Electrochemical corrosion of silicon carbide ceramics in sodium hydroxide
Source abstract
Abstract
Abstract Sintered silicon carbide ceramics have found widespread use due to their high corrosion stability. This corrosion stability can be affected by electrochemical processes. Electrochemical corrosion experiments conducted on an SSiC material in NaOH at different voltages and subsequent detailed investigation of the formed surfaces were carried out. Systematic local measurement of the corrosion rate was carried out using the AFM technique. The results revealed the recession of the SiC grain surfaces under anodic electrochemical loading, with the extents differing strongly from grain to grain. The recession rates were not found to correlate with the SiC grain orientations or polytypes. Rather, the data and the observed microstructure indicated that the behaviour was caused by variations in the resistivities of the grain boundaries.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Corrosion Behavior and Inhibition · Semiconductor materials and devices
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (29)
Show source-provided references
1. Silicon carbide and boron carbide based hard materials
2. Zur Beständigkeit von Hochleistungskeramiken gegen Flüssigkorrosion
3. Zur Beständigkeit von Hochleistungskeramiken gegen Flüssigkorrosion
4. Corrosion behaviour of different technical ceramics in acids basic solutions and under hydrothermal condition
5. 1984 · vol. B2 (Part 1) · 139
6. Secondary electron imaging of SiC-based structures in secondary electron microscope10.1016/j.susc.2007.04.142 ↗
7. Schottky barrier formation in liquid-phase sintered silicon carbide10.3139/146.030211 ↗
8. Interface characteristics affecting electrical properties of Y-doped SiC10.1557/JMR.2003.0365 ↗
9. Charge transport in silicon carbide: atomic and microscopic effects10.1063/1.363054 ↗
10. The AC conductivity of liquid-phase-sintered silicon carbide10.1111/j.1551-2916.2007.01792.x ↗
11. Evaluation of grain-boundary conduction of dense AlN–SiC solid solution by scanning nonlinear dielectric microscopy10.1111/j.1551-2916.2010.04230.x ↗
12. Anomalous charge carrier transport phenomena in highly aluminum doped SiC10.1002/pssc.200564150 ↗
13. The influence of porosity on the electrical properties of liquid phase sintered silicon carbide10.3139/146.101285 ↗
14. Electrically driven cold water corrosion of SiC
15. Electrochemical corrosion of silicon carbide ceramics in H2SO410.1016/j.jeurceramsoc.2013.08.024 ↗
16. Corrosion of silicon carbide ceramics using conventional and electrochemical methods10.1179/000705994798267692 ↗
17. Electrochemical techniques for corrosion rate determination in ceramics10.1111/j.1151-2916.1989.tb06217.x ↗
18. Electrochemical corrosion of solid and liquid phase sintered silicon carbide in acidic and alkaline environments10.1016/j.jeurceramsoc.2006.07.011 ↗
19. Electrochemical corrosion of silicon carbide ceramics Part 1: electrochemical investigation of sintered silicon carbide (SSiC)10.1002/maco.200905448 ↗
20. Electrochemical corrosion of liquid-phase sintered silicon carbide
21. Electrochemical etching of n-type 6H–SiC using aqueous KOH solutions10.4028/www.scientific.net/MSF.433-436.665 ↗
22. Electrochemical etching of 6H–SiC10.1149/1.2054810 ↗
23. Theoretische grundlagen der ermittlung von korrosionsstromdichten aus polarisationswiderständen10.1002/maco.19760270406 ↗
24. Thin anodic oxide layers on aluminium and other valve metals10.1016/0927-796X(93)90005-N ↗
25. ECM of SiC-based ceramics–a first approach
26. Kleebe H-J. Private communication.
27. Core–shell structure from the solution-reprecipitation process in hot-pressed AlN-doped SiC-ceramics10.1016/j.actamat.2007.06.037 ↗
28. Core/rim structure of liquid-phase-sintered silicon carbide10.1111/j.1151-2916.1993.tb03677.x ↗
29. New ways of revealing the microstructures of SiC materials10.3139/147.110141 ↗