journal article·2008-01

Oxidation behaviour of Si3N4/Y2O3 system ceramics and effect of crack-healing treatment on oxidation

M. Nakatani, K. Ando, K. Houjou

Publisher page

Abstract

Abstract This paper describes the oxidation behaviour of Si 3 N 4 /Y 2 O 3 -based ceramics. We prepared three kinds of ceramics, which have excellent crack-healing abilities, in different composites – Si 3 N 4 /Y 2 O 3 , Si 3 N 4 /SiC/Y 2 O 3 , and Si 3 N 4 /Y 2 O 3 /Al 2 O 3 – and investigated the effect of crack-healing treatment on their oxidation behaviour. The oxidation tests were carried out at 700–1200 °C for 500 h. Measurements of weight gain and bending strength and observations of the oxidized surfaces were carried out. The main results obtained are as follows: (1) when Y 2 O 3 was used as an additive, Si 3 N 4 ceramics exhibited extensive oxidation at low temperatures (700–1000 °C). (2) Si 3 N 4 /Y 2 O 3 ceramics with 3-wt% Al 2 O 3 added as an additive showed no extensive oxidation. (3) Crack-healing, as a pre-oxidation treatment, is useful for increasing the oxidation–resistance of ceramics at 1000 °C and for increasing the strength.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Recycling and utilization of industrial and municipal waste in materials production

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (10)

Show source-provided references
1. Crack healing in a silicon nitride ceramics10.1111/j.1151-2916.1998.tb02558.x ↗
2. Crack-healing behavior of Si3N4/SiC ceramics under stress and fatigue strength at the temperature of healing (1000°C)10.1016/S0955-2219(01)00435-6 ↗
3. (Crack-healing+proof test): a new methodology to guarantee the structural integrity of a ceramics components10.1016/S0955-2219(01)00236-9 ↗
4. Crack-healing and oxidation behavior of silicon nitride ceramics10.1016/S0955-2219(03)00645-9 ↗
5. Effect of sintering additives on the oxidation behavior of Si3N4 ceramics at 1300°C10.1016/j.jeurceramsoc.2004.03.023 ↗
6. Phase relations and stability studies in the Si3N4–Y2O3–SiO2 pseudoternary system10.1111/j.1151-2916.1977.tb14118.x ↗
7. The low-temperature oxidation problem in yttria-densified silicon nitride ceramics
8. Abnormal oxidation behavior of Si3N4–SiC–Y2O3 composite at about 1000°C10.2109/jcersj.105.31 ↗
9. Improvement of static fatigue strength of Si3N4/SiC crack-healed under cyclic stress10.1016/j.jeurceramsoc.2004.06.010 ↗
10. Importance of phase equilibria on process control of Si3N4 fabrication10.1007/978-1-4684-3965-6_15 ↗