Harmonized toughening and strengthening in pressurelessly reactive-sintered Ta0.8Hf0.2C-SiC composite
Source abstract
Abstract
Abstract Ta0.8Hf0.2C-27 vol%SiC (99.0% in relative density) composite was toughened and strengthened via pressurelessly in-situ reactive sintering process. HfC and β-SiC particles were formed after reaction of HfSi2 and carbon black at 1650 °C. Ta0.8Hf0.2C was obtained from solid solutioning of HfC and commercial TaC. The β-α phase transformation of SiC proceeded below 2200 °C. High aspect ratio, platelet-like α-SiC grains formed and interconnected as interlocking structures. Toughness and flexural strength values of 5.4 ± 1.2 MPa m1/2 and 443 ± 22 MPa were measured respectively. The toughening mechanisms by highly directional growth of discontinuous α-SiC grains were crack branching, bridging and deflection behaviors.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced materials and composites · Advanced ceramic materials synthesis · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (25)
Show source-provided references
1. Melting point in systems ZrC-HfC, TaC-ZrC, TaC-HfC10.1007/BF00773385 ↗
2. Effect of solid solution formation on densification of hot-pressed ZrC ceramics with MC (M=V, Nb, and Ta) additions10.1016/j.jeurceramsoc.2011.10.045 ↗
3. Sintering behaviour, solid solution formation and characterisation of TaC, HfC and TaC–HfC fabricated by spark plasma sintering10.1016/j.jeurceramsoc.2016.02.009 ↗
4. Prediction of the material with highest known melting point from ab initio molecular dynamics calculations10.1103/PhysRevB.92.020104 ↗
5. Solid solution synthesis of tantalum carbide-hafnium carbide by spark plasma sintering10.1111/jace.14778 ↗
6. Influence of hafnium carbide on vacuum plasma spray processed tantalum carbide microstructures10.1016/j.jeurceramsoc.2012.10.029 ↗
7. Pressureless densification, microstructure tailoring and properties of Ta0.8Hf0.2C-based composites10.1016/j.jeurceramsoc.2017.10.025 ↗
8. The thermal shock resistance of solids10.1016/S1359-6454(98)00127-X ↗
9. Hertzian indentation of a ZrB2–30% SiC ultra‐high‐temperature ceramic up to 800°C in air10.1111/j.1551-2916.2010.03631.x ↗
10. Nacre-like ceramic refractories for high temperature applications10.1016/j.jeurceramsoc.2017.10.042 ↗
11. Low-temperature sintering of HfC/SiC nanocomposites using HfSi2-C additives10.1111/jace.14301 ↗
12. Fracture toughness determinations by indentation10.1111/j.1151-2916.1976.tb10991.x ↗
13. Synthesis of highly dispersed super-refractory tantalum-zirconium carbide Ta4ZrC5 and tantalum-hafnium carbide Ta4HfC5 via sol-gel technology10.1134/S0036023611110258 ↗
14. High toughness in pressureless densified ZrB2-based composites co-doped with boron–titanium carbides10.1016/j.scriptamat.2011.12.036 ↗
15. Untersuchungen im system hafnium-tantal-kohlenstoff10.1007/BF00903490 ↗
16. Quantitative X-ray diffraction analysis of reactive infiltrated boron carbide–aluminium composites10.1016/S0955-2219(02)00304-7 ↗
17. Effect of initial α-phase content of SiC on microstructure and mechanical properties of SiC–TiC composites10.1016/S0955-2219(00)00160-6 ↗
18. In situ-toughened silicon carbide10.1111/j.1151-2916.1994.tb07024.x ↗
19. The β→α transformation in polycrystalline SiC: IV, a comparison of conventionally sintered, hot‐pressed, reaction‐sintered, and chemically vapor‐deposited samples10.1111/j.1151-2916.1981.tb09584.x ↗
20. Toughness properties of a silicon carbide with an in situ induced heterogeneous grain structure10.1111/j.1151-2916.1994.tb04637.x ↗
21. Ablation tests on HfC-and TaC-based ceramics for aeropropulsive applications10.1016/j.jeurceramsoc.2014.11.018 ↗
22. In situ synthesis of ZrB2–ZrCx ceramic tool materials toughened by elongated ZrB2 grains10.1016/j.matdes.2013.01.062 ↗
23. Pressureless sintering of ZrB2–SiC ceramics10.1111/j.1551-2916.2007.02006.x ↗
24. Toughening of a particulate‐reinforced ceramic‐matrix composite by thermal residual stress10.1111/j.1151-2916.1990.tb05209.x ↗
25. Strengthening and toughening mechanisms of ceramic nanocomposites10.1111/j.1151-2916.1998.tb02503.x ↗