Mechanical, thermal, and dielectric properties of SiCf/SiC composites reinforced with electrospun SiC fibers by PIP

Pengpeng Yu, Zijia Lin, Jie Yu

Publisher page

Abstract

Abstract Electrospun unidirectional SiC fibers reinforced SiCf/SiC composites (e-SiCf/SiC) were prepared with ∼10% volume fraction by polymer infiltration and pyrolysis (PIP) process. Pyrolysis temperature was varied to investigate the changes in microstructures, mechanical, thermal, and dielectric properties of e-SiCf/SiC composites. The composites prepared at 1100 °C exhibit the highest flexural strength of 286.0 ± 33.9 MPa, then reduced at 1300 °C, mainly due to the degradation of electrospun SiC fibers, increased porosity, and reaction-controlled interfacial bonding. The thermal conductivity of e-SiCf/SiC prepared at 1300 °C reached 2.663 W/(m∙K). The dielectric properties of e-SiCf/SiC composites were also investigated and the complex permittivities increase with raising pyrolysis temperature. The e-SiCf/SiC composites prepared at 1300 °C exhibited EMI shielding effectiveness exceeding 24 dB over the whole X band. The electrospun SiC fibers reinforced SiCf/SiC composites can serve as a potential material for structural components and EMI shielding applications in the future.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Electromagnetic wave absorption materials · Advanced ceramic materials synthesis · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (50)

Show source-provided references
1. A review of third-generation SiC fibers and SiCf/SiC composites10.1016/j.jmst.2019.07.020 ↗
2. Design, Preparation and properties of non-oxide CMCs for application in engines and nuclear reactors: An overview10.1016/S0266-3538(03)00230-6 ↗
3. Current status and recent research achievements in SiC/SiC composites10.1016/j.jnucmat.2014.06.003 ↗
4. Improved thermal conductivity of silicon carbide fibers-reinforced silicon carbide matrix composites by chemical vapor infiltration method10.1016/j.ceramint.2018.10.132 ↗
5. A review of absorption properties in silicon-based polymer derived ceramics10.1016/j.jeurceramsoc.2016.02.002 ↗
6. Thermal and mechanical properties of SiC/SiC-CNTs composites fabricated by CVI combined with electrophoretic deposition10.1016/j.msea.2014.12.105 ↗
7. Enhanced thermal and mechanical properties of optimized SiCf/SiC composites with in-situ CNTs on PyC interface10.1016/j.ceramint.2020.04.126 ↗
8. Mechanical properties and strengthening mechanism of SiCf/SiC mini-composites modified by SiC nanowires10.1016/j.ceramint.2020.09.008 ↗
9. Effect of fiber directionality on the static and dynamic mechanical properties of 3D SiCf/SiC composites10.1016/j.msea.2016.02.006 ↗
10. Fabrication of SiCf/SiC composites by chemical vapor infiltration and vapor silicon infiltration10.1016/j.matlet.2010.05.013 ↗
11. Influence of pyrolytic carbon interface thickness on microstructure and mechanical properties of SiC/SiC composites by NITE process10.1016/j.compscitech.2007.05.037 ↗
12. Enchanced high-temperature performances of SiC/SiC composites by high densification and crystalline structure10.1016/j.compscitech.2010.11.026 ↗
13. Properties and microstructure evolution of Cf/SiC composites fabricated by polymer impregnation and pyrolysis (PIP) with liquid polycarbosilane
14. Effect of degree of crystallinity on elastic properties of silicon carbide fabricated using polymer pyrolysis10.1016/j.jeurceramsoc.2016.06.010 ↗
15. Effect of pyrolysis temperature on the mechanical evolution of SiCf/SiC composites fabricated by PIP10.1016/j.ceramint.2019.09.087 ↗
16. Processing-temperature dependent micro- and macro-mechanical properties of SiC fiber reinforced SiC matrix composites10.1016/j.compositesb.2017.07.079 ↗
17. Appropriate thickness of pyrolytic carbon coating on SiC fiber reinforcement to secure reasonable quasi-ductility on NITE SiC/SiC composites10.1016/j.ceramint.2018.07.158 ↗
18. Mechanical properties of the SiCf/SiC composites reinforced with KD-I and KD-II fibers fabricated assisted by a microwave heating method10.1016/j.ceramint.2019.03.223 ↗
19. Influence of surface fibre properties and textural organization of a pyrocarbon interphase on the interfacial shear stress of SiC/SiC minicomposites reinforced with Hi-Nicalon S and Tyranno SA3 fibres10.1016/j.jeurceramsoc.2013.08.027 ↗
20. High temperature electromagnetic wave absorption properties of SiCf/Si3N4 composite induced by diff ;erent SiC fIbers10.1016/j.ceramint.2018.12.142 ↗
21. Highly aligned polyacrylonitrile-based nano-scale carbon fibers with homogeneous structure and desirable properties10.1016/j.compscitech.2013.08.001 ↗
22. Strong electrospun nanometer-diameter polyacrylonitrile carbon fiber yarns10.1016/j.carbon.2009.06.027 ↗
23. Highly flexible and strong SiC fiber mats prepared by electrospinning and hot-drawing10.1080/17436753.2021.1904767 ↗
24. Preparation and characterization of SiC fibers with diverse electrical resistivity through pyrolysis under reactive atmospheres10.1016/j.jeurceramsoc.2016.09.023 ↗
25. The subtracting pore effect method as an accurate and reliable surface area determination of porous carbons10.1016/j.carbon.2020.12.075 ↗
26. Characterization of diamond films by Raman spectroscopy10.1557/JMR.1989.0385 ↗
27. Effects of temperature and atmosphere on microstructural evolution and mechanical properties of KD-II SiC fibers10.1016/j.ceramint.2020.06.225 ↗
28. Enhanced mechanical and dielectric properties of SiCf/SiC composites with silicon oxycarbide interphase10.1016/j.ceramint.2017.09.222 ↗
29. the effects of the SiC precursors on the microstructures and mechanical properties of SiCf/SiC composites prepared via Polymer impregnation and pyrolysis process10.1016/j.ceramint.2014.11.112 ↗
30. Mechanical properties of SiC/SiC composites with PyC and the BN interface10.1016/j.ceramint.2015.02.041 ↗
31. Mechanical and dielectric properties of SiCf/SiC composites fabricated by PIP combined with CIP process10.1016/j.ceramint.2016.01.057 ↗
32. Influence of the carbon interface on the mechanical behavior of SiC/SiC composites10.1016/j.compositesa.2020.105867 ↗
33. Effects of the fiber surface characteristics on the interfacial microstructure and mechanical properties of the KD SiC fiber reinforced SiC matrix composites10.1016/j.msea.2009.07.018 ↗
34. Microstructural investigations of the pyrocarbon interphase in SiC fiber-reinforced SiC matrix composites10.1016/j.matlet.2009.06.040 ↗
35. Microstructural instability and the resultant strength of Si-C-O (Nicalon) and Si-N-C-O (HPZ) fibres10.1016/0955-2219(95)00178-6 ↗
36. Effects of BN/SiC dual-layer interphase on mechanical and dielectric properties of SiCf/SiC composites10.1016/j.ceramint.2013.09.091 ↗
37. Effect of SiC nanowires on the mechanical properties and thermal conductivity of 3D-SiCf/SiC composites prepared via precursor infiltration pyrolysis10.1016/j.jeurceramsoc.2021.04.003 ↗
38. Theoretical consideration of the effect of porosity on thermal conductivity of porous materials10.1007/s10934-006-8043-0 ↗
39. Microstructure design and control for improvement of thermal conductivity of SiCf/SiC composites10.1016/j.jnucmat.2013.03.008 ↗
40. Effect of grain growth on the thermal conductivity of liquid-phase sintered silicon carbide ceramics10.1016/j.jeurceramsoc.2017.04.050 ↗
41. Grain size dependence of the thermal conductivity of polycrystalline chemical vapor deposited SiC at low temperatures10.1063/1.346852 ↗
42. Parallel aligned nickel nanocone arrays for multiband microwave absorption10.1021/acsami.0c04247 ↗
43. Enhanced mechanical and microwave absorption properties of SiCf/SiC composite using aluminum powder as active filler10.1016/j.jallcom.2019.03.171 ↗
44. Complex permittivity and microwave absorbing properties of SiC fiber woven fabrics10.1007/s10853-010-5140-x ↗
45. Effect of pyrolysis temperatures on the performance of SiCf/SiC composites10.1016/j.fusengdes.2017.04.056 ↗
46. Enhancement of the microwave absorption properties of PyC-SiCf/SiC composites by electrophoretic deposition of SiC nanowires on SiC fibers10.1016/j.ceramint.2019.12.185 ↗
47. Effects of upgrading temperature on electromagnetic shielding properties of three-dimensional graphene/SiBCN/SiC ceramic composites10.1016/j.ceramint.2019.07.110 ↗
48. Effect of carbon nanotubes on the electromagnetic shielding properties of SiCf/SiC composites10.1016/j.jallcom.2018.02.166 ↗
49. Effects of SiC fibers on microwave absorption and electromagnetic interference shielding properties of SiCf/SiCN composites10.1016/j.ceramint.2016.09.089 ↗
50. Temperature-dependent electromagnetic shielding properties of SiCf/BN/SiC composites fabricated by chemical vapor infiltration process10.1016/j.jallcom.2017.07.084 ↗