Pursuing enhanced oxidation resistance of ZrB2 ceramics by SiC and WC co-doping
Source abstract
Abstract
Abstract The oxidative degradation of ZrB2 ceramics is the main challenge for its extensive application under high temperature condition. Here, we report an effective method for co-doping suitable compounds into ZrB2 in order to significantly improve its anti-oxidation performance. The incorporation of SiC and WC into ZrB2 matrix is achieved using spark plasma sintering (SPS) at 1800 °C. The oxidation behavior of ZrB2-based ceramics is investigated in the temperature range of 1000 °C–1600 °C. The oxidation resistance of single SiC-doped ZrB2 ceramics is improved due to the formation of silica layer on the surface of the ceramics. As for the WC-doped ZrB2, a dense ZrO2 layer is formed which enhances the oxidation resistance. Notably, the SiC and WC co-doped ZrB2 ceramics with relative density of almost 100% exhibit the lowest oxidation weight gain in the process of oxidation treatment. Consequently, the co-doped ZrB2 ceramics have the highest oxidation resistance among all the samples.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · MXene and MAX Phase Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (26)
Show source-provided references
1. Oxidation-based materials selection for 2000°C + hypersonic aerosurfaces: theoretical considerations and historical experience10.1023/B:JMSC.0000041686.21788.77 ↗
2. Ultra High temperature ceramic composites
3. Effect of thermal exposure on strength of ZrB2-based composites with nano-sized SiC particles10.1016/j.compscitech.2008.06.021 ↗
4. Mechanical, thermal, and oxidation properties of refractory hafnium and zirconium compounds10.1016/S0955-2219(99)00129-6 ↗
5. Combined effects of WC and SiC on densification and thermo-mechanical stability of ZrB2 ceramics10.1016/j.matdes.2016.06.114 ↗
6. Advances in microstructure and mechanical properties of zirconium diboride based ceramics10.1016/S0921-5093(02)00520-8 ↗
7. Refractory diborides of zirconium and hafnium10.1111/j.1551-2916.2007.01583.x ↗
8. Thermal shock behavior of ZrB2–SiC ultra-high temperature ceramics with addition of zirconia10.1016/j.jallcom.2008.11.045 ↗
9. Oxidation mechanism and resistance of ZrB2–SiC composites10.1016/j.corsci.2009.07.005 ↗
10. Densification of ZrB2-based composites and their mechanical and physical properties: a review10.1016/j.jeurceramsoc.2008.11.008 ↗
11. Oxidation kinetics of hot-pressed ZrB2–SiC ceramic matrix composites10.1016/j.ceramint.2012.09.091 ↗
12. The ZrB2 volatility diagram10.1111/j.1551-2916.2005.00599.x ↗
13. Long-term oxidation behavior and mechanical strength degradation of a pressurelessly sintered ZrB2–MoSi2 ceramic10.1016/j.scriptamat.2005.07.026 ↗
14. Oxidation-resistant ZrB2–SiC composites at 2200°C10.1016/j.compscitech.2007.08.017 ↗
15. Oxidation of ZrB2-based ceramics in dry air10.1149/1.1618226 ↗
16. Improved oxidation resistance of zirconium diboride by tungsten carbide additions10.1111/j.1551-2916.2008.02713.x ↗
17. Oxidation of zirconium diboride with tungsten carbide additions10.1111/j.1551-2916.2010.04216.x ↗
18. Oxygen contamination on the surface of ZrB2 powders and its removal10.1016/j.scriptamat.2016.09.020 ↗
19. In situ microscopy observation of liquid flow, zirconia growth, and CO bubble formation during high temperature oxidation of zirconium diboride–silicon carbide10.1016/j.jeurceramsoc.2010.01.034 ↗
20. Oxidation of zirconium diboride–silicon carbide ceramics under an oxygen partial pressure of 200Pa: formation of zircon10.1016/j.corsci.2010.06.004 ↗
21. Oxidation of ZrB2–SiC ultra-high temperature composites over a wide range of SiC content10.1016/j.jeurceramsoc.2012.05.021 ↗
22. Thermodynamic analysis of ZrB2–SiC oxidation: formation of a SiC-depleted region10.1111/j.1551-2916.2006.01329.x ↗
23. Sublimation thermodynamics of tungsten trioxide10.1016/0021-9614(85)90018-7 ↗
24. Numerical data for some commonly used solid state reaction equations10.1111/j.1151-2916.1966.tb13289.x ↗
25. Kinetic analysis of thermogravimetric data10.1021/ac50159a046 ↗
26. Kinetics of high-temperature oxidation of inorganic nonmetallic materials10.1111/j.1551-2916.2008.02903.x ↗