journal article·2019-04

Improved shear strength of SiC-coated 3D C/SiC composite joints with a tailored Ti-Si-C interlayer

Xing Zhao, Liuyang Duan, Yiguang Wang

Publisher page

Abstract

Abstract SiC-coated 3D C/SiC composites were successfully joined using SPS technology with a Ti-Si-C interlayer. The interface morphologies, phase composition, and mechanical properties of the joints were investigated in detail. By adjusting the joining temperature, the interlayer transitioned, in situ, from Ti-Si-C compounds to Ti3SiC2 grains without decomposition. Because of the plastic deformation behavior of Ti3SiC2 grains, the ability of the interlayer to inhibit crack propagation increased. For joints with different interlayer thickness, the distribution of thermal residual stress was calculated using finite element analysis, and the distribution was associated with the evolution of interlayer morphologies, which was eventually used to establish fracture models. Optimized bonding was achieved without erosion of carbon fibers and also without interfacial defects. Finally, a reliable joint with shear strength of 51 ± 3.0 MPa was obtained by precisely controlling the interlayer reaction and optimizing thermal residual stress.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · MXene and MAX Phase Materials · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (33)

Show source-provided references
1. Design, preparation and properties of non-oxide CMCs for application in engines and nuclear reactors: an overview10.1016/S0266-3538(03)00230-6 ↗
2. Joining of C/SiC composites by spark plasma sintering technique10.1016/j.jeurceramsoc.2013.10.028 ↗
3. Postirradiation fiber debonding and pull-out in SiC-SiC composites10.1016/0022-3115(94)90174-0 ↗
4. Joining of ceramic matrix composites to high temperature ceramics for thermal protection systems10.1016/j.jeurceramsoc.2015.09.038 ↗
5. Ablation behavior of C/SiC-HfC composites in the plasma wind tunnel10.1016/j.jeurceramsoc.2016.03.017 ↗
6. Secure tightening of a CMC fastener for the heat shield of re-entry vehicles10.1016/j.compstruct.2009.07.002 ↗
7. Shear and bending strength of SiC/SiC joined by a modified commercial adhesive10.1111/j.1744-7402.2011.02739.x ↗
8. Effect of brazing parameters on microstructure and mechanical properties of Cf/SiC and Nb-Zr joints brazed with Ti-Co-Nb filler alloy10.1016/j.jeurceramsoc.2016.09.031 ↗
9. Reactive brazing Cf/SiC to itself and to Mo using the NiPdPtAu-Cr filler alloy10.1016/j.jeurceramsoc.2017.05.025 ↗
10. Interfacial microstructure and mechanical property of ZrC-SiC ceramic and Ti6Al4V joint brazed with AgCuTi alloy10.1016/j.jeurceramsoc.2017.02.056 ↗
11. Microstructure characteristic and its influence on the strength of SiC ceramic joints diffusion bonded by spark plasma sintering10.1016/j.ceramint.2017.11.185 ↗
12. Effects of z-pin’s porosity on shear properties of 2D C/SiC z-pinned joint10.1016/j.compstruct.2017.04.013 ↗
13. A new partial transient liquid-phase bonding process with powder-mixture interlayer for bonding Cf/SiC composite and Ti-6Al-4V alloy10.1016/j.matlet.2014.12.110 ↗
14. Fast joining SiC ceramics with Ti3SiC2 tape film by electric field-assisted sintering technology10.1016/j.jnucmat.2015.08.004 ↗
15. Joining of carbon fiber reinforced carbon composites with Ti3SiC2 tape film by electric field assisted sintering technique10.1016/j.carbon.2016.02.036 ↗
16. Joining of CVD SiC coated and uncoated fibre reinforced ceramic matrix composites with pre-sintered Ti3SiC2 MAX phase using Spark Plasma Sintering10.1016/j.jeurceramsoc.2016.06.025 ↗
17. High temperature properties of the monolithic CVD beta-SiC materials joined with a pre-sintered MAX phase Ti3SiC2 interlayer via solid-state diffusion bonding10.1016/j.jeurceramsoc.2016.11.006 ↗
18. Flash joining of CVD-SiC coated Cf/SiC composites with a Ti interlayer10.1016/j.jeurceramsoc.2017.05.016 ↗
19. Thickness-dependent phase evolution and bonding strength of SiC ceramics joints with active Ti interlayer10.1016/j.jeurceramsoc.2016.12.009 ↗
20. Room-temperature ductile carbides10.1007/s11661-999-0325-0 ↗
21. Modeling thermal and irradiation-induced swelling effects on the integrity of Ti3SiC2/SiC joints10.1016/j.jnucmat.2017.09.011 ↗
22. Barsoum · 2013
23. Microstructure and properties of dense Tyranno-ZMI SiC/SiC containing Ti3Si(Al)C2 with plastic deformation toughening mechanism10.1016/j.jeurceramsoc.2017.10.052 ↗
24. Micro-scale plastic deformation of polycrystalline Ti3SiC2 under room-temperature compression10.1016/S0955-2219(00)00310-1 ↗
25. Elastic and mechanical properties of the MAX phases
26. Processing and mechanical properties of Ti3SiC2: II, effect of grain size and deformation temperature10.1111/j.1151-2916.1999.tb02167.x ↗
27. Microstructure and mechanical properties of SiC-SiC joints joined by spark plasma sintering10.1016/j.ceramint.2016.06.049 ↗
28. Thermal properties of Ti3SiC210.1016/S0022-3697(98)00313-8 ↗
29. Investigation of thermal expansion of 3D-stitched C-SiC composites10.1016/j.jeurceramsoc.2009.04.005 ↗
30. Handbook of SiC properties for fuel performance modeling10.1016/j.jnucmat.2007.05.016 ↗
31. Pressureless sintering and reaction mechanisms of Ti3SiC2 ceramics10.1111/jace.12903 ↗
32. Joining of Cf-SiC composites and ZrB2-SiC based composites for ultra high temperature applications10.1016/j.ceramint.2018.03.080 ↗
33. Microstructure and mechanical properties of low-activation glass-ceramic joining and coating for SiC/SiC composites10.1016/S0022-3115(00)00096-9 ↗