Abstract

Abstract To regulate the microstructures of carbide ceramic-doped C/C (C/C-ceramic) composites using reactive melting infiltration (RMI) in a controlled manner, an electromagnetic induction heating RMI (ERMI) was proposed and used to fabricate typical C/C–SiC composites herein. Because the tedious heating and cooling regions could be bypassed using ERMI, excessive graphitization and ceramic overreactions of the ERMI-C/C-SiC composites were effectively avoided, which made the interfacial bonding strength (τ) of the ERMI-C/C–SiC composites (∼25.7 MPa) much lower than that of the CRMI-C/C-SiC composites (∼36.1 MPa) (fabricated using conventional RMI (CRMI)). A weaker τ value triggered strengthening/toughening mechanisms such as crack deflection, and crack arrest, which ultimately led to higher flexural strength and displacement of the ERMI-C/C–SiC composites than the CRMI-C/C–SiC composites. The proposed ERMI exhibited relatively good controlling capability to regulate the microstructures of C/C-ceramic composites.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (39)

Show source-provided references
1. Advances in oxidation and ablation resistance of high and ultra-high temperature ceramics modified or coated carbon/carbon composites10.1016/j.jeurceramsoc.2017.08.013 ↗
2. Ultra-high temperature ceramics: materials for extreme environments10.1016/j.scriptamat.2016.10.018 ↗
3. Effects of SiC interphase on the mechanical and ablation properties of C/C-ZrC-ZrB2-SiC composites prepared by precursor infiltration and pyrolysis10.1016/j.matdes.2017.02.086 ↗
4. Wet oxidation behavior of SiC/(SiC-SiBCN)x composites prepared by CVI combined with PIOP process10.1111/jace.16497 ↗
5. Fast Sol–gel preparation of silicon carbide–silicon oxycarbide nanocomposites10.1111/j.1551-2916.2011.04707.x ↗
6. Preparation and mechanism of C/C-SiC composite through polymer-Si slurry reactive melt infiltration10.1016/j.ceramint.2019.11.002 ↗
7. Microstructure and ablation behavior of SiC coated C/C–SiC–ZrC composites prepared by a hybrid infiltration process10.1016/j.carbon.2013.08.014 ↗
8. Analysis of reactive melt infiltration in the processing of ceramics and ceramic composites10.1016/S0009-2509(97)00379-5 ↗
9. Cost effective processing of composites by melt infiltration (LSI process)10.1002/9780470294680.ch52 ↗
10. Reaction mechanism and microstructure development of Zr-Si alloyed melt-Infiltrated ZrC-Modified C/C composite10.1111/jace.13595 ↗
11. Interphase degradation of three-dimensional Cf/SiC–ZrC–ZrB2 composites fabricated via reactive melt infiltration10.1111/jace.14983 ↗
12. An environmentally friendly route to prepare hierarchical carbon/carbon-SiC composites by carbothermal reduction10.1016/j.carbon.2010.08.029 ↗
13. Microstructure and mechanical properties of three dimensional Cf/SiC–ZrC–ZrB2 composites prepared by reactive melt infiltration method10.1016/j.jeurceramsoc.2016.07.002 ↗
14. Microwave heating controlled reactive melt infiltration for graphite-Si-SiC ceramics manufacturing10.1111/jace.16124 ↗
15. Effects of high-temperature annealing on the microstructure and properties of C/ZrC composites prepared by reactive melt infiltration10.1016/j.msea.2016.12.059 ↗
16. Influence of the carbonization temperature on the mechanical properties of thermoplastic polymer derived C/C-SiC composites10.1016/j.jeurceramsoc.2016.09.005 ↗
17. A general method to synthesize and sinter bulk ceramics in seconds10.1126/science.aaz7681 ↗
18. Graphite-Si-SiC ceramics produced by microwave assisted reactive melt infiltration10.1016/j.jeurceramsoc.2019.01.057 ↗
19. Field-assisted sintering technology/spark plasma sintering: mechanisms, materials, and technology developments10.1002/adem.201300409 ↗
20. High temperature deformability of ductile flash-sintered ceramics via in-situ compression
21. Enhanced properties of nanostructured ZrO2–graphene composites rapidly sintered via high-frequency induction heating10.1016/j.ceramint.2014.08.042 ↗
22. The effect of graphene reinforcement on the mechanical properties of Al2O3 ceramics rapidly sintered by high-frequency induction heating10.1016/j.ijrmhm.2014.10.011 ↗
23. Flash Sintering of Nanograin Zirconia in <5 s at 850°C10.1111/j.1551-2916.2010.04089.x ↗
24. Review of flash sintering: materials, mechanisms and modelling10.1080/17436753.2016.1251051 ↗
25. Microstructure and mechanical properties of Fe–Si alloy modified C/C–SiC composites10.1016/j.ceramint.2019.07.153 ↗
26. Microstructure and tribological characteristics of needled C/C–SiC brake composites fabricated by simultaneous infiltration of molten Si and Cu10.1016/j.triboint.2015.08.047 ↗
27. Influence of h-BN as additive on microstructure and oxidation mechanism of C/C-SiC composite10.1016/j.jeurceramsoc.2019.06.032 ↗
28. Fang · 1994
29. Effect of reaction melt infiltration temperature on the ablation properties of 2D C/C–SiC–ZrC composites10.1016/j.corsci.2012.01.001 ↗
30. Effects of extreme transverse deformation on the strength of UHMWPE single filaments for ballistic applications10.1007/s10853-016-0077-3 ↗
31. Influence of surface fibre properties and textural organization of a pyrocarbon interphase on the interfacial shear stress of SiC/SiC minicomposites reinforced with Hi-Nicalon S and Tyranno SA3 fibres10.1016/j.jeurceramsoc.2013.08.027 ↗
32. Multi-scale modeling of thermal expansion coefficients of C/C composites at high temperature10.1016/j.matdes.2015.05.061 ↗
33. Influence of the carbonization temperature on the mechanical properties of thermoplastic polymer derived C/C-SiC composites10.1016/j.jeurceramsoc.2016.09.005 ↗
34. Effect of infiltration time on the microstructure and mechanical properties of C/C-SiC composite prepared by Si-Zr10 alloyed melt infiltration10.1016/j.ceramint.2014.11.088 ↗
35. Effect of graphitization on the microstructure and properties of Mo2C-Modified C/C-Cu composites10.1002/adem.201500489 ↗
36. Effect of fiber microstructure studied by Raman spectroscopy upon the mechanical properties of carbon fibers10.1002/jrs.5569 ↗
37. Effect of microstructure on the mechanical properties of PAN-based carbon fibers during high-temperature graphitization10.1007/s10853-008-2633-y ↗
38. Weak interface dominated high temperature fracture strength of carbon fiber reinforced mullite matrix composites10.1016/j.jeurceramsoc.2017.03.033 ↗
39. Microscopic analysis of single-fiber push-out tests on ceramic matrix composites performed with Berkovich and flat-end indenter and evaluation of interfacial fracture toughness10.1016/j.jeurceramsoc.2012.09.009 ↗