journal article·2006-01

Yb2O3 and Y2O3 co-doped zirconia ceramics

Yanmei Kan, Guojun Zhang, Peiling Wang, Omer Van der Biest, Jef Vleugels

Publisher page

Abstract

Abstract A suspension stabilizer-coating technique was employed to prepare x mol% Yb 2 O 3 ( x = 1.0, 2.0, 3.0 and 4.0) and 1.0 mol% Y 2 O 3 co-doped ZrO 2 powder. A systematic study was conducted on the sintering behaviour, phase assemblage, microstructural development and mechanical properties of Yb 2 O 3 and Y 2 O 3 co-doped zirconia ceramics. Fully dense ZrO 2 ceramics were obtained by means of pressureless sintering in air for 1 h at 1450 °C. The phase composition of the ceramics could be controlled by tuning the Yb 2 O 3 content and the sintering parameters. Polycrystalline tetragonal ZrO 2 (TZP) and fully stabilised cubic ZrO 2 (FSZ) were achieved in the 1.0 mol% Y 2 O 3 stabilised ceramic, co-doped with 1.0 mol% Yb 2 O 3 and 4.0 mol% Yb 2 O 3 , respectively. The amount of stabilizer needed to form cubic ZrO 2 phase in the Yb 2 O 3 and Y 2 O 3 co-doped ZrO 2 ceramics was lower than that of single phase Y 2 O 3 -doped materials. The indentation fracture toughness could be tailored up to 8.5 MPa m 1/2 in combination with a hardness of 12 GPa by sintering a 1.0 mol% Yb 2 O 3 and 1.0 mol% Y 2 O 3 ceramic at 1450 °C for 1 h.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Microwave Dielectric Ceramics Synthesis · Semiconductor materials and devices

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (18)

Show source-provided references
1. Quantitative characterization of various tetragonal zirconia polycrystals (TZPs)10.1016/S0955-2219(01)00261-8 ↗
2. Mechanical properties of toughened ZrO2–Y2O3 ceramics10.1111/j.1151-2916.1986.tb04823.x ↗
3. Mechanical properties and microstructure for 3mol% yttria doped zirconia/silicon carbide nanocomposites10.1016/S0955-2219(02)00168-1 ↗
4. Characterization of the electrical properties of Y2O3-doped CeO2-rich CeO2–ZrO2 solid solutions10.1016/j.ssi.2003.10.001 ↗
5. Influence of microstructure on the ionic conductivity of yttria-stabilized zirconia electrolyte10.1016/S0921-5093(01)01935-9 ↗
6. Ionic conductivity of yttrium-doped zirconia and the composite effect10.1016/0167-2738(95)00137-U ↗
7. Mechanical properties of Y2O3/Al2O3-coated Y-TZP ceramics10.1016/S0955-2219(01)00389-2 ↗
8. Effect of Y2O3 content on cavity formation in ZrO2-based ceramics10.1016/S0167-577X(02)00859-5 ↗
9. Fabrication and characterization of (Nd, Y)-TZP ceramics from stabilizer-coated nanopowder10.1016/j.matlet.2004.05.078 ↗
10. Emerging materials and process for thermal barrier systems10.1016/j.cossms.2004.03.009 ↗
11. Effect of heat treatment on grain size, phase assemblage, and mechanical properties of 3mol% Y-TZP10.1111/j.1151-2916.1996.tb08980.x ↗
12. Transformation toughening in zirconia-containing ceramics10.1111/j.1151-2916.2000.tb01221.x ↗
13. Synthesis and characterisation of CeO2-coated ZrO2 powder-based TZP10.1016/S0167-577X(00)00180-4 ↗
14. Sintering microstructure and mechanical properties of commercial Y-TZPs10.1007/BF01152158 ↗
15. A critical evaluation of indentation techniques for measuring fracture toughness: I. Direct crack measurements10.1111/j.1151-2916.1981.tb10320.x ↗
16. Calibration curve for quantitative analysis of the monoclinic–tetragonal ZrO2 system by X-ray diffraction10.1111/j.1151-2916.1984.tb19614.x ↗
17. Metastable crystallization, phase partitioning, and grain growth of ZrO2–Gd2O3 materials processed from liquid precursors10.1111/j.1151-2916.1991.tb06844.x ↗
18. Role of cerium–zirconium mixed oxides as catalysts for car pollution: A short review10.1016/S0925-8388(98)00477-0 ↗