journal article·2017-11

Strength distribution and fracture analyses of LiNbO 3 and LiTaO 3 single crystals under biaxial loading

M. Gruber, I. Kraleva, P. Supancic, J. Bielen, D. Kiener, R. Bermejo

Publisher page

Abstract

Abstract The strength distribution and fracture behaviour of miniaturized Lithium niobate (LiNbO 3 ) and Lithium tantalate (LiTaO 3 ) single crystals were assessed under biaxial bending. The susceptibility of these materials to environmental assisted cracking (SCCG) was studied by means of constant cross-head displacement rate experiments in air and in water. Two different sample sizes were tested and compared to assess the Weibull volume effect. Experimental results showed a significant difference in strength, LiNbO 3 being weaker than LiTaO 3 . No apparent SCCG and no volume effect on strength were found. A different distribution to Weibull behaviour was observed in LiNbO 3 . Fractography showed differences in the fracture patterns, due to the different cutting orientation of the two investigated materials with respect to the loading plane. New cleavage planes were identified as {10.1} for LiNbO 3 and {1 2 ¯ .3} for LiTaO 3 . Fracture surfaces of LiNbO 3 revealed surface damage, which may be responsible for the lower strength compared to LiTaO 3 .
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Ultrasonics and Acoustic Wave Propagation · High-Velocity Impact and Material Behavior · Fatigue and fracture mechanics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (50)

Show source-provided references
1. Hashimoto · 2000
2. Morgan · 2007
3. The temperature coefficients of acoustic surface wave velocity and delay on lithium niobate lithium tantalate, quartz, and tellurium dioxide
4. Surface acoustic waves and SAW materials
5. Hashimoto · 2009
6. Ruppel · 2000
7. Temperature dependence of surface acoustic wave velocity on α quartz10.1063/1.1659311 ↗
8. Optimum cut for rotated Y-cut LiNbO3 crystal used as the substrate of acoustic-surface wave filters10.1109/PROC.1976.10181 ↗
9. Microscale material testing of single crystalline silicon: process effects on surface morphology and tensile strength10.1016/S0924-4247(00)00350-2 ↗
10. Fractographic analysis of very small theta specimens10.4028/www.scientific.net/KEM.409.201 ↗
11. F., Strength distribution of single-crystal silicon theta-like specimens10.1016/j.scriptamat.2010.04.047 ↗
12. Probabilistic strength of 1 1 1 n-type silicon10.1023/A:1008973231053 ↗
13. Biaxial fracture test of silicon wafers10.1002/adem.200400406 ↗
14. Fracture testing at small-length scales: from plasticity in Si to brittleness in Pt10.1007/s11837-015-1489-2 ↗
15. The mechanical strength of polysilicon films: part 1. The influence of fabrication governed surface conditions10.1016/S0022-5096(03)00051-6 ↗
16. Controlling and testing the fracture strength of silicon on the mesoscale10.1111/j.1151-2916.2000.tb01413.x ↗
17. Strength and fracture analysis of silicon-based components for embedding10.1016/j.jeurceramsoc.2010.10.029 ↗
18. Influence of deposited metal structures on the failure mechanisms of silicon-based components10.1016/j.jeurceramsoc.2012.06.027 ↗
19. Fracture of advanced ceramics10.1002/adem.200700347 ↗
20. Direct measurements of the surface energies of crystals10.1063/1.1735524 ↗
21. Cleavage of natural and synthetic single crystal quartz10.1016/0025-5408(87)90134-6 ↗
22. Strength and sharp contact fracture of silicon10.1007/s10853-006-6567-y ↗
23. Orientation dependence of fracture toughness measured by indentation methods and its relation to surface energy in single crystal silicon10.1007/s10704-006-0021-7 ↗
24. Kuz’minov · 1999
25. Volk · 2008
26. Thermal shock cracking of lithium niobate single crystal10.1023/A:1018581710568 ↗
27. Analysis of cracking of lithium tantalate (LiTaO3) single crystals due to thermal stress10.1007/s10853-006-0500-2 ↗
28. Study on the mechanical properties of lithium tantalate and the influence on its machinability
29. Munz · 1999
30. VESTA 3 for three-dimensional visualization of crystal, volumetric and morphology data10.1107/S0021889811038970 ↗
31. Modern crystallography I, symmetry of crystals. Methods of structural crystallography10.1002/crat.2170170316 ↗
32. Lithium niobate: summary of physical properties and crystal structure10.1007/BF00614817 ↗
33. Ferroelectric lithium niobate. 3. Single crystal X-ray diffraction study at 24°C10.1016/0022-3697(66)90072-2 ↗
34. Synchroton X-ray studies of LiNbO3 and LiTaO310.1107/S010876819600777X ↗
35. Temperature dependence of the elastic, piezoelectric, and dielectric constants of lithium tantalate and lithium niobate10.1063/1.1660528 ↗
36. Material constants of LiTaO3 determined from surface acoustic wave velocities10.1143/JJAP.33.2976 ↗
37. Wong · 2002
38. The ball on three balls test for strength testing of brittle discs: stress distribution in the disc10.1016/S0955-2219(01)00458-7 ↗
39. The ball on three balls test for strength testing of brittle discs: part II: analysis of possible errors in the strength determination10.1016/j.jeurceramsoc.2003.10.035 ↗
40. Biaxial tensile strength test for brittle rectangular plates10.2109/jcersj.114.1054 ↗
41. Strength reliability of 3D low temperature co-fired multilayer ceramics under biaxial loading10.1016/j.jeurceramsoc.2010.11.031 ↗
42. Simmons · 1971
43. EN 843-5 · 1997 · 40
44. Subcritical crack growth in low temperature co-fired ceramics under biaxial loading10.1016/j.engfracmech.2012.12.004 ↗
45. Weibull · 1939
46. A general strength distribution function for brittle materials10.1016/0955-2219(92)90021-5 ↗
47. Single crystal cleavage of brittle materials10.1007/BF00012370 ↗
48. Quinn · 2007
49. Towards a deeper understanding of plastic deformation in mono-crystalline silicon10.1016/S0020-7403(01)00024-8 ↗
50. The phenomenon of rupture and flow in solids