High temperature strength of silicon carbide sintered with 1 wt.% aluminum nitride and lutetium oxide
Source abstract
Abstract
Abstract A heat-resistant SiC ceramic was developed from submicron β-SiC powders using a small amount (1 wt.%) of AlN–Lu2O3 additives at a molar ratio of 60:40. Observation of the ceramic using high-resolution transmission electron microscopy (HRTEM) showed a lack of amorphous films in both homophase (SiC–SiC) boundaries and junction areas. The junction phase consisted of Lu–Si–O elements, and the homophase boundaries contained Lu, Al, O, and N atoms as segregates. The ceramic maintained its room temperature (RT) strength up to 1600 °C. The flexural strength of the ceramic was 630 MPa and 633 MPa at RT and 1600 °C, respectively.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (34)
Show source-provided references
1. SiC and Si3N4 materials with improved fracture resistance10.1016/0955-2219(92)90028-C ↗
2. High temperature mechanical behavior of liquid phase sintered silicon carbide10.1016/S0955-2219(97)00163-5 ↗
3. Influence of the α/β-SiC phase transformation on microstructural development and mechanical properties of liquid phase sintered silicon carbide10.1023/A:1004552704872 ↗
4. Effects of additives on densification, microstructure and properties of liquid-phase sintered silicon carbide10.1023/A:1004881430804 ↗
5. Oxidation and burner rig corrosion of liquid phase sintered SiC10.1016/S0955-2219(99)00160-0 ↗
6. Fracture properties of SiC ceramics with oxynitride additives10.1016/S0955-2219(02)00132-2 ↗
7. Microstructural changes in liquid-phase-sintered silicon carbide during creep in an oxidizing environment10.1111/j.1151-2916.2003.tb03328.x ↗
8. Ambient to high-temperature fracture toughness and cyclic fatigue behavior in Al-containing silicon carbide ceramics10.1016/j.actamat.2003.08.038 ↗
9. Effect of AlN-content on the microstructure and fracture toughness of hot-pressed and heat-treated LPS-SiC ceramics10.1016/j.jeurceramsoc.2004.01.024 ↗
10. Preparation of dense nanocrystalline silicon carbide ceramics by sinter forging in the presence of a liquid phase10.1002/adem.200500009 ↗
11. Grain boundary crystallization during furnace cooling of α-SiC sintered with Y2O3–Al2O3–CaO10.1016/j.jeurceramsoc.2005.01.050 ↗
12. Densification of liquid phase sintered silicon carbide10.1016/j.jeurceramsoc.2005.03.253 ↗
13. High-temperature strength of silicon carbide ceramics sintered with rare-earth oxide and aluminum nitride10.1016/j.actamat.2006.08.059 ↗
14. Particle size effect of starting SiC on processing, microstructure and mechanical properties of liquid phase-sintered SiC10.1016/j.jeurceramsoc.2010.02.026 ↗
15. Anomalous oxidation behavior of pressureless liquid-phase-sintered SiC10.1016/j.jeurceramsoc.2011.05.015 ↗
16. Influence of small amount of sintering additives on unlubricated sliding wear properties of SiC ceramics10.1016/j.ceramint.2011.06.018 ↗
17. Effect of intergranular phase chemistry on the sliding-wear resistance of pressureless liquid-phase-sintered α-SiC10.1016/j.jeurceramsoc.2011.09.011 ↗
18. Grain-boundary viscosity of preoxidized and nitrogen-annealed silicon carbides10.1111/j.1151-2916.2001.tb01017.x ↗
19. Role of the grain-boundary phase on the elevated-temperature strength, toughness, fatigue and creep resistance of silicon carbide sintered with Al, B and C10.1016/S1359-6454(00)00246-9 ↗
20. Improved high temperature properties of SiC-ceramics sintered with Lu2O3-containing additives10.1016/S0955-2219(02)00282-0 ↗
21. Effect of rare-earth cation additions on the high temperature oxidation behavior of LPS-SiC10.1016/j.msea.2003.11.037 ↗
22. Comparative bending creep behavior of silicon carbide sintered with oxynitride additives10.1016/j.scriptamat.2005.04.024 ↗
23. Liquid phase sintered silicon carbide (LPS-SiC) ceramics having remarkably high oxidation resistance in wet air10.1016/j.jeurceramsoc.2005.05.015 ↗
24. Chemical compatibility of SiC composite structure with fusion reactor helium coolant at high temperatures10.1016/0920-3796(93)90008-6 ↗
25. Consolidation of nanostructured SiC with disorder–order transformation10.1016/j.scriptamat.2003.09.027 ↗
26. Processing of nano-SiC ceramics: densification by SPS and mechanical characterization10.1016/j.jeurceramsoc.2011.10.006 ↗
27. Processing of high performance silicon carbide10.2109/jcersj2.116.665 ↗
28. Effect of in situ-synthesized nano-size SiC addition on density and electrical resistivity of liquid-phase sintered silicon carbide ceramics10.2109/jcersj2.119.965 ↗
29. Kim YW, Lim KY, Kim KJ. Electrical resistivity of silicon carbide ceramics sintered with 1wt.% aluminum nitride and rare earth oxide. J Eur Ceram Soc, in press.
30. Microstructure stability of fine-grained silicon carbide ceramics during annealing10.1023/B:JMSC.0000030713.40220.07 ↗
31. Effects of the initial α-SiC content on the microstructure, mechanical properties, and permeability of macroporous silicon carbide ceramics10.1016/j.jeurceramsoc.2011.11.040 ↗
32. Effect of grain boundary segregation on high-temperature strength of hot-pressed silicon carbide10.1016/S1359-6454(96)00179-6 ↗
33. Heat-resistant silicon carbide with aluminum nitride and scandium oxide10.1016/j.actamat.2005.07.002 ↗
34. Heat-resistant silicon carbide with aluminum nitride and erbium oxide10.1111/j.1151-2916.2001.tb00958.x ↗