Degradation mechanisms of SiC/BN/SiC after low temperature humidity exposure
Source abstract
Abstract
The environmental degradation of SiC/BN/SiC CMCs under low temperature water exposure is still an unexplored field. This work shows how the effect of low temperature humid environments can be detrimental for amorphous BN interfaces, leading to a drop in mechanical properties. Furthermore, initial low-temperature humid environments can induce a faster degradation during subsequent thermal exposure. In order to understand how low temperature water exposure affects the CMC and how these changes affect the material response to subsequent exposures, intermediate temperature (800°C) exposures have been studied before and after the low temperature humidity tests. The main challenge of this work consists of understanding how different constituents of the CMC structure (e.g. fibres and interfaces) are degrading and consequently affecting the overall bulk mechanical performance and failure modes of the material. For this, linking the change in morphology and chemistry of the interfaces with the micromechanical properties of the individual constituents has been crucial. STEM-EDS has shown a change in morphology of the BN interface after the low temperature water exposure, which has been linked to a decrease in interfacial shear strength and friction (measured via in-situ fibre push-out tests) of ≈ 90%. STEM-EELS has shown how, after the interfaces have been exposed to the humidity as well as to subsequent intermediate temperatures in the presence of the remaining BN, induces degradation of the SiC fibres which results in a tensile strength reduction of ≈ 25% (measured via in-situ 3-point bending of individual fibres). These results provide a new insight into how low temperature water exposures must be considered in future degradation studies of CMCs. Additionally, we propose a new methodology to fundamentally understand the complex failure modes of CMCs.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Aluminum Alloys Composites Properties · Silicon Carbide Semiconductor Technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (51)
Show source-provided references
1. Ceramic matrix composites
2. The mechanics of matrix cracking in brittle-matrix10.1016/0001-6160(85)90124-5 ↗
3. The mechanical properties of reinforced ceramic, metal and intermetallic matrix composites10.1016/0921-5093(91)90726-4 ↗
4. Ceramics and ceramic composites as high-temperature structural materials: challenges and opportunities
5. Aeroengine composites, part 1: the CMC invasion
6. Ceramic matrix composites taking flight at GE aviation
7. Influence of the interphase and associated interfaces on the deflection of matrix cracks in ceramic matrix composites10.1016/S1359-835X(00)00095-6 ↗
8. Interfacial characterization of a slurry-cast melt-infiltrated SiC/SiC ceramic-matrix composite10.1016/S1359-6454(00)00248-2 ↗
9. Concept of a strong interface applied to SiC/SiC composites with a BN interphase10.1016/S1359-6454(00)00247-0 ↗
10. Boron nitride interphase in ceramic-matrix composites10.1111/j.1151-2916.1991.tb06789.x ↗
11. Tensile stress rupture of SiCf/SiCm minicomposites with carbon and boron nitride interphases at elevated temperatures in air10.1111/j.1151-2916.1997.tb03087.x ↗
12. Evaluating the effect of oxygen content in BN interfacial coatings on the stability of SiC/BN/SiC composites10.1016/S1359-835X(98)00135-3 ↗
13. Intermediate-temperature stress rupture of a woven hi-nicalon, BN-Interphase, SiC-Matrix composite in air
14. Fatigue and stress-rupture behaviors of SiC / SiC composite under humid environment at elevated temperature10.1016/j.compscitech.2006.02.013 ↗
15. High‐temperature stability of SiC‐Based composites in high‐water‐Vapor‐Pressure environments10.1111/j.1151-2916.2003.tb03463.x ↗
16. Borosilicate glass-induced Fiber degradation of SiC/BN/SiC composites exposed in combustion environments10.1111/ijac.12499 ↗
17. Fatigue behavior of sylramic-iBN/BN/CVI SiC ceramic matrix composite in combustion environment10.1007/s10853-015-9302-8 ↗
18. High temperature oxidation of ceramic composites10.1351/pac199870020493 ↗
19. Synthesis and structure of chemically vapour-deposited boron nitride10.1007/BF01145537 ↗
20. High-Temperature Oxidation of Boron Nitride: II, Boron Nitride Layers in Composites
21. Degradation of boron nitride interfacial coatings fabricated by chemical vapor infiltration on SiC fibers under ambient air/room temperature conditions10.1016/j.ceramint.2018.12.191 ↗
22. Analyses on fiber push-out tests performed on Nicalon/SiC composites with tailored interfaces10.1016/0961-9526(95)99801-A ↗
23. Ceramic composites: A review of toughening mechanisms and demonstration of micropillar compression for interface property extraction10.1557/jmr.2017.473 ↗
24. Linking microstructure and local mechanical properties in SiC-SiC fiber composite using micromechanical testing10.1016/j.actamat.2019.02.001 ↗
25. Strengths of ceramic fiber bundles: theory and practice10.1111/jace.15062 ↗
26. Weibull parameters obtained from dependence of fiber strength on fiber length and area10.1111/jace.15709 ↗
27. Oxidation kinetics strength of Hi-NicalonTM-S SiC fiber after oxidation in dry and wet air10.1111/jace.14833 ↗
28. Model for SiC fiber strength after oxidation in dry and wet air10.1111/jace.15907 ↗
29. Micromechanical strength of individual Al2O3 platelets10.1016/j.scriptamat.2017.01.008 ↗
30. Microscopic strength of silicon particles in an aluminium-silicon alloy10.1016/j.actamat.2015.12.006 ↗
31. Light and strong SiC networks10.1002/adfm.201504051 ↗
32. On understanding the microstructure of SiC/SiC Ceramic Matrix Composites (CMCs) after a material removal process10.1016/j.msea.2018.11.037 ↗
33. Effects of Heat - treatment on the microstructure and
34. Interfaces and interfacial mechanics: influence on the mechanical behavior of ceramic matrix composites (CMC)
35. HRTEM and EELS studies on the amorphization of hexagonal boron nitride induced by ball milling10.1111/j.1151-2916.2000.tb01204.x ↗
36. Wilson · 2018
37. Knauf · 2017
38. A review of SiC fiber oxidation with a new study of hi-nicalon SiC fiber oxidation10.1002/adem.201600166 ↗
39. Silicon carbide fiber oxidation behavior in the presence of boron nitride
40. “Nist.” [Online]. Available: https://srdata.nist.gov/xps/main_search_menu.aspx. [Accessed: 12-May-2019].
41. Interfacial bond strength in SiC / C / SiC composite materials, as studied by single-fiber push-out tests
42. Influence of interfaces and interphases on the mechanical behavior of fiber-reinforced ceramic matrix composites
43. Statistically sound application of fiber push-out method for the study of locally non-uniform interfacial properties of SiC-SiC fiber composites10.1016/j.jeurceramsoc.2019.11.041 ↗
44. Origin and characterization of different stick−slip friction mechanisms †10.1021/la950896z ↗
45. Effect of interfacial roughness on the frictional stress measured using pushout tests10.1111/j.1151-2916.1991.tb06845.x ↗
46. Recent developments of the SiC fiber Nicalon and its composites, including properties of the SiC fiber Hi Nicalon for ultra-high temperature10.1016/0266-3538(94)90184-8 ↗
47. Characterization of nearly stoichiometric SiC ceramic fibres10.1023/A:1017988827616 ↗
48. A review of the development of three generations of small diameter silicon carbide fibres10.1007/s10853-006-6566-z ↗
49. FactSage Thermochemical software and databases10.1016/S0364-5916(02)00035-4 ↗
50. The Kelvin equation and capillary condensation10.1038/290575a0 ↗
51. The application of in situ analytical transmission electron microscopy to the study of preferential intergranular oxidation in Alloy 60010.1016/j.ultramic.2016.11.014 ↗