Effect of cooling rate on the microstructure and mechanical properties of melt-grown Al2O3/YAG/ZrO2 eutectic ceramic
Source abstract
Abstract
Abstract Melt-grown Al 2 O 3 /YAG/ZrO 2 ternary eutectic samples were solidified by quenching and with controlled cooling rates of 10, 50, and 250 °C/min, respectively. Effect of cooling rate on microstructure and mechanical properties were examined. With the increase of cooling rate, three classical characteristic microstructures are obtained and developed from colony structure to dendrite structure and to cell structure. In the quenching process, the sample consists of lamellar eutectic cells and its fracture toughness increases to 4.13 ± 0.8 MPa m 1/2 . The microstructure transitions with the cooling rate are attributed to instability of the solid–liquid interface. In this work, the interface instability is analyzed to explain the microstructure evolutions in terms of undercooling and characteristic lengths of solute diffusion and capillarity effect.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Magnesium Oxide Properties and Applications · Microwave Dielectric Ceramics Synthesis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (31)
Show source-provided references
1. High temperature characteristics of unidirectionally solidified eutectic ceramic composites and some potential applications10.4028/www.scientific.net/MSF.638-642.997 ↗
2. Application of eutectic composites to gas turbine system and fundamental fracture properties up to 1700C10.1016/j.jeurceramsoc.2005.01.003 ↗
3. Ultra-high-strength nanofibrillar Al2O3-YAG-YSZ eutectics10.1002/adma.200602379 ↗
4. Directional solidification and microstructural development of Al2O3/GdAlO3 eutectic ceramic in situ composite under rapid growth conditions10.1016/j.jallcom.2011.01.107 ↗
5. Microstructure: growth mechanism and mechanical property of Al2O3-based eutectic ceramic in situ composites10.1016/j.jeurceramsoc.2010.11.008 ↗
6. Microstructure and mechanical properties of Al2O3/Er3Al5O12 eutectic rods grown by the laser-heated floating zone method10.1016/j.jeurceramsoc.2010.05.004 ↗
7. Growth and characterization of Al2O3/Y3Al5O12/ZrO2 ternary eutectic fibers10.1016/S0022-0248(01)01375-6 ↗
8. Microstructure of Y2O3 doped Al2O3–ZrO2 eutectics grown by the laser floating zone method10.1016/S0955-2219(02)00121-8 ↗
9. Al2O3–Y3Al5O12(YAG)-ZrO2 ternary composite rapidly solidified from the eutectic melt10.1016/j.jeurceramsoc.2005.01.012 ↗
10. Microstructures and properties of rapidly solidified Y2O3 doped Al2O3/ZrO2 composites prepared by combustion synthesis10.1016/j.scriptamat.2006.07.007 ↗
11. Microstructure and mechanical properties of near-eutectic ZrO2-60 wt.% Al2O3 produced by quenched plasma spraying10.1016/j.msea.2008.11.034 ↗
12. Binary eutectic solidification
13. Effect of the melt temperature on the solidification process of liquid garnets Ln3Al5O12 (Ln=Dy: Y, and Lu)10.1111/j.1151-2916.1992.tb04408.x ↗
14. Platzki · 1995
15. Temperature dependence of flexural strength and microstructure of Al2O3/Y3Al5O12/ZrO2 ternary melt growth composites10.1023/A:1016073115264 ↗
16. Microstructure and mechanical properties of Al2O3/Y3Al5O12/ZrO2 ternary eutectic materials10.1016/j.jeurceramsoc.2005.01.034 ↗
17. Rapid solidification of Al2O3/Y3Al5O12/ZrO2 eutectic in situ composites by laser zone remelting10.1016/j.jcrysgro.2007.06.029 ↗
18. Processing and microstructural study of surface laser remelted Al2O3–YSZ–YAG eutectic plates10.1016/j.jeurceramsoc.2010.08.016 ↗
19. Cooling-rate determination in splat-cooling of oxides10.1007/BF00540936 ↗
20. Metastable phase formation in plasma-sprayed ZrO2 (Y2O3)–Al2O310.1111/j.1151-2916.2003.tb03485.x ↗
21. Rapid solidification of Y3Al5O12 garnet from hypercooled melt10.1016/S1359-6454(01)00107-0 ↗
22. A fracture-mechanics analysis of indentation-induced palmqvist crack in ceramics10.1007/BF00725625 ↗
23. Directionally solidified eutectic ceramic oxides10.1016/j.pmatsci.2005.10.002 ↗
24. Mechanical properties of melt-grown alumina-yttrium aluminum garnet eutectics up to 1900K10.1111/j.1551-2916.2005.00265.x ↗
25. Kurz · 1998
26. Melting behavior and metastability of yttrium aluminum garnet (YAG) and YAlO3 determined by optical differental thermal-analysis10.1007/BF00550589 ↗
27. Solidification microstructure of laser remelted Al2O3–ZrO2 eutectic10.1016/S1359-6454(97)00198-5 ↗
28. Solidification and shape casting of Al2O3–YAG eutectic ceramics from the undercooled melt produced by melting Al2O3–YAP eutectics10.1016/j.stam.2003.10.022 ↗
29. Understanding the heat transfer and solidification of plasma-sprayed yttria-partially stabilized zirconia coatings10.1081/AMP-120029855 ↗
30. Microstructure characteristics of rapidly solidified alloys10.1016/0921-5093(94)90531-2 ↗
31. Investigation of the solidification behavior of Al2O3/YAG/YSZ ceramic in situ composite with off-eutectic composition10.1016/j.jeurceramsoc.2010.06.011 ↗