Self-generating oxidation protective high-temperature glass-ceramic coatings for C f /C‐SiC‐TiC‐TaC UHTC matrix composites
Source abstract
Abstract
The ablation/oxidation resistance of a carbon fibre (C-f)/carbon matrix (C)-SiC-TiC-TaC ceramic matrix composite (CMC) produced by melt infiltration of alloy into a C-f/C preform and tested in severely oxidising conditions was quantitatively determined and discussed. An oxyacetylene flame shot of 7.5 s (4 MW/m(2) nominal heat flux), as well as oxidising conditions imposed by a radiant furnace in air at 1873 K up to 480 s were the selected testing conditions. Detailed post-test microstructure investigations of the oxidised/ablated infiltrated CMC samples, compared to unprotected CMCs tested in nominally identical conditions, enabled to establish an increase in ablation/oxidation resistance of one order of magnitude. The occurrence of a self-generating protective high-temperature glass-ceramic, disclosed by microstructure analyses, played a substantial role for that performance jump during oxidation/ablation. The C-f/C-SiC-TiC-TaC composite herein tested can be a valuable candidate for uses in severe aerospace applications (propulsion and hypersonic flight). (C) 2017 Elsevier Ltd. All rights reserved.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Intermetallics and Advanced Alloy Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (37)
Show source-provided references
1. Analytical evaluation of hybrid ceramic design concepts for optimized structural performance10.1016/j.msea.2006.12.091 ↗
2. Validation of silicon and boron based oxygen-impermeable material systems for protection of continuous fiber reinforced carbon composites10.1016/j.msea.2007.10.125 ↗
3. Oxidation-based materials selection for 2000°C+ hypersonic aerosurfaces: theoretical considerations and historical experience10.1023/B:JMSC.0000041686.21788.77 ↗
4. High-temperature erosion resistance of ZrB2-based ceramic coating for lightweight carbon/carbon composites under simulated atmospheric re-entry conditions by high frequency plasma wind tunnel test10.1016/j.ceramint.2016.03.029 ↗
5. UHTCs – ultra-High temperature ceramic materials for extreme environment applications10.1149/2.F04074IF ↗
6. Ablation behavior of ZrB2–SiC protective coating for carbon/carbon composites10.1016/j.ceramint.2015.02.096 ↗
7. Preparation and properties of 2D C/SiC–ZrB2–TaC composites10.1016/j.ceramint.2010.10.033 ↗
8. Ablation behavior and mechanism of C/ZrC, C/ZrC–SiC and C/SiC composites fabricated by polymer infiltration and pyrolysis process10.1016/j.corsci.2014.05.005 ↗
9. Ultra-high temperature ceramic TaB2–TaC–SiC coating for oxidation protection of SiC-coated carbon/carbon composites10.1016/j.ceramint.2014.02.013 ↗
10. Phase relations in the system CaO-Ta2O5-SiO210.1111/j.1151-2916.1969.tb11968.x ↗
11. Ablation behaviors of ultra-high temperature ceramic composites10.1016/j.msea.2007.02.040 ↗
12. Ablation behaviors of carbon/carbon composites with C-SiC-TaC multi-interlayers10.1016/j.apsusc.2009.07.006 ↗
13. Effects of TaC addition on the ablation resistance of C/SiC10.1016/j.matlet.2010.04.051 ↗
14. Self-generating high-temperature oxidation-resistant glass-ceramic coatings for C–C composites using UHTCs10.1111/jace.13017 ↗
15. Microstructure, mechanical properties and oxidation behavior of TaC- and HfC-based materials containing short SiC fiber10.1016/j.ceramint.2014.09.070 ↗
16. Oxidation studies on TaC based ultra-high temperature ceramic composites under plasma arc jet exposure10.1016/j.corsci.2016.03.013 ↗
17. Effect of oxide additions on the polymorphism of tantalum pentoxide (System Ta2O5–TiO2)10.6028/jres.072A.018 ↗
18. Morphology, thermal response and anti-ablation performance of 3D-four directional pitch-based carbon/carbon composites10.1016/j.corsci.2012.04.036 ↗
19. Evaluation of the high temperature performance of HfB2 UHTC particulate filled Cf/C composites10.1111/ijac.12659 ↗
20. Degradation behavior of 4D carbon/carbon composites under supersonic oxidative air plasma10.1016/j.ceramint.2013.02.056 ↗
21. UHTC–carbon fibre composites: preparation, oxyacetylene torch testing and characterisation10.1016/j.jeurceramsoc.2012.08.018 ↗
22. Preparation and properties of 2D C/SiC-TaC composites
23. Preparation and characterization of C/SiC–ZrB2 composites by precursor infiltration and pyrolysis process10.1016/j.ceramint.2009.11.015 ↗
24. Processing, microstructure and ablation behavior of C/SiC–Ti3SiC2 composites fabricated by liquid silicon infiltration10.1016/j.corsci.2013.04.029 ↗
25. Erosion resistance of C/C-SiC-ZrB2 composites exposed to oxyacetylene torch10.1016/j.jeurceramsoc.2016.04.007 ↗
26. Ablation behavior of TaB2-SiC coating for carbon/carbon composites under oxyacetylene torch10.1016/j.vacuum.2016.06.022 ↗
27. HfC-ZrC-SiC multiphase protective coating for SiC-coated C/C composites prepared by supersonic atmospheric plasma spraying10.1016/j.ceramint.2016.10.120 ↗
28. Ablation resistance of SiC-modified ZrC coating prepared by SAPS for SiC-coated carbon/carbon composites
29. Ablation resistance of ZrB2-SiC coating prepared by supersonic atmosphere plasma spraying for SiC-coated carbon/carbon composites10.1016/j.ceramint.2014.06.064 ↗
30. Ablation properties of carbon/carbon composites with tungsten carbide10.1016/j.apsusc.2008.12.063 ↗
31. Effect of heat flux on ablation behaviour and mechanism of C/C–ZrB2–SiC composite under oxyacetylene torch flame10.1016/j.corsci.2013.04.052 ↗
32. Anti-oxidation and ablation properties of carbon/carbon composites infiltrated by hafnium boride10.1016/j.carbon.2012.09.053 ↗
33. Fabrication and ablation property of carbon/carbon composites with novel SiC–ZrB2 coating10.1016/S1003-6326(15)64012-2 ↗
34. Oxidation and ablation resistance of Fe2O3 modified ZrB2–SiC–Si coating for carbon/carbon composites10.1016/j.ceramint.2015.08.105 ↗
35. Oxidation and ablation resistance of the ZrB2–CrSi2–Si/SiC coating for C/C composites at high temperature10.1016/j.jallcom.2015.12.011 ↗
36. Thermochemical and mechanical stabilities of the oxide scale of ZrB2 +SiC and oxygen transport mechanisms10.1111/j.1551-2916.2008.02319.x ↗
37. A. Roine. HSC Chemistry v6.12, Outotec Research Oy1974-2007 Finland.