journal article·2019-04Open access

Studying the wettability of Si and eutectic Si-Zr alloy on carbon and silicon carbide by sessile drop experiments

Manoj Naikade, Beate Fankhänel, Ludger Weber, Alberto Ortona, Michael Stelter, Thomas Graule

Abstract

Abstract The contact angles of two different systems, molten silicon and a eutectic Si-8 at. pct Zr alloy and their evolution over timeon vitreous carbon and polycrystalline silicon carbide (SiC) substrates were investigated at 1500°C under vacuum, as well as in argon using the sessile drop technique. The contact angle and microstructure of the liquid droplet/solid substrate interface were studied to understand fundamental features of reactive wetting as it pertains to the infiltration process of silicon and silicon alloys into carbon or C/SiC preforms. Both pure Si and theeutectic alloy showed good wettability onvitreous carbon and SiC characterized by equilibrium contact angles between 29° and 39°. Theeutectic alloy showed a higher initial contact angle and slower spreading as compared to that of pure Si. On vitreous carbon bothsilicon and the eutecticalloy formed SiC at the interface, while no reaction was observed on the SiC substrates.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Semiconductor materials and devices · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (34)

Show source-provided references
1. Cost effective processing of CMC composites by melt infiltration (LSI-process)
2. Microstructural evolution during silicon carbide (SiC) formation by liquid silicon infiltration using optical microscopy10.1016/j.ijrmhm.2009.09.002 ↗
3. High temperature load–deflection behaviour of reaction bonded SiC (RBSC)10.1016/S0272-8842(00)00120-6 ↗
4. Silicon melt infiltrated ceramic composites (HiPerComp™)
5. Study of process of erosion of various types of carbon fibres by molten silicon10.1007/s10692-012-9407-7 ↗
6. Reaction-bonded silicon carbide by reactive infiltration10.1021/ie001029e ↗
7. Self-diffusion of 14C in polycrystalline β-SiC10.1007/BF00737031 ↗
8. Diffusion of C-13 and Si-29 implanted ions in sic10.1016/0921-5107(92)90235-2 ↗
9. Reactions between silicon and graphite substrates at high temperature: in situ bbservations10.1007/s11663-013-9947-0 ↗
10. The role of the chemical reaction in the infiltration of porous carbon by NiSi alloys10.1016/j.scriptamat.2006.02.015 ↗
11. Reactive infiltration of porous graphite by NiSi alloys10.1016/j.actamat.2008.01.011 ↗
12. C/C-ZrC composite prepared by chemical vapor infiltration combined with alloyed reactive melt infiltration10.1016/j.ceramint.2012.04.017 ↗
13. Liquid-phase reaction-bonding of silicon carbide using alloyed silicon-molybdenum melts10.1111/j.1151-2916.1990.tb05179.x ↗
14. Y.M. Chiang, R.P. Messner, Method of preparing refractory silicon carbide composites and coatings, Massachusetts Institute Of Technology, Patent number US5079195 A (1992).
15. Processing-microstructure-properties relationships of MoSi2-SiC composites10.1016/S0955-2219(02)00035-3 ↗
16. C/C-SiC-ZrC composites fabricated by reactive melt infiltration with Si0.87Zr0.13 alloy10.1016/j.ceramint.2012.02.016 ↗
17. Fabrication of 2D C/ZrC–SiC composite and its structural evolution under high-temperature treatment up to 1800°C10.1016/j.ceramint.2009.03.030 ↗
18. Wetting dynamics versus interfacial reactivity of AlSi alloys on carbon10.1007/s10853-009-3909-6 ↗
19. C/SiC–ZrB2–ZrC composites fabricated by reactive melt infiltration with ZrSi2 alloy10.1016/j.ceramint.2012.05.035 ↗
20. Wetting properties of Molten Silicon with10.1007/s11661-010-0362-8 ↗
21. Wetting and infiltration of graphite materials by molten silicon10.1016/S0956-716X(99)80068-5 ↗
22. Reactivity between liquid Si or Si alloys and graphite10.1016/j.jeurceramsoc.2012.05.020 ↗
23. Wetting of SiC, Si3N4, and carbon by Si and binary Si alloys10.1111/j.1151-2916.1975.tb19006.x ↗
24. Wettability and reactivity of molten silicon with various substrates10.1007/s00339-002-2001-8 ↗
25. Mechanisms of reactive wetting: the question of triple line configuration10.1016/S1359-6454(96)00372-2 ↗
26. Influence of interfacial reaction rates on the wetting driving force in metal/ceramic systems10.1007/BF02663868 ↗
27. Wetting and reactivity in Ni–Si/C system: experiments versus model predictions10.1007/s10853-006-1483-8 ↗
28. Wetting of ceramics by molten silicon and silicon alloys: a review10.1007/s10853-012-6663-0 ↗
29. Capillary interactions between molten silicon and porous graphite10.1007/s10853-009-3889-6 ↗
30. Survey on wetting of SiC by molten metals10.1016/j.ceramint.2010.01.001 ↗
31. Dynamic wetting of graphite and SiC by ferrosilicon alloys and silicon at 1550°C10.2355/isijinternational.46.1570 ↗
32. Examination of the interaction between liquid silicon and bulk silicon carbide10.1016/j.jcrysgro.2015.05.013 ↗
33. Wetting and infiltration of carbon by liquid silicon10.1007/s10853-005-1950-7 ↗
34. Thermodynamic assessment of the C–Si–Zr system10.1016/j.jallcom.2008.06.086 ↗