Fabrication of zero-thermal-expansion ZrSiO4/Y2W3O12 sintered body
Source abstract
Abstract
Abstract We focused on the linear negative thermal expansion of Y2W3O12 in a wide-temperature range and on the chemical stability of ZrSiO4 in the fabrication of the composite material ZrSiO4/Y2W3O12 with a zero-thermal-expansion. The compact composed of Y2W3O12 and ZrSiO4 had a thermal shrinkage rate smaller than that of Y2W3O12 and higher than that of ZrSiO4. SEM–EDX observation clarified that the ZrSiO4/Y2W3O12 sintered body fabricated at 1400 °C for 10 h had a microstructure composed of ZrSiO4 and Y2W3O12 grains, and XRD indicated that only ZrSiO4 and Y2W3O12 phases existed in the sintered body. The relative density of the ZrSiO4/Y2W3O12 sintered body reached 92%, which was larger than that of the ZrSiO4 sintered body because Y2W3O12 grains could be sintered at lower temperatures. The average linear thermal expansion coefficients of the ZrSiO4/Y2W3O12 sintered body were −0.4 × 10−6 and −0.08 × 10−6 °C−1 in the temperature ranges from 25 to 500 °C and from 25 to 1000 °C, respectively, which showed an almost zero-thermal-expansion.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Thermal Expansion and Ionic Conductivity · Microwave Dielectric Ceramics Synthesis · Thermodynamic and Structural Properties of Metals and Alloys
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (21)
Show source-provided references
1. Synthesis of ZrO2/ZrW2O8 composites with low thermal expansion10.1016/j.compscitech.2006.05.012 ↗
2. Preparation of dense ZrO2/ZrW2O8 cosintered ceramics with controlled thermal expansion coefficients10.2109/jcersj.112.271 ↗
3. Fracture strength of zero-thermal-expansion glass-ceramics for ultra-precision components10.1016/S0007-8506(07)62113-1 ↗
4. Fabrication of near-zero thermal expansion (FexSc1−x)2Mo3O12–MoO3 ceramic composite using the reaction sintering process10.1016/S0921-5093(00)01906-7 ↗
5. Glass-ceramics with zero thermal expansion in the system BaO/Al2O3/B2O310.1016/j.jnoncrysol.2005.06.013 ↗
6. Glass-ceramics in the system BaO/TiO2(ZrO2)/Al2O3/B2O3 and their thermal expansion10.1016/j.jnoncrysol.2007.03.016 ↗
7. Mechanical and optical properties of silica glass optical fiber with low-expansion glass-ceramic jacket10.2109/jcersj.111.640 ↗
8. ZrW2O8-containing composites with near-zero coefficient of thermal expansion fabricated by various methods: comparison and optimization10.1016/j.compscitech.2008.09.032 ↗
9. Negative thermal expansion in Y2W3O1210.1016/S1466-6049(99)00021-5 ↗
10. X-ray diffraction study of Y2W3O12·3H2O10.1023/A:1012557411736 ↗
11. Structural and thermal expansion properties of solid solution Nd2−xEuxW3O12 (0.0≦×≦0.6 and 1.5≦×≦2.0)10.1016/j.solidstatesciences.2006.02.030 ↗
12. Negative thermal expansion in Sc2(WO4)310.1006/jssc.1998.7744 ↗
13. Enhanced negative thermal expansion in Lu2W3O1210.1006/jssc.1998.7967 ↗
14. Negative thermal expansion materials
15. Synthesis and thermal expansion of ZrO2/ZrW2O8 composites10.1016/j.jeurceramsoc.2004.09.015 ↗
16. Preparation of dense negative-thermal expansion oxide by rapid quenching of ZrW2O8 melt10.2109/jcersj.110.544 ↗
17. Full potential investigations of structural and electronic properties of ZrSiO410.1016/j.mee.2005.03.055 ↗
18. Preparation of zircon bodies from amorphous precursor powder synthesized by sol–gel processing10.1016/S0955-2219(02)00038-9 ↗
19. Hygroscopicity and bulk thermal expansion in Y2W3O1210.1016/j.materresbull.2004.09.009 ↗
20. Dilatometric studies of Y2W3O12 with added Al2O310.1007/BF02708259 ↗
21. Negative thermal expansion in Eu2W3O12 and Yb2W3O12 by high temperature X-ray diffraction10.1016/j.mseb.2004.08.015 ↗