journal article·2016-01Open access

Hydrofluoric acid etching of dental zirconia. Part 2: effect on flexural strength and ageing behavior

Quentin Flamant, Marc Anglada

Abstract

Among the diverse treatments proposed to promote the osseointegration of zirconia dental implants, hydrofluoric acid (HF) etching appears to be a good candidate. However little is known on the effect of this process on the mechanical properties and long-term reliability. In this work, the surface integrity, the flexural strength and the ageing sensitivity of yttria-stabilized zirconia were assessed after etching in HF 40%. Results show that etching induces an increase of monoclinic phase content and a decrease in flexural strength. The strength decrease is limited to 15% for etching times below 60 min, whereas it reaches 29% after 120 min because of the formation of large etching pits. No substantial change in the ageing sensitivity was evidenced. Within the limits of this study, HF 40% etched zirconia appears to be reliable for long-term implantation provided that the etching duration does not exceed 60 mm. (C) 2015 Elsevier Ltd. All rights reserved.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Dental materials and restorations · Dental Implant Techniques and Outcomes · Bone Tissue Engineering Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (29)

Show source-provided references
1. What future for zirconia as a biomaterial?10.1016/j.biomaterials.2005.07.034 ↗
2. Ceramic steel?10.1038/258703a0 ↗
3. Environmental degradation of zirconia ceramics10.1016/0955-2219(95)00035-S ↗
4. State of the art of zirconia for dental applications10.1016/j.dental.2007.05.007 ↗
5. Fracture strength of zirconia implants after artificial aging10.1111/j.1708-8208.2008.00105.x ↗
6. Ceramic implants (Y-TZP): are they a viable alternative to titanium implants for the support of overdentures? A randomized clinical trial10.1111/clr.12272 ↗
7. One-piece zirconia oral implants: one-year results from a prospective cohort study. 1. Single tooth replacement10.1111/j.1600-051X.2012.01876.x ↗
8. On implant surfaces: a review of current knowledge and opinions
9. A comparison study of the osseointegration of zirconia and titanium dental implants. A biomechanical evaluation in the maxilla of pigs10.1111/j.1708-8208.2009.00168.x ↗
10. Response of osteoblast-like cells to zirconia with different surface topography10.4012/dmj.2012-208 ↗
11. Microstructured zirconia surfaces modulate osteogenic marker genes in human primary osteoblasts10.1007/s10856-014-5350-x ↗
12. Hydrofluoric acid etching of dental zirconia. Part 1: etching mechanism and surface characterization10.1016/j.jeurceramsoc.2015.09.021 ↗
13. Five-year success rate of 831 consecutively placed Zirconia dental implants in humans: a comparison of three different rough surfaces
14. A new testing protocol for zirconia dental implants10.1016/j.dental.2014.09.002 ↗
15. Low-temperature aging of Y-TZP ceramics10.1111/j.1151-2916.1999.tb02055.x ↗
16. Calibration curve for quantitative analysis of the monoclinic–tetragonal ZrO2 system by X-ray diffraction10.1111/j.1151-2916.1984.tb19614.x ↗
17. The ball on three balls test for strength testing of brittle discs: stress distribution in the disc10.1016/S0955-2219(01)00458-7 ↗
18. Effect of coloring with various metal oxides on the microstructure, color, and flexural strength of 3Y-TZP10.1002/jbm.b.31107 ↗
19. Munz · 1999 · 36
20. Wet Chemical Etching of Silicon {111}: autocatalysis in pit formation10.1149/1.2830841 ↗
21. Fracture toughness of zirconia from a shallow notch produced by ultra-short pulsed laser ablation10.1016/j.jeurceramsoc.2014.05.009 ↗
22. Generalized orowan-petch plot for brittle fracture10.1111/j.1151-2916.1998.tb02657.x ↗
23. In vitro aging of yttria-stabilized zirconia10.1111/j.1151-2916.1989.tb06194.x ↗
24. Transformation-toughened zirconia for dental inlays, crowns and bridges: chemical stability and effect of low-temperature aging on flexural strength and surface structure10.1016/S0109-5641(01)00095-1 ↗
25. The effect of low temperature aging on the mechanical property & phase stability of Y-TZP ceramics10.4047/jap.2009.1.3.113 ↗
26. Low-temperature degradation of different zirconia ceramics for dental applications10.1016/j.actbio.2011.11.016 ↗
27. Weibull strength statistics of hydrothermally aged 3 mol% yttria-stabilised tetragonal zirconia10.1016/j.ceramint.2014.04.131 ↗
28. Strengthening of Vickers indented 3Y-TZP by hydrothermal ageing10.1016/j.jeurceramsoc.2011.08.019 ↗
29. Reinforcement by crack-tip blunting in porous ceramics10.1016/S0955-2219(03)00365-0 ↗