Low temperature preparation and electrical properties of sodium–potassium bismuth titanate lead-free piezoelectric thick films by screen printing
Source abstract
Abstract
Abstract Sodium–potassium bismuth titanate (NKBT) thick films with thickness of 40 μm were prepared by screen printing. To improve the homogeneity, the sintering aids were added into the pastes as a chemical liquid-phase doping method. The results show that the addition of Bi–Li sintering aids was beneficial for both the reduction of the sintering temperature and the improvement of the electrical performance of the thick films. The thick films containing 5 wt.% Bi–Li sintering aids demonstrated optimal dielectric properties with the maximum dielectric constant of 725 and minimum dielectric loss of 2.5%. Moreover, the NKBT thick films containing 3 wt.% Bi–Li sintering aids sintered at 950 °C exhibited the remanent polarization of 19.6 μC/cm 2 , room-temperature pyroelectric coefficient of 1.56 × 10 −4 C/(m 2 °C), figure of merit for specific detectivity of 0.48 × 10 −5 Pa −0.5 , and effective longitudinal piezoelectric coefficient of 88 pm/V, which are comparable to that of the high-temperature sintered thick films without sintering aids.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Ferroelectric and Piezoelectric Materials · Acoustic Wave Resonator Technologies · Microwave Dielectric Ceramics Synthesis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (37)
Show source-provided references
1. Lead-free piezoelectric ceramics of (Bi1/2Na1/2)TiO3–1/2(Bi2O3 Sc2O3) system10.1143/JJAP.36.6055 ↗
2. (Bi1/2 Na1/2)TiO3–BaTiO3 system for lead-free piezoelectric ceramics10.1143/JJAP.30.2236 ↗
3. Large piezoelectric constant and high curie temperature of lead-free piezoelectric ceramic ternary system based on bismuth sodium titanate–bismuth potassium titanate–barium titanate near the morphotropic phase boundary10.1143/JJAP.42.7401 ↗
4. Na0.5Bi0.5TiO3–K0.5Bi0 (NBT–KBT) system: a structural and electrical study10.1002/pssa.2211570234 ↗
5. Dielectric and piezoelectric properties of (Bi0.5Na0.5)TiO3–(Bi0.5K0.5)TiO3 systems10.1143/JJAP.38.5564 ↗
6. Ferroelectric Na0.5Bi0.5TiO3 and K0.5Bi0.5TiO3 perovskites and their solid solutions10.1080/001501990910276 ↗
7. Electrical properties and depolarization temperature of (Bi1/2Na1/2)TiO3–(Bi1/2K1/2)TiO3 lead-free piezoelectric ceramics10.1143/JJAP.45.4493 ↗
8. Electroceramic thick film fabrication for MEMS10.1023/B:JECR.0000033999.74149.a3 ↗
9. Thick-film piezoceramics and devices10.1007/s10832-007-9040-7 ↗
10. Fabrication and characterization of free-standing thick-film piezoelectric cantilevers for energy harvesting10.1088/0957-0233/20/12/124010 ↗
11. Improving the piezoelectric properties of thick-film PZT: the influence of paste composition, powder milling process and electrode material10.1016/j.sna.2003.09.027 ↗
12. Piezoelectric property in morphotropic phase boundary Bi0.5(Na0.82K0.18)0.5TiO3 lead free thick film deposited by screen printing10.1063/1.2911744 ↗
13. Effect of repeated composite sol infiltrations on the dielectric and piezoelectric properties of a Bi0.5(Na0.82K0.18)0.5TiO3 lead free thick film10.1016/j.jeurceramsoc.2008.07.049 ↗
14. Pyroelectric and dielectric properties of Mn modified 0.82Bi0.5Na0.5TiO3–0.18Bi0.5K0.5TiO3 lead-free thick films10.1111/j.1551-2916.2009.03166.x ↗
15. Properties of low temperature sintered neodymium doped lead zirconate titanate ceramics10.1007/BF00271328 ↗
16. Low-temperature sintering of PZT ceramics10.1016/0272-8842(87)90066-6 ↗
17. Effect of simultaneous addition of BiFeO3 and Ba(Cu0.5W0.5)O3 on lowering of sintering temperature of Pb(Zr,Ti)O3 ceramics10.1111/j.1151-2916.1998.tb02439.x ↗
18. Properties of screen-printed lead zirconate titanate piezoelectric thick films on electroded silicon10.1111/j.1151-2916.2001.tb01106.x ↗
19. Dielectric, ferroelectric, and piezoelectric properties of lead zirconate titanate thick films on silicon substrates10.1063/1.358621 ↗
20. A novel micropump design with thick-film piezoelectric actuation10.1088/0957-0233/8/1/008 ↗
21. Screen-printed piezoelectric ceramic thick films with sintering additives introduced through a liquid-phase approach10.1016/j.sna.2004.08.022 ↗
22. Enhancing electrical properties in NBT–KBT lead-free piezoelectric ceramics by optimizing sintering temperature10.1111/j.1551-2916.2008.02469.x ↗
23. Effect of excess Bi2O3 on the electrical properties and microstructure of (Bi1/2Na1/2)TiO3 ceramics10.1007/s00339-003-2350-y ↗
24. Structure electrical properties and temperature characteristics of Bi0.5Na0.5TiO3–Bi0.5K0.5TiO3–Bi0.5Li0.5TiO3 lead-free piezoelectric ceramics10.1007/s00339-008-4667-z ↗
25. Enhanced piezoelectric properties of (Bi0.5K0.5+xLiy)TiO3 ceramics by K nonstoichiometry and Li addition10.1063/1.3081018 ↗
26. Effects of PbO content on the sintering behavior, microstructure, and properties of La-doped PZST antiferroelectric ceramics10.1023/B:JMSE.0000011353.05508.73 ↗
27. Interactions between alumina and PLZT thick films10.1016/S0025-5408(99)00227-5 ↗
28. Interactions between lead oxide and ceramic substrates for thick film technology10.1557/JMR.1997.0072 ↗
29. Preparation of Ba(Ti,Zr)O3 thick films by screen printing10.1143/JJAP.41.6948 ↗
30. Ferroelectric domain morphology evolution and octahedral tilting in lead-free (Bi1/2Na1/2)TiO3–(Bi1/2K1/2)TiO3–(Bi1/2Li1/2)TiO3–BaTiO3 ceramics at different temperatures10.1111/j.1551-2916.2008.02592.x ↗
31. Detection of phase transitions in sodium bismuth titanate–barium titanate single crystals by acoustic emission10.1063/1.2828698 ↗
32. Reinvestigation of phase transitions in Na0.5Bi0.5TiO3 by TEM. Part I: First order rhombohedral to orthorhombic phase transition10.1021/cm8004634 ↗
33. Reinvestigation of phase transitions in Na0.5Bi0.5TiO3 by TEM. Part II: Second order orthorhombic to tetragonal phase transition10.1021/cm800464d ↗
34. Effects of manganese addition on pyroelectric properties of (Bi0.5Na0.5TiO3)0.94(BaTiO3)0.06 ceramics10.1080/10584580600656502 ↗
35. Dorey RA, Whatmore RW. Pyroelectric PZT/PMNZTU composite thick films. J Eur Ceram Soc 2005;25:2379–82.10.1016/j.jeurceramsoc.2005.03.060 ↗
36. Nonlinear local piezoelectric deformation in ferroelectric thin films studied by scanning force microscopy10.1063/1.1891273 ↗
37. Stress and frequency dependence of the direct piezoelectric effect in ferroelectric ceramics10.1063/1.365981 ↗