Densification and mechanical properties of pulsed electric current sintered B4C with in situ synthesized Al3BC obtained by the molten-salt method
Source abstract
Abstract
Abstract The in situ generated ternary compound Al 3 BC shows good dispersion on the surfaces of B 4 C particles (10 ± 0.6 μm), obtained using the molten-salt method rather than the ball-milling method, which can form a conductive network in the pulse electric current sintering process to improve the sinterability of B 4 C. The sintering behaviour, microstructure and mechanical properties of compacts were investigated at different sintering temperatures and Al 3 BC contents. The study found that the relative density, elastic modulus, Vickers hardness, and fracture toughness of samples reached as high as 100%, 495 GPa, 37.0 GPa, and 6.32 MPa m 1/2 at 1700 °C, respectively, when the content of Al 3 BC was 18 wt.%. The crack propagation mode can provide an explanation for the higher toughness than that of pure B 4 C (3.19 MPa m 0.5 ). Additionally, the good dispersion of Al 3 BC in B 4 C was found to change the fracture mode from the single transgranular mode to a mixture of intergranular and transgranular modes. The compositions of the compacts were almost pure B 4 C.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Aluminum Alloys Composites Properties · Boron and Carbon Nanomaterials Research · Advanced ceramic materials synthesis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (35)
Show source-provided references
1. Engineering properties of carbides
2. Hardness and wear resistance of B4C ceramics prepared with several additives10.1016/j.matlet.2005.04.047 ↗
3. Gamma and neutron attenuation behaviours of boron carbide-silicon carbide composites10.1016/j.anucene.2014.03.026 ↗
4. High-temperature fracture of boron-carbide – experiments and simple theoretical-models10.1007/BF02403232 ↗
5. SiC-B4C composites for synergistic enhancement of thermoelectric property10.1016/S0955-2219(03)00213-9 ↗
6. Processing and mechanical properties of boron carbide sintered with TiC10.1016/S0955-2219(98)00071-5 ↗
7. Pressure sintering and microstructural development of B4C–TiB2 composites10.1111/j.1551-2916.1988.tb00169.x ↗
8. Densification and mechanical properties of B4C with Al2O3 as a sintering aid10.1111/j.1151-2916.2000.tb01647.x ↗
9. Ductile phase toughening and R-curve behavior in a B4C-AL cermet10.1007/BF01117938 ↗
10. Reactive formation of coatings at boron-carbide interface with Ti and Cr powders10.1016/0955-2219(95)00014-L ↗
11. Structure and properties of boron carbide with aluminum incorporation10.1016/S0921-5107(99)00597-8 ↗
12. Influence of spark plasma sintering parameters on densification and mechanical properties of boron carbide10.1016/j.ijrmhm.2013.09.004 ↗
13. Sintering behavior and mechanical properties of B4C ceramics fabricated by spark plasma sintering
14. Toughening of super-hard ultra-fine grained B4C densified by spark-plasma sintering via SiC addition10.1016/j.jeurceramsoc.2013.01.018 ↗
15. Densification and mechanical properties of spark plasma sintered B4C with Si as a sintering aid10.1111/j.1551-2916.2010.03931.x ↗
16. The effect of electric field and pressure on the synthesis and consolidation of materials: a review of the spark plasma sintering method10.1007/s10853-006-6555-2 ↗
17. Synthesis of Al8B4C7 ceramic powder from Al/B4C/C mixtures10.1016/j.powtec.2012.05.001 ↗
18. Chemical composition and microstructure of Al3BC3 prepared by different densification methods10.1016/j.jeurceramsoc.2009.09.027 ↗
19. Al-B-C phase development and effects on mechanical-properties of B4C/AL-derived composites10.1111/j.1151-2916.1995.tb08801.x ↗
20. Composition and lattice-parameters of a new aluminum-rich borocarbide10.1007/BF00728915 ↗
21. First-principles prediction of low shear-strain resistance of Al3BC3: a metal borocarbide containing short linear BC2 units10.1063/1.2220549 ↗
22. Synthesis and crystal structure of Al3BC, the first boride carbide of aluminium10.1016/S0925-8388(96)02721-1 ↗
23. Madsen · 2008
24. X’Pert HighScore Plus · 2012
25. Data · 2000
26. Linear intercept technique for measuring grain-size in 2-phase polycrystalline ceramics10.1111/j.1151-2916.1972.tb11224.x ↗
27. A critical-evaluation of indentation techniques for measuring fracture-toughness. 1. Direct crack measurements10.1111/j.1151-2916.1981.tb10320.x ↗
28. Al3BC3 powder: processing and synthetic mechanism10.1111/j.1551-2916.2009.03292.x ↗
29. Processing of boron carbide-aluminum composites10.1111/j.1151-2916.1989.tb06216.x ↗
30. Identification of novel dual-scale Al3BC particles in Al based composites10.1016/j.matdes.2015.12.104 ↗
31. Processing and microstructural characterisation of AA 1070 and AA 6063 matrix B4Cp reinforced composites10.1016/j.matdes.2009.11.064 ↗
32. Preparation of Al2O3-TiB2 nanocomposite powder by mechanochemical reaction between Al, B2O3 and Ti10.1016/j.apt.2010.07.010 ↗
33. Equation of state and thermal stability of Al3BC10.1016/j.ssc.2006.01.015 ↗
34. Thermal stability of Al3BC310.1111/j.1551-2916.2009.03171.x ↗
35. Mechanical properties of nanocrystalline materials10.1016/j.pmatsci.2005.08.003 ↗