journal article·2020-04Open access

Reaction-bond composite synthesis of SiC-TiB2 by spark plasma sintering/field-assisted sintering technology (SPS/FAST)

Corson L. Cramer, Jacob W. McMurray, Michael J. Lance, Richard A. Lowden

Abstract

Abstract High-density SiC-TiB2 composites were fabricated using the displacement reaction spark plasma sintering/field-assisted sintering technology (SPS/FAST) and SiC, B4C, TiC, and Si powders. The reaction process was performed in a narrow time frame compared hot pressing. The SiC-TiB2 composites were sintered with precursor SiC at various pressures to determine the effects of processing with SPS/FAST. The composites completed synthesis during SPS/FAST processing, which occurs more quickly than hot pressing. SEM, STEM, and Raman spectroscopy are used to show the conversion and microstructure. The composite of 53.6 wt.% SiC and 46.4 wt.% TiB2 has 99 % theoretical density, hardness of 26.4 GPa, and fracture toughness of 5.12 MPa m1/2.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (41)

Show source-provided references
1. Densification and grain growth during microwave sintering of titanium diboride10.1016/j.scriptamat.2013.07.012 ↗
2. Processing and properties of monolithic TiB 2 based materials10.1179/174328006X102529 ↗
3. Advances in silicon carbide science and technology at the micro- and nanoscales10.1116/1.4807902 ↗
4. Microstructural effects on the mechanical properties of SiC-15 vol% TiB2 particulate-reinforced ceramic composites
5. In situ platelet-toughened TiB2–SiC composites prepared by reactive pulsed electric current sintering10.1016/j.scriptamat.2011.03.015 ↗
6. Sliding wear of silicon carbide-titanium boride ceramic-matrix composite10.1111/j.1151-2916.1993.tb03815.x ↗
7. Sintering of covalent solids10.1111/j.1151-2916.1976.tb10979.x ↗
8. Liquid phase sintering of SiC with additions of Y2O3, Al2O3 and SiO210.1016/j.jeurceramsoc.2003.09.002 ↗
9. In-situ synthesized TiB2 toughened SiC10.1016/0955-2219(95)00116-6 ↗
10. Sintering of in-situ synthesized Sic-TiB2 composites with improved fracture toughness10.1111/j.1151-2916.1992.tb05600.x ↗
11. Silicon carbide–titanium diboride ceramic composites10.1016/j.jeurceramsoc.2013.03.031 ↗
12. Pressureless sintering of internally synthesized SiC-TiB2 composites with improved fracture strength10.1016/j.jallcom.2010.09.152 ↗
13. SiC matrix composites reinforced with internally synthesized TiB210.1007/BF00544201 ↗
14. Reaction synthesis of TiB2-SiC composites from TiH2-Si-B4C10.1016/0167-577X(95)00159-X ↗
15. TiB2-Ti(C, N)-SiC composites prepared by reactive hot pressing10.1007/BF01855600 ↗
16. Combustion synthesis/dynamic densification of a TiB2-SiC composite10.1111/j.1151-2916.1996.tb07896.x ↗
17. TiC–TiB2 composites: a review of phase relationships, processing and properties10.1016/j.jeurceramsoc.2007.11.011 ↗
18. Microstructural evolution during transient plastic phase processing of titanium carbide-titanium boride composites10.1111/j.1151-2916.1996.tb08017.x ↗
19. Microstructure and mechanical properties of TiB2–SiC ceramic composites by Reactive Hot Pressing10.1016/j.ijrmhm.2013.10.007 ↗
20. A study on in-situ synthesis of TiB2–SiC ceramic composites by reactive hot pressing10.1016/j.ceramint.2013.07.152 ↗
21. Synthesis mechanism and mechanical properties of TiB2–SiC composites fabricated with the B4C–TiC–Si system by reactive hot pressing10.1016/j.jallcom.2014.09.030 ↗
22. Effects of particle size of raw materials on the characteristics of TiB2–SiC composites fabricated from B4C, TiC and Si powders
23. Field-assisted sintering technology/spark plasma sintering: mechanisms, materials, and technology developments10.1002/adem.201300409 ↗
24. Simultaneous spark plasma synthesis and densification of TiC-TiB2 composites10.1111/j.1551-2916.2005.00832.x ↗
25. Rapid fabrication of Ti3SiC2–SiC nanocomposite using the spark plasma sintering-reactive synthesis (SPS-RS) method10.1016/j.scriptamat.2006.09.029 ↗
26. Electric current activation of sintering: a review of the pulsed electric current sintering process10.1111/j.1551-2916.2010.04210.x ↗
27. Microstructural evolution during silicon carbide (SiC) formation by liquid silicon infiltration using optical microscopy
28. Formation mechanism of spherical TiC in Ni-Ti-C system during combustion synthesis10.3390/ma10091007 ↗
29. Characterization of aluminosilicate zeolites by UV Raman spectroscopy10.1016/S1387-1811(01)00271-2 ↗
30. Atomic structure of amorphous shear bands in boron carbide10.1038/ncomms3483 ↗
31. Pressure-induced depolarization and resonance in Raman scattering of single-crystalline boron carbide10.1103/PhysRevB.81.060102 ↗
32. Indentation fracture of WC-Co cermets10.1007/BF00555296 ↗
33. Fracture toughness of cemented carbides: testing method and microstructural effects
34. A critical evaluation of indentation techniques for measuring fracture toughness: II, strength method10.1111/j.1151-2916.1981.tb10321.x ↗
35. Direct comparison between hot pressing and electric field-assisted sintering of submicron alumina10.1016/j.actamat.2009.07.043 ↗
36. FactSage thermochemical software and databases10.1016/S0364-5916(02)00035-4 ↗
37. Combustion synthesis of advanced materials: principles and applications
38. A model for boundary diffusion controlled creep in polycrystalline materials10.1063/1.1702656 ↗
39. Evidence for Coble creep in the relaxation of surface‐compressive stresses in tempered polycrystalline aluminum oxide10.1063/1.1663851 ↗
40. Diffusion-accommodated grain boundary sliding and dislocation glide in the creep of sintered alpha silicon carbide10.1111/j.1151-2916.1992.tb07198.x ↗
41. Flexural strength, fracture toughness, and hardness of silicon carbide and boron carbide armor ceramics10.1111/j.1744-7402.2010.02501.x ↗