Microwave dielectric properties of porous Mg2SiO4 filling with TiO2 prepared by a liquid phase deposition process
Source abstract
Abstract
Abstract Forsterite (Mg 2 SiO 4 ) possesses a high quality factor ( Q · f ) of 270,000 GHz and a low dielectric constant ɛ r of 6.8. However, it shows a relatively large negative temperature coefficient of resonant frequency τ f of −73 ppm/°C. For microwave telecommunication, a τ f of nearly 0 ppm/°C is desirable to keep the frequency stability. In order to improve τ f , we have tried to produce pure Mg 2 SiO 4 –TiO 2 composite ceramics with no secondary phases using a liquid phase deposition (LPD) method. Porous Mg 2 SiO 4 ceramics was prepared by sintering Mg 2 SiO 4 with polymethyl methacrylate (PMMA) particles, and then TiO 2 was filled in the pores of Mg 2 SiO 4 by the LPD method. The porosity and microstructure of porous Mg 2 SiO 4 was controlled by amount and particle sizes of PMMA and formation process. τ f of Mg 2 SiO 4 filled with TiO 2 by LPD method was improved to −46 ppm/°C.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Microwave Dielectric Ceramics Synthesis · Ferroelectric and Piezoelectric Materials · Advanced ceramic materials synthesis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (5)
Show source-provided references
1. Zero temperature coefficient τf and sinterability of forsterite ceramics by rutile addition
2. Effects of TiO2 on sinterability and dielectric properties of high-Q forsterite ceramics10.1016/S0955-2219(03)00177-8 ↗
3. Photocatalytic activity of titanium oxide prepared by liquid phase deposition (LPD)10.1039/a801499j ↗
4. Liquid-phase infiltration (LPI) process for the fabrication of highly nano-ordered materials10.1021/cm034846o ↗
5. Hakki · IRE Trans. Microw. Theory Tech. · 1960 · MTT-8 · 40210.1109/TMTT.1960.1124749 ↗