Abstract
Abstract To improve the oxidation resistances of SiC coated C/C composites by a pack cementation (PC) method at high temperature and alleviate the siliconization erosion of molten silicon on C/C substrate during the preparation of SiC coating, a SiO2-SiC reticulated layer with SiC nanowires was pre-prepared on C/C composites through combined slurry painting and thermal treatment before the fabrication of SiC coating. The presence of porous SiO2-SiC layer with SiC nanowires was beneficial to fabricate a compact and homogeneous SiC coating resulting from synergistic effect of further reaction between SiO2 and pack powders and the reinforcement of SiC nanowires. Therefore, the results of thermal shock and isothermal oxidation tests showed that the mass loss of modified SiC coating was only 0.02 % after suffering 50-time thermal cycles between room temperature and 1773 K and decreased from 5.95 % to 1.08 % after static oxidation for 49.5 h in air at 1773 K. Moreover, due to the blocking effect of SiO2-SiC reticulated layer on siliconization erosion during PC, the flexural strength of SiC coated C/C composites with SiO2-SiC reticulated layer increased by 64.8 % compared with the untreated specimen.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Nuclear materials and radiation effects
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (50)
Show source-provided references
1. The effect of carbon fabric treatment on delamination of 2D-C/C composites10.1016/j.compscitech.2006.03.025 ↗
2. Mechanical and thermal properties of C/C composites modified with SiC nanofiller10.1016/j.msea.2018.01.048 ↗
3. Effects of thermal and thermomechanical induced mechanical changes of C/C composites10.1016/j.carbon.2010.04.040 ↗
4. Oxidation protection for carbon fibre composites10.1007/BF00357844 ↗
5. Oxidation protective multilayer coatings for carbon-carbon composites10.1016/S0008-6223(01)00151-8 ↗
6. An oxidation protective Si-Mo-Cr coating for C/SiC coated carbon/carbon composites10.1016/j.carbon.2007.10.022 ↗
7. Tailored macro-pores during the formation of C/C-SiC via liquid phase pyrolysis10.1016/j.jeurceramsoc.2020.10.006 ↗
8. TaxHf1-xB2-SiC multiphase oxidation protective coating for SiC-coated carbon/carbon composites10.1016/j.corsci.2014.07.016 ↗
9. Erosion protective coatings for low density, highly porous carbon/carbon composites10.1016/j.carbon.2009.01.045 ↗
10. Multilayer and multi-component oxidation protective coating system for carbon/carbon composites from room temperature to 1873 K10.1016/j.corsci.2013.03.006 ↗
11. Characterization of the oxidation of C/C/SiC composites by X-ray microtomography10.1016/j.jeurceramsoc.2020.06.042 ↗
12. A CrSi2-HfB2-SiC coating providing oxidation and ablation protection over 1973 K for SiC coated C/C composites10.1016/j.corsci.2020.108536 ↗
13. SiC/MoSi2 based coatings for Cf/C composites by two step pack cementation10.1016/j.jeurceramsoc.2018.01.024 ↗
14. Influence of the preparation temperature on the phase, microstructure and anti-oxidation property of a SiC coating for C/C composites10.1016/j.carbon.2004.01.066 ↗
15. ZrB2-SiC based composites for thermal protection by reaction sintering of ZrO2+B4C+Si10.1007/s40145-017-0244-2 ↗
16. Preparation of an oxidation protection coating for C/C composites by low pressure chemical vapor deposition10.1016/S0008-6223(00)00086-5 ↗
17. Oxidation through coating cracks of SiC-protected carbon/carbon10.1016/j.surfcoat.2008.09.013 ↗
18. Resistance to oxidation and ablation of SiC coating on graphite prepared by chemical vapor reaction10.1016/j.corsci.2013.05.009 ↗
19. Silicon carbide based plasma sprayed coatings10.1016/j.surfcoat.2012.06.062 ↗
20. Structure and flexural properties of 3D needled carbon fiber reinforced carbon and silicon carbide (C/C-SiC) composites fabricated by gaseous and liquid silicon infiltration10.1016/j.ceramint.2019.06.016 ↗
21. Influence of preparation temperature on the oxidation resistance and mechanical properties of C/SiC coated C/C composites10.1016/j.corsci.2014.05.009 ↗
22. Oxidation and mechanical properties of SiC/SiC-MoSi2-ZrB2 coating for carbon/carbon composites10.1016/j.jmst.2013.09.006 ↗
23. The oxidation behavior and mechanical properties of MoSi2-CrSi2-SiC-Si coated carbon/carbon composites in high-temperature oxidizing atmosphere10.1016/j.corsci.2011.08.018 ↗
24. Oxidation and ablation resistance of ZrB2-SiC-Si/B-modified SiC coating for carbon/carbon composites10.1016/j.corsci.2012.10.041 ↗
25. An oxidation and ablation protective WSi2-HfB2-SiC coating for SiC coated C/C composites at 1973 K and above10.1016/j.corsci.2020.108964 ↗
26. A C/SiC gradient oxidation protective coating for carbon/carbon composites10.1016/j.surfcoat.2006.07.239 ↗
27. Damage development during flexural loading of a 5-directional braided C/C-SiC composites, characterized by X-ray tomography and digital volume correlation10.1016/j.ceramint.2018.12.020 ↗
28. In situ synthesis of SiC nanowire porous layer on carbon/carbon composites10.1111/jace.15296 ↗
29. Simple approach to fabricate SiC-SiO2 composite nanowires and their oxidation resistance10.1016/j.mseb.2010.01.042 ↗
30. Thermal evaporation synthesis of SiC/SiOx nanochain heterojunctions and their photoluminescence properties10.1039/C4TC01391C ↗
31. Thermal shock resistance and isothermal oxidation behavior of C/SiC-SiCnano functionally gradient coating on graphite produced via reactive melt infiltration (RMI)10.1016/j.matchemphys.2016.07.004 ↗
32. Effects of pyrocarbon on morphology stability of SiC nanowires at high temperatures10.1111/jace.15524 ↗
33. SiC nanowire-induced fabrication of fine-grained and highly-density SiC coating by pressure-less reactive sintering10.1016/j.jallcom.2018.05.001 ↗
34. Sintering behavior, microstructural evolution, and mechanical properties of ultra-fine grained alumina synthesized via in-situ spark plasma sintering10.1016/j.ceramint.2015.11.106 ↗
35. Aluminum composite reinforced with multiwalled carbon nanotubes from plasma spraying of spray dried powders10.1016/j.surfcoat.2008.12.004 ↗
36. Bamboo-shaped SiC nanowire-toughened SiC coating for oxidation protection of C/C composites10.1016/j.corsci.2012.12.009 ↗
37. Influence of SiC nanowires on the properties of SiC coating for C/C composites between room temperature and 1500 °C10.1016/j.corsci.2011.05.046 ↗
38. SiC coating toughened by SiC nanowires to protect C/C composites against oxidation10.1016/j.ceramint.2011.05.159 ↗
39. Toughening by SiC nanowires in a dense SiC-Si ceramic coating for oxidation protection of C/C Composites10.1111/j.1551-2916.2012.05412.x ↗
40. Oxidation protection of C/C composites with a multilayer coating of SiC and Si + SiC + SiC nanowires10.1016/j.carbon.2011.10.048 ↗
41. A SiC-ZrB2-ZrC coating toughened by electrophoretically-deposited SiC nanowires to protect C/C composites against thermal shock and oxidation10.1016/j.apsusc.2015.05.028 ↗
42. SiC nanoparticles toughened-SiC/MoSi2-SiC multilayer functionally graded oxidation protective coating for carbon materials at high temperatures10.1007/s11665-017-2725-4 ↗
43. Nanowire-toughened transition layer to improve the oxidation resistance of SiC-MoSi2-ZrB2 coating for C/C composites10.1016/j.corsci.2016.05.013 ↗
44. A SiCnw/PyC-toughened ZrB2-SiC coating for protecting Si-SiC coated C/C composites against oxidation10.1016/j.apsusc.2018.06.246 ↗
45. Improved thermal shock resistance of SiCnw/PyC core-shell structuretoughened CVD-SiC coating10.1016/j.jeurceramsoc.2018.02.017 ↗
46. Oxidation pre-treatment and electrophoretic deposition of SiC nanowires to improve the thermal shock resistance of SiC coating for C/C composites10.1016/j.jallcom.2015.02.075 ↗
47. Nanowire-toughened CVD-SiC coating for C/C composites with surface pre-oxidation10.1080/02670844.2017.1292705 ↗
48. Effect of carbon nanotubes on the toughness, bonding strength and thermal shock resistance of SiC coating for C/C-ZrC-SiC composites10.1016/j.jallcom.2015.04.223 ↗
49. Surface dissolution and diffusion of oxygen molecules in SiO2 glass10.2109/jcersj.112.559 ↗
50. Effects of ZrB2 and SiC dual addition on the oxidation resistance of graphite at 1600-2000 °C10.1016/j.corsci.2013.06.041 ↗