Abstract
Abstract Varistor ceramics were prepared by spark plasma sintering (SPS) using two doped zinc oxide based powders. Optimized sintering cycle for the commercial powder (mixture of oxides) yielded dense parts (>99%) containing mainly ZnO grains (1 μm) and additional Bi 2 O 3 and Zn 7 Sb 2 O 12 oxides. Sintering at the low oxygen partial pressure inherent to SPS leads to the reduction of Bi 2 O 3 into metallic Bi. To reduce the grain size, improve the distribution of dopants and the grain size distribution, we used co-precipitation to synthesize a powder with the same formulation as the commercial powder. Due to the high reactivity of this powder, fully dense parts were obtained at temperature as low as 400 °C under air atmosphere using carbide tools. Such conditions led to limited ZnO grain growth and bismuth reduction during the thermal cycle. The fine microstructure obtained led to varistances with to high electrical properties (threshold field higher than 2300 V/mm).
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: ZnO doping and properties · High-Temperature Coating Behaviors · Transition Metal Oxide Nanomaterials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (21)
Show source-provided references
1. Theory of conduction in ZnO varistors10.1063/1.326191 ↗
2. The grain junction in zinc oxide varistors
3. Statistics and grain size in zinc oxide varistors10.1063/1.325882 ↗
4. Application of zinc oxide varistors10.1111/j.1151-2916.1990.tb05232.x ↗
5. Voronoi network model of ZnO varistors with different types of grain boundaries10.1063/1.363645 ↗
6. A comprehensive review of ZnO materials and devices10.1063/1.1992666 ↗
7. Sintering and densification of nanocrustalline ceramic oxide powders. A review10.1179/174367508X297812 ↗
8. Shaping of nanostructured materials or coatings through spark plasma sintering
9. Densification and preservation of the ceramic nanocrystalline character by spark plasma sintering10.1179/1743676111Y.0000000074 ↗
10. Consolidation/synthesis of materials by electric current activated/assisted sintering10.1016/j.mser.2008.09.003 ↗
11. Fabrication and characterization of polycrystalline bulk ZnO with large grain size of similar to 100 mu m by the spark plasma sintering10.1002/pssc.200564711 ↗
12. Observation of internal pulsed current flow through the ZnO specimen in the spark plasma sintering method10.1007/s10853-008-2906-5 ↗
13. Influence of texture on electrical properties of ZnO ceramics prepared by extrusion and spark plasma sintering10.1016/j.ceramint.2005.08.005 ↗
14. Size effect on properties of varistors made from zinc oxide nanoparticles through low temperature spark plasma sintering10.1002/adfm.200801067 ↗
15. Nonohmic characteristics of ZnO–V2O5 ceramics10.1063/1.357254 ↗
16. Electrical properties of grain boundaries in polycrystalline compound semiconductors10.1088/0268-1242/5/2/001 ↗
17. Processing strategies to control grain growth in ZnO based varistors10.1016/j.jeurceramsoc.2005.03.175 ↗
18. Effects of cobalt doping on nonlinearity of zinc oxide10.1016/j.mseb.2006.02.058 ↗
19. The electrical properties of Mn2O3 doped ZnO10.1016/j.ceramint.2003.12.028 ↗
20. Mory JE, Guy I, Schneider D, Rousset A, Legros R, Peigney A. Doped zinc oxide powder, preparation thereo and ceramic produced there from. Patent WO1994022765 A1. 1994.
21. Thermal evolution of ZnO–Bi2O3–Sb2O3 system in the region of interest varistors10.1007/s10853-006-7168-5 ↗