journal article·2014-09

The ablation behavior of ZrB2/Cu composite irradiated by high-intensity continuous laser

Zhenyu Yan, Zhuang Ma, Ling Liu, Shizhen Zhu, Lihong Gao

Publisher page

Abstract

Abstract Ultra high temperature ceramics (UHTCs) based composite ZrB 2 /20 vol.% Cu was prepared by spark plasma sintering (SPS) at 1650 C° for 3 min. The ablation behavior of composite irradiated for 2–20 s by 20 MW/m 2 high-intensity continuous laser was investigated. The phase and microstructure evolution of ZrB 2 /20 vol.% Cu during ablation was demonstrated by XRD and SEM, respectively. The results reveal that no macroscopic damage but only one ablated layer with 40 μm in thickness is observed even after being ablated for 20 s. It implies that ZrB 2 /20 vol.% Cu composite exhibits good ablation resistance against high-intensity continuous laser. The continuous Cu in composite evaporates preferentially, which impacts on the following ablation behavior. The generated ZrO 2 at the spot center shows different forms such as closely packed nano-ZrO 2 , micron ZrO 2 or melting ZrO 2 for different ablation time. The melting ZrO 2 is helpful to promote the ablation resistance of ZrB 2 /20 vol.% Cu.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · High-Temperature Coating Behaviors

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (16)

Show source-provided references
1. Evaluation of ultra-high temperature ceramics for aeropropulsion use10.1016/S0955-2219(02)00140-1 ↗
2. Aerothermodynamic study of UHTC-based thermal protection systems10.1016/j.ast.2004.12.003 ↗
3. Material property requirements for analysis and design of UHTC components in hypersonic applications10.1016/j.jeurceramsoc.2010.01.026 ↗
4. Refractory diborides of zirconium and hafnium10.1111/j.1551-2916.2007.01583.x ↗
5. Processing and characterization of ZrB2-based ultra-high temperature monolithic and fibrous monolithic ceramics10.1023/B:JMSC.0000041691.41116.bf ↗
6. Structure evolution of ZrB2-SiC during the oxidation in air10.1557/JMR.2008.0251 ↗
7. Oxidation-based materials selection for 2000 degree C plus hypersonic aerosurfaces: theoretial considerations and historical experience10.1023/B:JMSC.0000041686.21788.77 ↗
8. High temperature oxidation at 1900 degree C of ZrB2-xSiC ultrahigh temperature ceramic composites10.1111/j.1551-2916.2008.02660.x ↗
9. Oxidation resistant ZrB2-SiC composites at 2200 degree C10.1016/j.compscitech.2007.08.017 ↗
10. Toward oxidation resistant ZrB2-SiC ultra high temperature ceramics10.1007/s11661-010-0540-8 ↗
11. Thermal ablation behavior of titanium diboride/(copper, nickel) C4 material10.1016/j.msea.2006.10.072 ↗
12. Plasma wind tunnel testing of ultra high temperature ZrB2-SiC composites under hypersonic re-entry conditions10.1016/j.jeurceramsoc.2010.01.029 ↗
13. The effect of zirconium carbide on ablation of carbon/carbon composites under an oxyacetylene flame10.1016/j.corsci.2010.09.028 ↗
14. Arc-jet testing on HfB2 and HfC-based ultra high temperature ceramic materials10.1016/j.jeurceramsoc.2007.11.021 ↗
15. Zirconia transport by liquid convection during oxidation of zirconium diboride-silicon carbide10.1111/j.1551-2916.2007.02142.x ↗
16. Melting and oxidation behavior of in-flight particles in plasma spray process10.1016/j.ijheatmasstransfer.2005.07.019 ↗