journal article·2020-12

Interfacial reaction mechanism of SiC joints joined by pure nickel foil

Haojiang Shi, Yidi Chai, Ning Li, Jiazhen Yan, Xin Zhu, Kangwei Chen, Dong Bai, Zihao Liu, Miaomiao Wu, Ruiqian Zhang, Ming Li, Mingliang Luo, Qi Sun, Chenglai Xin, Wenmin Hu, Xin Dong

Publisher page

Abstract

Abstract To investigate the reaction mechanism of Ni/SiC system, 0.1 μm-thick pure nickel foil is used to join SiC ceramic at 1245 °C for different times. Interfacial melting is calculated to occur at 964 °C along the interface due to the low eutectic point of θ-Ni2Si and NiSi, a periodical layered structure, consisting alternating layers of silicides/silicides+graphite, is formed along the interface due to periodical detachment of graphite from SiC reaction interface during the reactions between Ni-Si liquid phase and SiC. The reaction products of Ni/SiC are successfully predicted by CALPHAD method, based on a home-made Ni-Si-C ternary database. The reaction processes between Ni and SiC and the morphology changes of the joined seam are discussed in detail in this paper. The average shear strengths of SiC joints held for 15 min, 30 min and 60 min are tested to be 16.53 MPa, 19.32 MPa and 29.43 MPa, respectively.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Aluminum Alloys Composites Properties · Intermetallics and Advanced Alloy Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (51)

Show source-provided references
1. A novel process with the characteristics of low-temperature bonding and high-temperature resisting for joining Cf/SiC composite to GH3044 alloy10.1016/j.jeurceramsoc.2019.08.031 ↗
2. Recent advances in joining of SiC-based materials (monolithic SiC and SiCf/SiC composites): joining processes, joint strength, and interfacial behavior10.1007/s40145-018-0297-x ↗
3. Study of SiC/nickel alloy bonding for high temperature applications10.1016/j.jeurceramsoc.2008.06.035 ↗
4. Ultrafast laser welding of ceramics10.1126/science.aaw6699 ↗
5. Brazing SiC matrix composites using Co-Ni-Nb-V alloy10.1007/s40194-017-0469-2 ↗
6. Flexural strength and shear strength of silicon carbide to silicon carbide joints fabricated by a molybdenum diffusion bonding technique10.1111/j.1551-2916.2005.00381.x ↗
7. Joining of SiC based ceramics and composites with Si-16Ti and Si-18Cr eutectic alloys10.1504/IJMPT.2004.004778 ↗
8. Joining of SiC ceramic to graphite using Ni-Cr-SiC powders as filler10.1016/j.msea.2008.01.082 ↗
9. Joining of SiC ceramic-based materials with ternary carbide Ti3SiC210.1016/j.mseb.2010.09.002 ↗
10. Microstructures and mechanical properties of vacuum brazed SiC ceramics joint
11. Silicon carbide diffusion bonding by spark plasma sintering10.1080/10426914.2014.952019 ↗
12. Brazing of SiC to a wrought nickel-based superalloy using CoFeNi(Si, B)CrTi filler metal10.1016/j.matlet.2007.03.003 ↗
13. Interfacial debonding by solid-state reactions of SiC with Ni and Co10.1016/0956-716X(93)90318-M ↗
14. In-situ high temperature X-ray diffraction study of Ni/SiC interface reactions10.1023/A:1004428816391 ↗
15. Raman study on the Ni/SiC interface reaction10.1063/1.1473226 ↗
16. Interfacial reactions of crystalline Ni and amorphous SiC thin films10.1007/s10853-018-1986-0 ↗
17. Tang · 2009
18. Prediction of interface reaction products between Cu and various solder alloys by thermodynamic calculation10.1016/S1359-6454(96)00325-4 ↗
19. Prediction of Ti/Al2O3 interface reaction products by diffusion simulation10.1016/S1359-6454(97)00108-0 ↗
20. High-temperature-reactivity of Al-Ti alloys in contact with SiC10.1016/j.jallcom.2019.152715 ↗
21. A new approach to establish both stable and metastable phase equilibria for fcc ordered/disordered phase transition: application to the Al-Ni and Ni-Si systems10.1016/j.matchemphys.2012.04.028 ↗
22. Thermodynamic calculation of the ternary system Al-Si-C10.1016/S0364-5916(96)00027-2 ↗
23. Thermodynamic modeling of the C-Co-Mo and C-Mo-Ni ternary systems10.1007/s11669-016-0471-1 ↗
24. Thermodynamic reassessment of the C-Ni-Si system using a four sublattice model for ordered/disordered fcc phases10.1007/s11669-017-0571-6 ↗
25. The Ni-Si (Nickel-Silicon) system
26. Solid-state reactions of SiC with Co, Ni, and Pt10.1557/JMR.1991.0796 ↗
27. Solid-state SiC/Ni alloy reaction10.1007/BF02644213 ↗
28. High-temperature interfacial reactions of SiC with metals10.1116/1.577673 ↗
29. Low-temperature formation of nanocrystalline β-SiC with high surface area and mesoporosity via reaction of mesoporous carbon and silicon powder10.1016/j.micromeso.2005.02.022 ↗
30. Interfacial reaction and adhesion between SiC and thin sputtered nickel films10.1023/A:1018623613741 ↗
31. Reactions at amorphous SiC/Ni interfaces10.1063/1.369580 ↗
32. Nickel-silicide : carbon contact technology for N-channel MOSFETs with silicon-carbon source/drain10.1109/LED.2007.910793 ↗
33. Wetting and bonding of Ni-Si alloys on silicon carbide10.1016/S1359-6454(98)00374-7 ↗
34. Thermodynamic brazing alloy design for joining silicon carbide10.1111/j.1151-2916.1991.tb07799.x ↗
35. The role of compound formation in reactive wetting: the Cu/SiC system10.1016/S1359-6454(00)00235-4 ↗
36. Study of reaction process on Ni/4H-SiC contact10.1179/174328406X118276 ↗
37. Pattern formation in Pt-SiC diffusion couples10.1016/S0167-2738(96)00578-4 ↗
38. Kinetics of formation of silicides: a review10.1557/JMR.1986.0205 ↗
39. Grain boundary reactive diffusion during Ni2Si formation in thin films and its dependence on the grain boundary angle10.1016/S0169-4332(98)00475-9 ↗
40. Nanostructuring in Ni/SiC reaction layers, investigated by imaging of atomic columns and DFT calculations10.1016/j.matchemphys.2008.10.060 ↗
41. Direct observation of interfacial reaction of Ni/6H-SiC and carbon redistribution by in situ transmission electron microscopy10.1016/j.matchar.2018.03.047 ↗
42. Observations of crystal-structure images of silicon
43. The structure of Ni2Si10.1107/S0365110X52001003 ↗
44. The structure of Ni5Si2 formed in Ni-Si thin-film lateral diffusion couples10.1063/1.339830 ↗
45. Combined synchrotron x-ray diffraction and wafer curvature measurements during Ni-Si reactive film formation10.1063/1.1999021 ↗
46. Influence of thermal exposure on microstructure evolution and tensile fracture behaviors of compacted graphite iron10.1016/j.msea.2016.03.118 ↗
47. Damaging micromechanisms in ferritic-pearlitic ductile cast irons10.1016/j.msea.2007.05.110 ↗
48. On stress propagation and fracture in compacted graphite iron10.1007/s00170-011-3157-1 ↗
49. First-principles investigation of mechanical and thermodynamic properties of nickel silicides at finite temperature10.1134/S1063783418050360 ↗
50. Thickness-dependent phase evolution and bonding strength of SiC ceramics joints with active Ti interlayer10.1016/j.jeurceramsoc.2016.12.009 ↗
51. Residual thermal stress of SiC/Ti3SiC2/SiC joints calculation and relaxed by postannealing10.1111/ijac.12900 ↗