journal article·2009-01

3D analysis of crack morphologies in silicate glass using FIB tomography

F. Elfallagh, B.J. Inkson

Publisher page

Abstract

The surface damage and induced cracks around Vickers indents in soda-lime-silicate glass have been examined for the first time in 3D by cross-sectioning the indents using a highly focused ion beam (FIB). The 3D FIB tomographic analysis determines quantitatively both the location and 3D shape of individual cracks within a cluster around an indentation, and the 3D FIB technique will be applicable to analyse other types of surface damage in amorphous materials. For silicate glass it is shown that increasing the applied indent load from 50 to 200 g, results in a significant increase in measured crack density and 3D interconnections. It is also observed that the planar FIB cross-section surfaces cut through the very centre of the indents can undergo time-dependant strain and bulge outwards in order to relieve high local residual stresses.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced Surface Polishing Techniques · Integrated Circuits and Semiconductor Failure Analysis · Advanced ceramic materials synthesis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (25)

Show source-provided references
1. Effects of very high pressures on glass10.1063/1.1721294 ↗
2. High pressure effects on glass10.1016/0022-3093(69)90012-X ↗
3. Direct observation and analysis of indentation cracking in glasses and ceramics10.1111/j.1151-2916.1990.tb05119.x ↗
4. Subcritical growth of indentation median cracks in soda-lime-silica glass10.1111/j.1151-2916.1995.tb08227.x ↗
5. Plastic flow in glass.10.1098/rspa.1964.0114 ↗
6. Study of the mechanical properties of ceramic materials by nanoindentation technique10.1016/S0955-2219(98)00083-1 ↗
7. Morphology of vickers indent flaws in soda-lime-silica glass10.1111/j.1151-2916.2001.tb01015.x ↗
8. The sub-critical indentation fracture process in sods-lime-silica glass10.1016/0013-7944(95)00255-3 ↗
9. Densification and residual stresses induced in glass surfaces by Vickers indentation10.1016/S0022-3093(00)00140-X ↗
10. Strength degradation of glass resulting from impact with spheres10.1111/j.1151-2916.1977.tb15531.x ↗
11. High temperature microhardness of soda-lime glass10.1016/j.jnoncrysol.2004.08.138 ↗
12. The effect of focused ion beam machining on residual stress and crack morphologies in Alumina10.1088/1742-6596/26/1/052 ↗
13. 3D mapping of subsurface cracks in alumina using FIB Fundamentals of nanoindentation and nanotribology
14. Subsurface damage analysis by TEM and 3D FIB crack mapping in alumina/5 vol.%SiC nanocomposites10.1016/S1359-6454(02)00387-7 ↗
15. Subsurface nanoindentation deformation of Cu–Al multilayers mapped in 3D by focused ion beam microscopy10.1046/j.1365-2818.2001.00767.x ↗
16. 3D FIB mapping of nanoindentation zones in a Cu–Ti multilayered coating10.1016/S0040-6090(02)00283-3 ↗
17. Computer visualization of three-dimensional image data using IMOD10.1006/jsbi.1996.0013 ↗
18. 3D reconstruction and characterization of polycrystalline microstructures using a FIB-SEM system10.1016/j.matchar.2006.01.019 ↗
19. Three dimensional imaging of deformation modes in TiN-based thin film coatings10.1016/j.tsf.2006.01.034 ↗
20. Crack opening profiles of indentation cracks in normal and anomalous glasses10.1016/j.actamat.2003.09.014 ↗
21. Vickers indentation behaviour of several commercial glasses at high temperature10.1007/s10853-007-2174-9 ↗
22. Indentation fracture and soft impresser fatigue in sapphire and polycrystalline alumina10.1016/S0263-4368(98)00041-9 ↗
23. Cyclic loading behaviour of soda-lime-silicate glass using indentation cracks10.1111/j.1460-2695.1997.tb00326.x ↗
24. Evolution of residual stress and crack morphologies during 3D FIB tomographic analysis of alumina10.1111/j.1365-2818.2008.01981.x ↗
25. Indentation of glass as a function of temperature10.1016/S0022-3093(00)00113-7 ↗