journal article·2021-08

Dynamic oxidation mechanism of SiC fiber reinforced SiC matrix composite in high-enthalpy plasmas

Lingwei Yang, Xueren Xiao, Li Jing, Jun Zhang, Liping Liu, Changhao Zhao, Guolin Wang

Publisher page

Abstract

Abstract A plasma wind tunnel was utilized to explore the dynamic oxidation mechanism of SiC fiber reinforced SiC matrix composite in high-enthalpy plasmas. The results suggest the occurrences of active and passive oxidations on SiC fiber/matrix with atomic oxygen at 900∼1600 °C and 1∼6 kPa. Increasing plasma pressure could retard the active oxidation and promote the passive oxidation. Severe corrosion of SiC fibers due to active oxidation is highlighted. The as-formed SiO2 layers cannot fully seal the open porosities and the interfacial gaps formed by oxidation of pyrocarbon interphases. This led to penetration of oxidized species and failure of fiber bundles directly exposed to heat flows. In addition, the spatial heat flux and temperature distributions were not homogeneous on the oxidized surface, which triggered early ‘temperature jump’ at ≈1600 °C (≈4.5 kPa) and severe localized ablation. If sealing the composite surface with SiC coating, the ablation resistance was significantly improved.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Diamond and Carbon-based Materials Research · Metal and Thin Film Mechanics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (29)

Show source-provided references
1. SiC/SiC mini-composites with yttrium disilicate fiber coatings: oxidation in steam10.1016/j.jeurceramsoc.2020.09.033 ↗
2. Self-healing enhancing tensile creep of 2D-satin weave SiC/(SiC-SiBCN)x composites in wet oxygen environment10.1016/j.jeurceramsoc.2020.03.052 ↗
3. Crack initiation and propagation in braided SiC/SiC composite tubes: effect of braiding angle10.1016/j.jeurceramsoc.2020.04.060 ↗
4. Oxidation behavior of SiC/SiC composites for helium cooled solid breeder blanket10.1016/j.fusengdes.2008.06.004 ↗
5. Influence of an O2 type oxidizing environment on SiCf/SiC composites: Properties/Microstructure10.1007/s11085-013-9384-0 ↗
6. High temperature oxidation of SiC under helium with low-pressure oxygen. Part 3: β-SiC-SiC/ PyC/SiC10.1016/j.jeurceramsoc.2011.08.005 ↗
7. Oxidation behaviour of SiC/SiC ceramic matrix composites in air, J. Eur10.1016/j.jeurceramsoc.2016.05.051 ↗
8. Effect of oxidation treatment on KD–II SiC fiber–reinforced SiC composites10.1016/j.ceramint.2017.05.001 ↗
9. Oxidation resistance of SiCf/SiC composites with a PyC/SiC multilayer interface at 500 °C to 1100 °C10.1016/j.corsci.2020.108522 ↗
10. Oxidation/corrosion of BN-based coatings as prospective interphases for SiC/SiC composites10.1016/j.jeurceramsoc.2020.07.056 ↗
11. Effect of interface types on the static and dynamic mechanical properties of 3D braided SiC/SiC composites after oxidation
12. Subsurface oxidation of boron nitride coatings on silicon carbide fibers in SiC/SiC ceramic matrix composites10.1016/j.ceramint.2018.06.221 ↗
13. Oxidation behaviour of SiC fibre reinforced SiC
14. Ablation behavior of C/SiC-HfC composites in the plasma wind tunnel10.1016/j.jeurceramsoc.2016.03.017 ↗
15. Carbon fiber reinforced silicon carbide composite-based sharp leading edges in high enthalpy plasma flows10.1016/j.compositesb.2017.09.060 ↗
16. Ablation behavior of C/SiC composites in plasma wind tunnel10.1016/j.carbon.2016.02.085 ↗
17. Thermo-chemical surface instabilities of SiC-ZrB2 ceramics in high enthalpy dissociated supersonic airflows10.1016/j.jeurceramsoc.2017.01.018 ↗
18. Oxidation and ablation behaviors of carbon fiber/phenolic resin composites modified with borosilicate glass and polycarbosilane interface10.1016/j.jallcom.2020.154277 ↗
19. Oxide-scale evolution and dynamic oxidation mechanism of ZrB2-SiC in high-enthalpy plasma wind tunnel
20. Experiments to determine surface catalytic recombination coefficients of ultra high temperature ceramics in high temperature dissociated flows
21. Dynamic oxidation of SiC with arc-heated plasma wind tunnel and laser heating10.1016/j.vacuum.2020.109899 ↗
22. Effects of oxidation temperature, time, and ambient pressure on the oxidation of ZrB2–SiC–graphite composites in atomic oxygen10.1016/j.jeurceramsoc.2016.02.040 ↗
23. Processing-temperature dependent micro- and macro-mechanical properties of SiC fiber reinforced SiC matrix composites10.1016/j.compositesb.2017.07.079 ↗
24. Oxidation resistance of NITE-SiC/SiC composites with/without CVD-SiC environmental barrier coating10.1016/j.ceramint.2018.06.194 ↗
25. Ablation behavior of an Ir-Hf coating: a novel idea for ultra-high temperature coatings in non-equilibrium conditions10.1016/j.jallcom.2019.152829 ↗
26. The effect of zirconium carbide on ablation of SiC-coated carbon/silicon carbide composites under an oxy-acetylene flame10.1111/ijac.12043 ↗
27. Roughness evolution in ablation of carbon-based materials: multi-scale modelling and material analysis
28. Formation mechanisms of characteristic structures on the surface of C/SiC composites subjected to thermal ablation10.1016/j.jeurceramsoc.2015.10.016 ↗
29. Influence of porosity on anisotropic thermal conductivity of SiC fiber reinforced SiC matrix composite: a microscopic modeling study10.1016/j.ceramint.2020.08.029 ↗