journal article·2021-12

Evolution of microstructure and tensile strength of Cansas-II SiC fibers under air oxidizing atmosphere

Xihui Chen, Zhigang Sun, Xiao Han, Xuming Niu, Yingdong Song

Publisher page

Abstract

Abstract The influence of oxidation on the microstructure and tensile strength of Cansas-II SiC fibers at 900–1500 ℃ in the air was investigated in depth. The growth of β-SiC grains ordering as well as the increase of the size of free carbon in the SiC core occurred due to the thermal exposure. The thickness of the amorphous SiO2 layer increases with the temperature, starting to transform to cristobalite at 1200 ℃. The activation energy in the ambient air is determined as 148KJ/mol, similar to that of Hi-Niaclon fibers (107∼151 KJ/mol). With the growth of the SiO2 layer, lots of bubbles appeared in the SiO2 layer due to the release of excess CO gas. Moreover, many cracks occurred on the fiber surface caused by the residual stress. The mean tensile strength decreased from initial 2.7 GPa to 0.3 GPa after the treatment at 1500 ℃, which could be mainly attributed to the SiO2 layer.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Diamond and Carbon-based Materials Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (57)

Show source-provided references
1. Design, preparation and properties of non-oxide CMCs for application in engines and nuclear reactors: an overview10.1016/S0266-3538(03)00230-6 ↗
2. Preparation and characterization of SiC fibers with diverse electrical resistivity through pyrolysis under reactive atmospheres10.1016/j.jeurceramsoc.2016.09.023 ↗
3. Mechanical properties and in situ crack growth observation of SiC/SiC composites10.1016/j.ceramint.2013.12.098 ↗
4. Tension-tension fatigue behavior of a PIP SiC/SiC composite at elevated temperature in air10.1016/j.ceramint.2015.10.116 ↗
5. Effects of temperature and atmosphere on microstructural evolution and mechanical properties of KD-II SiC fibers10.1016/j.ceramint.2020.06.225 ↗
6. Damage and failure of SiC fiber tows during environment activated slow crack growth: residual behavior and Strength-Probability-Time diagrams10.1016/j.actamat.2017.03.073 ↗
7. Development of a silicon carbide fibre with high tensile strength10.1038/261683a0 ↗
8. A review of the development of three generations of small diameter silicon carbide fibres10.1007/s10853-006-6566-z ↗
9. On the thermal degradation of lox-M tyranno® fibres10.1016/0955-2219(95)00004-E ↗
10. Thermal stability of SiC fiber prepared by an irradiation- curing process10.1016/S0266-3538(99)00010-X ↗
11. High-strength alkali-resistant sintered SiC fibre stable to 2,200 °C10.1038/35820 ↗
12. Microstructure and mechanical properties of Hi-NicalonTM Type S fibers annealed and crept in various oxygen partial pressures10.1016/j.matchar.2009.01.017 ↗
13. Effect of heat treatment on the microstructure and tensile strength of KD-II SiC fibers10.1016/j.msea.2016.07.066 ↗
14. Effect of frequency and environment on fatigue behavior of a CVI SiC/SiC ceramic matrix composite at 1200°C10.1016/j.compscitech.2010.11.008 ↗
15. Thermal and mechanical stabilities of Hi-Nicalon SiC fiber under annealing and creep in various oxygen partial pressures10.1016/j.corsci.2008.08.003 ↗
16. Degradation mechanism of amorphous silicon carbide Fiber due to air-exposure at high temperatures10.2320/matertrans.48.111 ↗
17. Kinetics of passive oxidation of Hi-Nicalon-S SiC fibers in wet air: relationships between SiO2 scale thickness, crystallization, and Fiber strength
18. Model for SiC fiber strength after oxidation in dry and wet air10.1111/jace.15907 ↗
19. Microstructure and oxidation behavior of silicon carbide fibers derived from Polycarbosilane10.1111/j.1151-2916.2000.tb01350.x ↗
20. Decomposition and oxidation resistance of Si-M(Ti, Zr)-C-O fibers at elevated temperature
21. Thermal behaviour of a polytitanocarbosilane-derived fibre with a low oxygen content: the Tyranno Lox-E fibre10.1023/A:1004395308173 ↗
22. SiC-based ceramic fibres : thermal stability and oxidation behaviour10.4028/www.scientific.net/KEM.132-136.1950 ↗
23. Fast parallel algorithms for short-range molecular dynamics10.1006/jcph.1995.1039 ↗
24. Mechanical size effects of amorphous polymer-derived ceramics at the nanoscale: experiments and ReaxFF simulations10.1039/C9NR00958B ↗
25. Determination of residual stresses in SiC monofilament reinforced metal-matrix composites using Raman spectroscopy10.1016/S1359-835X(02)00157-4 ↗
26. Interpretation of Raman spectra of disordered and amorphous carbon10.1103/PhysRevB.61.14095 ↗
27. Silicon oxycarbide formation on SiC surfaces and at the SiC/SiO2 interface10.1116/1.580951 ↗
28. Oxidation behavior of Si3N4 fibers derived from polycarbosilane10.1016/j.corsci.2018.02.032 ↗
29. Hi-NicalonTM-S SiC Fiber oxidation and scale crystallization kinetics10.1111/j.1551-2916.2011.04647.x ↗
30. Oxidation behavior of Hi-Nicalon SiC monofilament fibres in air and O2-H2O-Ar atmospheres10.1016/j.corsci.2011.12.019 ↗
31. Electron irradiation induced crystalline-to-amorphous transition in quartz single crystals10.1016/0022-3093(90)91039-T ↗
32. The oxidation of Silicon in dry oxygen, wet oxygen and steam
33. Thermal stability of a PCS-derived SiC fibre with a low oxygen content (Hi-Nicalon)10.1023/A:1018541030308 ↗
34. Effect of composition and heat treatment conditions on the tensile strength and creep resistance of SiC-based fibers10.1016/S0955-2219(99)00114-4 ↗
35. Numerical modeling of oxidized C/SiC microcomposite in air oxidizing environments below 800°C: microstructure and mechanical behavior10.1016/j.jeurceramsoc.2015.05.039 ↗
36. Review of SiCf/SiCm corrosion, erosion and erosion-corrosion in high temperature helium relevant to GFR conditions
37. Effect of water vapor on the oxidation of hot-pressed silicon nitride and Silicon Carbide10.1111/j.1151-2916.1976.tb09398.x ↗
38. Oxidation of silicon carbide in a wet atmosphere10.1007/BF01106816 ↗
39. Intrinsic strain in SiO2 thin films10.1063/1.366759 ↗
40. High temperature oxidation of SiC under helium with low-pressure oxygen. Part 2: CVD β-SiC10.1016/j.jeurceramsoc.2010.04.031 ↗
41. Active oxidation of SiC10.1007/s11085-010-9216-4 ↗
42. General relationship for the thermal oxidation of Silicon10.1063/1.1713945 ↗
43. A review of SiC Fiber oxidation with a new study of hi-nicalon SiC Fiber oxidation10.1002/adem.201600166 ↗
44. Monazite coatings on SiC fibers II: oxidation protection10.1111/j.1551-2916.2006.01241.x ↗
45. Si-C-N ceramics with a high microstructural stability elaborated from the pyrolysis of new polycarbosilazane precursors10.1007/BF00354712 ↗
46. Oxidation kinetics of silicon carbide crystals and ceramics: I, in dry oxygen10.1111/j.1151-2916.1986.tb07470.x ↗
47. Oxidation mechanisms and kinetics of SiC-matrix composites and their constituents10.1023/B:JMSC.0000048745.18938.d5 ↗
48. Variation of the oxidation rate of Silicon Carbide with water-vapor pressure10.1111/j.1151-2916.1999.tb01810.x ↗
49. Oxidation of nicalon SiC fibres10.1007/BF00609170 ↗
50. Oxidation kinetics of low-oxygen silicon carbide fiber10.1023/A:1004883607913 ↗
51. Oxidation behavior and thermal stability of Si-C-O fibers (Nicalon) in carbon dioxide10.1023/A:1016162428932 ↗
52. Passive-Oxidation Kinetics of High-purity Silicon Carbide from 800° to 1100°C10.1111/j.1151-2916.1996.tb08724.x ↗
53. A comparison of the oxidation kinetics of SiC and Si3 N 410.1149/1.2048559 ↗
54. Structural evolution and mechanical properties of Cansas-III SiC fibers after thermal treatment up to 1700 °C
55. ReaxFF molecular dynamics simulation of oxidation behavior of 3C-SiC in O2 and CO210.1016/j.commatsci.2021.110341 ↗
56. Evolution of the structure and mechanical performance of Cansas-II SiC fibres after thermal treatment
57. The effect of heat treatment on the microstructure and mechanical properties of KD-II SiC fibers in air10.4028/www.scientific.net/KEM.726.132 ↗