Fiber size effects on mechanical behaviours of SiC fibres-reinforced Ti3AlC2 matrix composites

Shuqi Guo

Publisher page

Abstract

Abstract In this study, different diameters SiC fibres-reinforced Ti 3 AlC 2 matrix composites were fabricated via hot-pressing. The mechanical behaviours of the obtained composites were evaluated at room temperature by using 4-point bending testing. The results show that the flexural strength and damage tolerance are significantly higher for smaller diameter fibres-containing composites than for large diameter fibres-containing ones. In addition, the mechanical properties of the composites were improved when smaller diameter fibres partially replaced large diameter fibres and the improvement increased with increase of the amount of smaller diameter fibre. Furthermore, the fracture fashion of the composites depended on fibre diameters used.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: MXene and MAX Phase Materials · Aluminum Alloys Composites Properties · Advanced ceramic materials synthesis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (21)

Show source-provided references
1. The MN+1AXN phases: a new class of solids; thermodynamically stable nanolaminates10.1016/S0079-6786(00)00006-6 ↗
2. Synthesis and characterization of Ti3AlC210.1111/j.1151-2916.2000.tb01281.x ↗
3. In situ synthesis and properties of Ti3AlC2/TiB2 composites10.1111/j.1551-2916.2007.01954.x ↗
4. Shell-like nanolayered Nb4AlC3 ceramic with high strength and toughness10.1016/j.scriptamat.2010.12.045 ↗
5. Layered machinable ceramics for high temperature applications10.1016/S1359-6462(96)00418-6 ↗
6. Ab initio study of irradiation tolerance for different M(n+1)AX(n) phase: Ti3SiC2 and Ti3AlC210.1063/1.4861384 ↗
7. Preparation of high strength Ti3AlC2 by spark plasma sintering10.1111/ijac.12254 ↗
8. Concept for a damage-tolerant ceramic composite with a strong interfaces10.1111/j.1151-2916.1996.tb08138.x ↗
9. Damage and failure in unidirectional ceramic-matrix composites10.1111/j.1151-2916.1992.tb05495.x ↗
10. SiC(SCS-6) fibre-reinforced Ti3AlC2 matrix composites: interfacial characterization and mechanical behaviour10.1016/j.jeurceramsoc.2014.11.034 ↗
11. Improvement of mechanical properties of SiC(SCS-6) fibre-reinforced Ti3AlC2 matrix composites with Ti barrier layer10.1016/j.jeurceramsoc.2015.12.039 ↗
12. Matrix fracture in fibre-reinforced ceramic10.1016/0022-5096(86)90035-9 ↗
13. Theory of mechanical properties of ceramic-matrix composite10.1111/j.1151-2916.1991.tb06852.x ↗
14. The microstructure of SCS-6 SiC fibre10.1557/JMR.1991.2234 ↗
15. Microstructure and role of outermost coating for tensile strength of SiC fibre10.1016/S1359-6454(98)00181-5 ↗
16. Continuous silicon carbide fibre MMCs
17. Tensile tests of ceramic-matrix composites: theory and experiment10.1111/j.1151-2916.1990.tb05273.x ↗
18. Residual stresses, strength and toughness of laminates with different layer thickness ratios10.1016/j.actamat.2006.06.008 ↗
19. The mechanical behaviour of ceramic matrix composites10.1016/0001-6160(89)90291-5 ↗
20. A uniaxially reinforced zircon-silicon carbide composite10.1007/BF00576772 ↗
21. Role of fiber-matrix interfacial shear stress on the toughness of reinforced oxide matrix composites10.1557/PROC-120-259 ↗