journal article·2012-08Open access

Effect of temperature on friction and wear behaviour of CuO–zirconia composites

Mahdiar Valefi, Matthijn de Rooij, Dirk J. Schipper, Louis Winnubst

Abstract

Results of wear tests using an alumina ball sliding against 5 wt% copper oxide doped tetragonal zirconia polycrystalline (CuO-TZP) ceramics are reported as a function of temperature up to 700 °C. The specific wear rate and friction coefficient are strongly dependent on temperature. Below a critical temperature (T < 600 °C), CuO-TZP showed a high coefficient of friction as well as a high wear rate. This was ascribed to the formation of a rough surface, caused by brittle fracture and abrasive wear, based on observations by scanning electron microscopy (SEM), laser scanning microscopy (LSM) and X-ray photoelectron spectroscopy (XPS). However, above 600 °C a self-healing layer is formed at the interface and results in low friction and wear. The mechanism of layer formation and restoration is discussed and rationalized by onset of plastic deformation caused by a reduction reaction of CuO to Cu2O at high temperatures.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced materials and composites · Advanced ceramic materials synthesis · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (38)

Show source-provided references
1. Self-healing behaviour in man-made engineering materials: bioinspired but taking into account their intrinsic character10.1098/rsta.2009.0020 ↗
2. Surface self-organization: from wear to self-healing in biological and technical surfaces10.1016/j.apsusc.2010.01.061 ↗
3. Nature's hierarchical materials10.1016/j.pmatsci.2007.06.001 ↗
4. Ceramic wear maps: zirconia10.1111/j.1151-2916.1993.tb08315.x ↗
6. Tribological properties of nanoscale alumina–zirconia composites10.1016/S0043-1648(98)00403-7 ↗
7. Microstructure and tribological properties of ZrO2(Y2O3) matrix composites doped with different solid lubricants from room temperature to 800°C10.1016/j.wear.2008.11.017 ↗
8. Effect of temperature on friction and oscillating sliding wear of dense and porous 3Y-TZP zirconia ceramics10.1016/0301-679X(94)90075-2 ↗
9. High-temperature tribological properties of strontium sulfate films formed on zirconia–alumina, alumina and silicon nitride substrates10.1016/j.triboint.2006.02.054 ↗
10. Environmental effects on friction and wear of dry sliding zirconia and alumina ceramics doped with copper oxide10.1016/j.ijrmhm.2005.05.001 ↗
11. NiAl matrix high-temperature self-lubricating composite10.1007/s11249-010-9727-9 ↗
12. Ni3Al matrix high temperature self-lubricating composites10.1016/j.triboint.2010.11.016 ↗
13. Friction reduction by adding copper oxide into alumina and zirconia ceramics10.1016/S0043-1648(03)00267-9 ↗
14. Further investigation on the tribological behaviour of Al2O3–20Ag20 CaF2 composite at 650°C10.1023/A:1019132328220 ↗
15. A mechanical model for surface layer formation on self-lubricating ceramic composites10.1016/j.wear.2010.01.012 ↗
16. High temperature tribological and self-lubricating behaviour of copper oxide-doped Y-TZP composite sliding against alumina10.1111/j.1551-2916.2011.04899.x ↗
17. The effect of alumina counterface on the friction reduction of CuO/3Y-TZP composite at room temperature10.1016/j.wear.2011.08.016 ↗
18. Effect of microstructure on the tribological and mechanical properties of CuO-doped 3Y-TZP ceramics10.1111/j.1551-2916.2007.01823.x ↗
19. A critical evaluation of indentation techniques for measuring fracture toughness: I, direct crack measurements10.1111/j.1151-2916.1981.tb10320.x ↗
20. Mechanical properties of CuO10.1515/HTMP.1990.9.1.1 ↗
21. Average grain size in polycrystalline ceramics10.1111/j.1151-2916.1969.tb11975.x ↗
22. Lubrication behaviour of Y-TZP/Al2O3/Mo nanocomposites at high temperature10.1016/j.wear.2010.01.009 ↗
23. High temperature friction and wear testing of silicon nitride ceramics10.1016/0301-679X(95)00020-5 ↗
24. Observations on the sliding wear of ceramics10.1080/05698198508981618 ↗
25. Wear transition diagram for silicon carbide10.1016/0301-679X(96)85544-7 ↗
26. 1992
27. Genesis and role of wear debris in sliding wear of ceramics10.1016/S0043-1648(00)00465-8 ↗
28. Sliding friction of ceramics: mechanical action of the wear debris10.1007/BF00575394 ↗
29. Wear of advanced ceramics10.1016/S0043-1648(02)00240-5 ↗
30. Sliding wear of silicon carbide–titanium boride ceramic–matrix composite10.1111/j.1151-2916.1993.tb03815.x ↗
31. Sintering behaviour of 0.8 mol%-CuO-doped 3Y-TZP ceramics10.1111/j.1551-2916.2005.00679.x ↗
32. Thermal analysis of 3-mol%-yttria-stabilized tetragonal zirconia powder doped with copper oxide10.1111/j.1151-2916.1996.tb08135.x ↗
33. Metallurgical
34. Reduction of metal oxides by mechanical alloying method10.1016/S0167-2738(97)00277-4 ↗
35. Plastic deformation of cuprous oxide10.1111/j.1151-2916.1968.tb11843.x ↗
36. The third-body approach: a mechanical view of wear10.1016/0043-1648(84)90025-5 ↗
37. Wear modeling and the third body concept10.1016/j.wear.2006.10.011 ↗
38. How third-body processes affect friction and wear10.1557/S088376940003061X ↗