Stress–corrosion cracking by indentation techniques of a glass coating on Ti6Al4V for biomedical applications
Source abstract
Abstract
Abstract The fixation of bone replacement implants to the hosting tissue can be improved if the implants have a bioactive surface that can precipitate hydroxyapatite in vivo. Titanium alloys, despite their desirable mechanical and nontoxic properties, are not bioactive and do not bond directly to the bone. One of the ways to change a bioinert metallic surface such as a titanium alloy is to coat it with a bioactive material. This work presents the microstructural and stress–corrosion cracking characterization of two glass coatings on Ti6Al4V with different SiO2 contents (61% and 64%). These coatings belong to the SiO2–CaO–MgO–Na2O–K2O–P2O5 system and they were obtained by a simple enamelling technique. They will be used as the first layer of a bioactive multilayer system which will have an outer layer with a lower SiO2 content in order to ensure the surface bioactivity. Microstructural characterization performed by scanning electron microscopy (SEM) and energy dispersive X-ray spectroscopy (EDS) shows that the coating porosity is clearly influenced by the firing time because of the longer extension of the reaction between Ti and SiO2. The X-ray diffraction (XRD) integration method shows that the amount of crystalline phase (2.4CaO 0.6Na2O P2O5) percentage is between 3 vol.% and 16 vol.%. After acid etching, a microstructure with clear boundaries is observed which is the result of the sintered glass particles separation. Stress–corrosion cracking was evaluated using Vickers and Hertzian (spherical) indentation, showing that both coatings are sensitive to subcritical crack growth, and that the coating with the lower silica content is more sensitive to stress–corrosion cracking. These two results are related with the larger residual stresses due to the thermal expansion mismatch. Finally, the stress–corrosion ring cracking behavior by Hertzian indentation is rationalized from the linear-elastic fracture mechanics framework.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Bone Tissue Engineering Materials · Titanium Alloys Microstructure and Properties · Metal and Thin Film Mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (36)
Show source-provided references
1. The ASM Committee on Titanium and Titanium Alloys, Properties of titanium and titanium alloys. In Metals Handbook, Vol. 3. Properties and Selection: Stainless Steels, Tool Materials and Special-Purpose Metals. American Society for Metals, Metals Park, Ohio, 1980, pp. 372–412.
2. Fracture of titanium orthopaedic implants10.1007/BF00543750 ↗
3. Bioceramics: from concept to clinic10.1111/j.1151-2916.1991.tb07132.x ↗
4. Processing and properties of hydroxiapatite-based biomaterials for use as hard tissue replacement implants10.1557/JMR.1998.0015 ↗
5. Hydroxilapatite coating
6. Hastings, G. W., Dayli, D., and Mores, S., In Bioceramics. Vol. 1, ed. Ohnishi, H., Aoki, H. and Sawai, K. Euroamerica, Ishyaku, 1989, pp. 355–358.
7. Cook · J. Biomed. Mater. Res. · 1993 · 27 · 150110.1002/jbm.820270115 ↗
8. Bioactive glass coatings
9. Characteristics of plasma-sprayed bioactive glass coatings on Ti6Al4V alloy: an in vitro study10.1016/0257-8972(95)02463-8 ↗
10. Bone-bonding behaviour of plasma-sprayed coatings of Bioglass®, AW-glass ceramic and tricalcium phosphate on titanium alloy10.1002/(SICI)1097-4636(199602)30:2<261::AID-JBM17>3.0.CO;2-P ↗
11. Glass-based coatings for titanium implant alloys10.1002/(SICI)1097-4636(19990915)46:4<549::AID-JBM13>3.0.CO;2-M ↗
12. Silicate glass coatings on Ti-based implants10.1016/S1359-6454(98)80039-6 ↗
13. Bioactive coatings on Ti and Ti6Al4V alloys for medical applications
14. Hench · J. Biomed. Res. Symp. · 1971 · 2 · 11710.1002/jbm.820050611 ↗
15. Ceramic-based layer structures for biomechanical applications10.1016/S1359-0286(02)00016-5 ↗
16. Kinematics theory on quantitative analysis of X-ray diffraction
17. Cullity · 1978
18. Noyan · 1987
19. Overview: residual stress. Part 1—measurement techniques10.1179/026708301101509980 ↗
20. Measuring mechanical properties of coatings: a methodology applied to nano-particle-filled sol-gel coatings on glass10.1016/S0927-796X(01)00040-7 ↗
21. Turner · J. Res. NBS · 1946 · 37 · 239
22. Bioactive glass coatings for orthopedic metallic implants10.1016/S0955-2219(03)00303-0 ↗
23. Thermal expansion of alumino-alkasilicate and alumino-borosilicate glasses—comparison of empirical model10.1023/A:1018566606548 ↗
24. The influence of chemical composition on the physical properties of glasses10.1111/j.1151-2916.1930.tb16561.x ↗
25. Relationship between chemical composition and the thermal expansion of glasses
26. Expansion coefficients of glasses10.1002/andp.18942870407 ↗
27. Contact induced damage in ceramic coatings on compliant substrate: fracture mechanics and design10.1111/j.1151-2916.2001.tb00791.x ↗
28. Lawn · 1993
29. Determining the fracture toughness of brittle materials by Hertzian indentation10.1016/0955-2219(95)93941-U ↗
30. Determination of surface stresses in brittle materials by Hertzian indentation: theory and experiment10.1111/j.1151-2916.1999.tb02003.x ↗
31. Probability of cone crack initiation due to the spherical contact loading10.1016/j.jeurceramsoc.2003.10.038 ↗
32. Zur Theorie der Berührung Fester Elasticher Körper
33. Local stress intensity factors for small semi-elliptical cracks under exponentially distributed stresses10.1016/S0013-7944(99)00060-0 ↗
34. Timoshenko · 1951
35. On the theory of Hertzian fracture10.1098/rspa.1967.0137 ↗
36. Stress–corrosion cracking of a bioactive glass10.1111/j.1551-2916.1988.tb00185.x ↗