina with different metal oxide additives10.1016/j.ceramint.2008.04.006 ↗
14. High-temperature tribological behavior of ZrO2–MoS2–CaF2 self-lubricating composites10.1016/j.jeurceramsoc.2012.08.003 ↗
15. Superplasticity in 3Y-TZP doped with small amounts of copper oxide10.1016/0956-716X(94)90476-6 ↗
16. Environmental degradation of CuO-doped Y-TZP ceramics10.1016/S0272-8842(01)00024-4 ↗
17. Environmental effects on friction and wear of dry sliding zirconia and alumina ceramics doped with copper oxide10.1016/j.ijrmhm.2005.05.001 ↗
18. Synthesis, sintering and microstructure of 3Y-TZP/CuO nano-powder composites10.1016/j.jeurceramsoc.2005.07.017 ↗
19. Sintering behavior of 0.8mol%-CuO-doped 3Y-TZP ceramics10.1111/j.1551-2916.2005.00679.x ↗
20. Effect of microstructure on the tribological and mechanical properties of CuO-doped 3Y-TZP ceramics10.1111/j.1551-2916.2007.01823.x ↗
21. Dry-sliding self-lubricating ceramics: CuO doped 3Y-TZP10.1016/j.wear.2009.06.033 ↗
22. Analysis of reactions during sintering of CuO-doped 3Y-TZP nano-powder composites10.1016/j.jeurceramsoc.2009.02.009 ↗
23. Manipulating microstructure and mechanical properties of CuO doped 3Y-TZP nano-ceramics using spark-plasma sintering10.1016/j.jeurceramsoc.2009.10.002 ↗
24. Synthesis and characteristics of nanocrystalline 3Y-TZP and CuO powders for ceramic composites10.1016/j.ceramint.2009.08.001 ↗
25. High-temperature tribological and self-lubricating behavior of copper oxide-doped Y-TZP composite sliding against alumina10.1111/j.1551-2916.2011.04899.x ↗
26. The effect of an alumina counterface on friction reduction of CuO/3Y-TZP composite at room temperature10.1016/j.wear.2011.08.016 ↗
27. Influence of countersurface materials on dry sliding performance of CuO/Y-TZP composite at 600°C10.1016/j.jeurceramsoc.2012.07.025 ↗
28. Densification and phase transformation during pressureless sintering of nanocrystalline ZrO2–Y2O3–CuO ternary system10.1111/j.1551-2916.2008.02265.x ↗
29. Quantitative analysis of monoclinic-stabilized cubic ZrO2 systems by X-ray diffraction10.1111/j.1151-2916.1984.tb19715.x ↗
30. Wear resistant TiMoN coatings deposited by magnetron sputtering10.1016/j.wear.2005.07.008 ↗
31. Effect of particle size on tribological behavior of Ni3Al matrix high temperature self-lubricating composites10.1016/j.triboint.2011.07.002 ↗
32. NiAl matrix high-temperature self-lubricating composite10.1007/s11249-010-9727-9 ↗
33. Tribological behavior of NiAl matrix composites with addition of oxides at high temperatures10.1016/j.wear.2011.11.006 ↗
34. Comparative tribological behaviors of TiN, CrN and MoNCu nanocomposite coatings10.1016/j.triboint.2007.04.008 ↗
35. Ion-beam deposited Cu–Mo coatings as high temperature solid lubricants10.1016/S0257-8972(96)02900-3 ↗