Oxidation behaviors and mechanisms of CVD Si-B-C ceramic in wet oxygen from 700 °C to 1400 °C
Source abstract
Abstract
Abstract Si-B-C ceramic is an effective self-healing component to improve the oxidation resistance of C/SiC composites for long-life applications in aircraft and aerospace fields. To clarify protection mechanisms, oxidation behaviors and mechanisms of CVD Si-B-C ceramic in wet oxygen from 700 °C to 1400 °C were investigated in this work. Microstructure, bonds transformation and phase evolution of Si-B-C ceramic after oxidation were analyzed. The weight loss of Si-B-C ceramic increased linearly with time between 700 °C and 1000 °C, while it changed in a non-linear way above 1200 °C. The oxidation production of Si-B-C ceramic in wet oxygen is mainly composed of Si(OH) 4 , SiO 2 , H 3 BO 3 , B 2 O 3 and B 2 O. The oxidation resistance of Si-B-C in wet oxygen is better than that of single-phase B 4 C ceramic because borosilicate glass is rapidly formed, which can effectively resist the wet oxygen. No fiber oxidation is found up to 1400 °C.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · MXene and MAX Phase Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (37)
Show source-provided references
1. Design, preparation and properties of non-oxide CMCs for application in engines and nuclear reactors: an overview10.1016/S0266-3538(03)00230-6 ↗
2. SiC-matrix composites: non-brittle ceramics for thermo-structural application10.1111/j.1744-7402.2005.02009.x ↗
3. Advanced ceramic matrix composite materials for current and future propulsion technology applications10.1016/j.actaastro.2004.05.052 ↗
4. Zhang · 2009 · 18
5. Microstructure and mechanical properties of three-dimensional carbon/silicon carbide composites fabricated by chemical vapor infiltration10.1016/S0008-6223(98)00076-1 ↗
6. Processing and properties of self-healing C/SiC ceramic matrix composites
7. Boron-bearing species in ceramic matrix composites for long-term aerospace applications10.1016/j.jssc.2003.03.005 ↗
8. A new route to fabricate SiB4 modified C/SiC composites10.1016/j.jeurceramsoc.2010.02.028 ↗
9. Preparation and oxidation resistance of 2D C/SiC composites modified by partial boron carbide self-sealing matrix10.1016/j.msea.2008.08.022 ↗
10. Preparation and oxidation protection of CVD SiC/a-BC/SiC coatings for 3D C/SiC composites10.1016/j.corsci.2009.01.026 ↗
11. Microstructural evolution of coating-modified 3D C/SiC composites after annealing in wet oxygen at different temperatures10.1016/j.corsci.2010.04.032 ↗
12. Effect of glass sealing on the oxidation behavior of three dimensional C/SiC composites in air10.1016/S0008-6223(00)00148-2 ↗
13. Enhancement of the oxidation resistance of interfacial area in C/C composites. Part I: oxidation resistance of B–C, Si–B–C and Si–C coated carbon fibres10.1016/S0955-2219(01)00410-1 ↗
14. Oxidation behaviour of a multi-layered ceramic-matrix composite (SiC)f/C/(SiBC)m10.1016/S0266-3538(00)00243-8 ↗
15. Effect of deposition temperature on dynamics and mechanism of deposition for Si-B-C ceramic from BCl3/SiCH3Cl3/H2 precursor10.1016/S1005-0302(12)60132-7 ↗
16. Effect of SiC coating and heat treatment on the thermal radiationproperties of C/SiC composites10.1016/j.jeurceramsoc.2013.12.012 ↗
17. Spectroscopic studies of BN films deposited by dynamic ion mixing10.1016/0040-6090(93)90185-R ↗
18. Core-electron binding energies for compounds of boron, carbon, and chromium10.1021/ic50085a035 ↗
19. Ignition mechanism of the titanium–boron pyrotechnic mixture10.1002/sia.740110614 ↗
20. Simple and coordination compounds. An X-ray photoelectron spectroscopic study of certain oxides
21. X-ray photoelectron spectroscopy of nickel boride catalysts: correlation of surface states with reaction products in the hydrogenation of acrylonitrile10.1016/0021-9517(80)90294-8 ↗
22. Surface characterization of aluminum foil annealed in the presence of ammonium fluoborate10.1016/0169-4332(89)90009-3 ↗
23. X-ray photoelectron spectroscopy with X-ray photons of higher energy10.1116/1.569459 ↗
24. Incorporation of OH radicals in anodic silicon oxide films studied by secondary-ion mass spectroscopy, X-ray photoelectron spectroscopy and ir analysis10.1016/S0040-6090(05)80042-2 ↗
25. An ESCA study of termination of the passivation of elemental metals10.1021/j100505a006 ↗
26. Surface characterization of aluminum foil annealed in the presence of ammonium fluoborate10.1016/0169-4332(89)90009-3 ↗
27. X-ray photoelectron spectroscopy of some silicates10.1016/0009-2614(76)85029-4 ↗
28. Oxidation behavior of C/SiC composite with CVD SiC-B4C coating in a wet oxygen environment10.1007/s10443-008-9077-z ↗
29. Oxidation of silicon carbide in a wet atmosphere10.1007/BF01106816 ↗
30. Oxidation kinetics of chemical vapor deposited silicon carbide in wet oxygen10.1111/j.1151-2916.1994.tb05357.x ↗
31. Variation of the oxidation rate of silicon carbide with water-vapor pressure10.1111/j.1151-2916.1999.tb01810.x ↗
32. Corrosion of silicon-based ceramics in combustion environments10.1111/j.1151-2916.1993.tb03684.x ↗
33. Corrosion of non-oxide ceramic10.1016/S0272-8842(96)00008-9 ↗
34. Phase relations in the system boron oxide–silica10.1111/j.1151-2916.1965.tb11803.x ↗
35. High temperature crack sealant based on SiO2–B2O3 for SiC coating on carbon–carbon composites10.1163/156855103772658498 ↗
36. Effect of carbon and boron on the high-temperature oxidation of silicon carbide10.1111/j.1151-2916.1995.tb08918.x ↗
37. Yang · 2009 · 39