Influence of h-BN as additive on microstructure and oxidation mechanism of C/C-SiC composite
Source abstract
Abstract
Abstract Due to the favorable self-healing performance, hexagonal boron nitride (h-BN) as additive in the matrix can significantly influence the oxidation behavior and the kinetic characteristics of C/C-SiC composites. In this work, C/C-SiC composites modified by h-BN (C/C-BN-SiC) were prepared by low-temperature compression molding (LTCM), pyrolysis and liquid silicon infiltration (LSI). Microstructure, oxidation behavior and kinetic characteristics of the C/C-BN-SiC composites were investigated compared with the C/C-SiC composite. Because h-BN is non-wetted by liquid silicon, the h-BN flakes in the matrix can obstruct and prolong the flow path of silicon, and protect the carbon fibers from corrosion to a certain extent. The oxidation kinetics of composites occur in low and high temperature domains, with different oxidation-controlling mechanisms, and the addition of h-BN can hinder the inward diffusion and lead to the decline of carbon recession and apparent activation energy.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Boron and Carbon Nanomaterials Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (29)
Show source-provided references
1. Damage analysis of 2.5D C/C-SiC composites subjected to fatigue loadings10.1016/j.jeurceramsoc.2019.01.014 ↗
2. Oxidation behavior of C/SiC-Ti3SiC2 at 800-1300 °C in air10.1016/j.jeurceramsoc.2016.03.029 ↗
3. Fatigue behavior and residual strength evolution of 2.5D C/C-SiC composites10.1016/j.jeurceramsoc.2016.07.009 ↗
4. Mechanical response and microstructure of 2D carbon fiber reinforced CMCs containing Cu-Si alloy exposed to fatigue stresses10.1016/j.compositesb.2018.10.016 ↗
5. Mechanical behavior of LSI based C/C-SiC composites subjected to flexural loadings10.1016/j.compositesa.2017.01.024 ↗
6. Effect of B4C on the microstructure and properties of B4C modified three-dimensional needled C/C-SiC composites10.1016/j.msea.2017.09.008 ↗
7. Preparation and oxidation resistance of 2D C/SiC composites modified by partial boron carbide self-sealing matrix10.1016/j.msea.2008.08.022 ↗
8. Degradation mechanisms of a self-healing SiC(f) /BN(i) /[SiC-B4C](m), composite at high temperature under different oxidizing atmospheres10.1016/j.jeurceramsoc.2018.05.001 ↗
9. Oxidation mechanisms and kinetics of SiC-matrix composites and their constituents10.1023/B:JMSC.0000048745.18938.d5 ↗
10. Oxidation kinetics and stress effects for the oxidation of continuous carbon fibers within a microcracked C/SiC ceramic matrix composite10.1111/j.1551-2916.2007.02170.x ↗
11. Oxidation behavior of 2D C/SiC composite modified by SiB4 particles in inter-bundle pores10.1016/j.compscitech.2007.10.016 ↗
12. Fabrication of carbon fiber reinforced ceramic matrix composites with improved oxidation resistance using boron as active filler10.1016/j.jeurceramsoc.2009.09.015 ↗
13. Review on the properties of hexagonal boron nitride matrix composite ceramics10.1016/j.jeurceramsoc.2016.05.007 ↗
14. A.F. Alexeev. High-temperature oxidation of boron nitride10.1016/S0272-8842(86)80006-2 ↗
15. High-temperature oxidation of boron nitride: II, boron nitride layers in composites10.1111/j.1151-2916.1999.tb01944.x ↗
16. Carbon/carbon–boron nitride composites with improved wear resistance compared to carbon/carbon10.1016/j.carbon.2004.05.024 ↗
17. Structure/oxidation behavior relationship in the carbonaceous constituents of 2D-C/PyC/SiC composites10.1016/0008-6223(93)90086-P ↗
18. Kinetics and mechanisms of oxidation of 2D woven C/SiC composites: II, theoretical approach10.1111/j.1151-2916.1994.tb07097.x ↗
19. Kinetics and mechanisms of oxidation of 2D woven C/SiC composites: I, experimental approach10.1111/j.1151-2916.1994.tb07096.x ↗
20. Long-term oxidation behaviors of C/SiC composites with a SiC/UHTC/SiC three-layer coating in a wide temperature range10.1016/j.corsci.2018.10.017 ↗
21. Wetting and adhesion of Si on Si3N4 and BN substrates10.1016/j.jeurceramsoc.2009.01.024 ↗
22. Preparation of C/C-SiC composite by low temperature compression molding-liquid silicon infiltration and its application in automobile brake10.1016/j.ceramint.2015.09.030 ↗
23. Huang · 2013
24. Oxidative erosion of graphite in air between 600 and 1000 K
25. Oxidation and ablation of 3D carbon-carbon composite at up to 3000 °C10.1016/0008-6223(94)00172-V ↗
26. Dynamic oxidation and protection of the PAN pre-oxidized fiber C/C composites10.1016/j.ceramint.2018.01.021 ↗
27. Oxidation of carbon/carbon composites—a theoretical analysis10.1016/0008-6223(88)90040-1 ↗
28. Oxidation behavior and protection of carbon/carbon composites prepared using rapid directional diffused CVI techniques10.1016/S0008-6223(02)00025-8 ↗
29. Relationship between oxidation resistance and structure of B4C–SiC/C composites with self-healing properties10.1016/S0008-6223(98)00184-5 ↗