Microstructural evolution of a commercial ultrafine alumina powder densified by different methods

Farhad Golestani-fard, Mehdi Mazaheri, Masoud Aminzare, T. Ebadzadeh

Abstract

The densification and grain growth of bodies made from a commercial ultrafine alumina powder was investigated. The primary powder was initially subjected to dry (uniaxial cold pressing) and wet shaping (slip casting), followed by conventional (CS)-, two step (TSS)-, and microwave (MS) sintering to explore the effect of each series of treatments on the densification and microstructural evolution of the specimens. It was demonstrated that a uniform microstructure with higher density would be obtained using the wet shaping method. In addition, microwave sintering was found to be more effective into the densification of the specimens and in yielding a finer grain structure. It is believed that the high heating rate and effective particle packing are responsible for the improvements in these properties. On this basis, it was also demonstrated that the fracture toughness of the samples increased significantly through the application of microwave sintering. (C) 2010 Elsevier Ltd. All rights reserved.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Intermetallics and Advanced Alloy Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (22)

Show source-provided references
1. Kang · 2005
2. Rahaman · 2003
3. Effects of the homogeneity of particle coordination on solid-state sintering of transparent alumina10.1111/j.1551-2916.2006.00985.x ↗
4. The influence of shaping method on the grain size dependence of strength in dense submicrometre alumina10.1016/0955-2219(96)00044-1 ↗
5. Processing of high-density submicrometer Al2O3 for new applications10.1111/j.1151-2916.2003.tb03339.x ↗
6. Sintering behavior of an ultrafine alumina powder shaped by pressure filtration and dry pressing10.1016/j.msea.2010.03.051 ↗
7. Sintering behavior of nano alumina powder shaped by pressure filtration10.1016/j.ceramint.2010.07.027 ↗
8. Hot pressing of nanocrystalline zinc oxide compacts: densification and grain growth during sintering10.1016/j.ceramint.2008.04.015 ↗
9. Sintering dense nanocrystalline oxide with-out final stage grain growth10.1038/35004548 ↗
10. Two-step sintering of nanocrystalline 8Y2O3 stabilized ZrO2 synthesized by glycine nitrate10.1016/j.ceramint.2007.09.009 ↗
11. Densification and grain growth of nanocrystalline 3Y-TZP during two-step sintering10.1016/j.jeurceramsoc.2008.04.030 ↗
12. Two-step sintering of nanocrystalline ZnO compacts: effect of temperature on densification and grain growth10.1111/j.1551-2916.2007.02029.x ↗
13. Processing of nanocrystalline 8mol% yttria-stabilized zirconia by conventional, microwave-assisted and two-step sintering10.1016/j.msea.2008.03.023 ↗
14. Microwave-assisted synthesis and sintering of mullite10.1016/j.ceramint.2009.05.013 ↗
15. Suppression of grain growth in sub-micrometer alumina via two-step sintering method10.1016/j.jeurceramsoc.2008.08.027 ↗
16. The effect of conformation method and sintering technique on the densification and grain growth of nanocrystalline 8mol% yttria-stabilized zirconia10.1111/j.1551-2916.2009.02959.x ↗
17. Low-temperature sintering and mechanical property evaluation of nanocrystalline 8mol% yttria fully stabilized zirconia10.1111/j.1551-2916.2007.01683.x ↗
18. Evidence for the microwave effect during hybrid sintering10.1111/j.1551-2916.2006.00976.x ↗
19. Microstructure and nonlinear properties of microwave-sintered ZnO–V2O5 varistors. II. Effect of Mn3O4 doping10.1111/j.1151-2916.1998.tb02718.x ↗
20. Microstructure and nonlinear properties of microwave-sintered ZnO–V2O5 varistors. I. Effect of V2O5 doping10.1111/j.1151-2916.1998.tb02717.x ↗
21. Two-step sintering of titania nanoceramics assisted by anatase-to-rutile phase transformation10.1016/j.scriptamat.2008.02.041 ↗
22. Fracture toughness of nanocrystalline ZrO2–3mol% Y2O3 determined by Vickers indentation10.1016/1359-6462(95)00587-0 ↗