Abstract Monolithic SiC, for the first time, was successfully joined using a SiC whisker-reinforced Ti3SiC2 composite (SiCw/Ti3SiC2) filler via electric field-assisted sintering technique. A thin Ti coating layer was formed on the SiC surface to minimize the residual stress at the joint interface by transforming it into a TiC gradient layer. After optimizing process parameters, a joint strength higher than 250 MPa was obtained, which is higher than the other values reported in the literature. Failure occurred at the SiC base rather than the joining interface because of the improved joint strength by the incorporation of SiCw. The addition up to 15 wt. % SiCw in the filler layer improved the joint strength by various strengthening mechanisms. On the other hand, the joint strength was lower with 20 wt. % SiCw addition, indicating the importance of thermal expansion mismatch between SiCw and Ti3SiC2 to obtain a sound SiC joint.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · MXene and MAX Phase Materials · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (39)
Show source-provided references
1. Continuous SiC fiber, CVI SiC matrix composites for nuclear applications: properties and irradiation effects10.1016/j.jnucmat.2013.06.040 ↗
2. Radiation-tolerant joining technologies for silicon carbide ceramics and composites10.1016/j.jnucmat.2013.10.002 ↗
3. KD-S SiCf/SiC composites with BN interface fabricated by polymer infiltration and pyrolysis process10.1007/s40145-018-0268-2 ↗
4. Handbook of SiC properties for fuel performance modeling10.1016/j.jnucmat.2007.05.016 ↗
5. Recent progress in the development of SiC composites for nuclear fusion applications10.1016/j.jnucmat.2018.06.017 ↗
6. Current status and prospects of SiCf/SiC for fusion structural applications10.1016/j.jeurceramsoc.2013.02.013 ↗
7. Effect of BNNTs/matrix interface tailoring on toughness and fracture morphology of hierarchical SiCf/SiC composites10.1007/s40145-019-0338-0 ↗
8. Recent advances in joining of SiC-based materials (monolithic SiC and SiCf/SiC composites): joining processes, joint strength, and interfacial behavior10.1007/s40145-018-0297-x ↗
9. Joining of β-SiC by spark plasma sintering10.1016/j.jeurceramsoc.2013.12.023 ↗
10. Thickness-dependent phase evolution and bonding strength of SiC ceramics joints with active Ti interlayer10.1016/j.jeurceramsoc.2016.12.009 ↗
11. Microstructure of reaction layer and its effect on the joining strength of SiC/SiC joints brazed using Ag-Cu-In-Ti alloy10.1007/s40145-014-0095-z ↗
12. Interfacial microstructure and mechanical properties of SiC joints achieved by reactive air brazing using Ag-V2O5 filler10.1016/j.jeurceramsoc.2019.03.013 ↗
13. A novel high entropy CoFeCrNiCu alloy filler to braze SiC ceramics10.1016/j.jeurceramsoc.2020.03.044 ↗
14. Solid-state joining of SiC using a thin Ti3AlC2, TiC, or Ti filler10.1016/j.jeurceramsoc.2019.09.031 ↗
15. In-situ formation of fine-grained carbide composite interlayer during diffusion bonding of SiC ceramic10.1016/j.jallcom.2018.06.013 ↗
16. High-strength SiC joints with a novel in-situ formed SiC/Al4SiC4 joining filler10.1016/j.jeurceramsoc.2020.07.041 ↗
17. Direct bonding of silicon carbide ceramics sintered with yttria10.1016/j.jeurceramsoc.2019.07.034 ↗
18. Microstructure and properties of SiCf/SiC joint brazed by Y-Al-Si-O glass10.1016/j.ceramint.2018.02.092 ↗
19. Flash joining of conductive ceramics in a few seconds by flash spark plasma sintering10.1016/j.jeurceramsoc.2019.07.036 ↗
20. Joining of SiCf/SiC using polycarbosilane and polysilazane preceramic mixtures10.1016/j.ceramint.2018.03.061 ↗
21. Nano-infiltration and transient eutectic (NITE) phase joining SiC ceramics at 1500 degrees C10.1016/j.ceramint.2019.08.193 ↗
22. Joining of SiCf/SiC using a layered Ti3SiC2-SiCw and TiC gradient filler10.1016/j.jeurceramsoc.2019.11.080 ↗
23. Joining of SiC monoliths using a thin MAX phase tape and the elimination of joining layer by solid-state diffusion10.1016/j.jeurceramsoc.2018.04.006 ↗
24. Pressureless joining of silicon carbide using Ti3SiC2 MAX phase at 1500 ℃10.1016/j.ceramint.2020.02.155 ↗
25. Low pressure joining of SiCf/SiC composites using Ti3AlC2 or Ti3SiC2 MAX phase tape10.4191/kcers.2017.54.4.08 ↗
26. Joining of CVD-SiC coated and uncoated fibre reinforced ceramic matrix composites with pre-sintered Ti3SiC2 MAX phase using spark plasma sintering10.1016/j.jeurceramsoc.2016.06.025 ↗
27. SiC ceramics joined with an in-situ reaction gradient layer of TiC/Ti3SiC2 and interface stress distribution simulations10.1016/j.ceramint.2018.05.255 ↗
28. The critical issues of SiC materials for future nuclear systems10.1016/j.scriptamat.2017.03.001 ↗
29. Fabrication of SiCf/Ti3SiC2 by the electrophoresis of highly dispersed Ti3SiC2 powder10.1016/j.ceramint.2020.04.138 ↗
30. A general Lewis acidic etching route for preparing MXenes with enhanced electrochemical performance in non-aqueous electrolyte10.1038/s41563-020-0657-0 ↗
31. Damage tolerance of Ti3SiC2 to high energy iodine irradiation10.1016/j.apsusc.2012.03.022 ↗
32. High temperature properties of the monolithic CVD β-SiC materials joined with a pre-sintered MAX phase Ti3SiC2 interlayer via solid-state diffusion bonding10.1016/j.jeurceramsoc.2016.11.006 ↗
33. Joining of SiC ceramic-based materials with ternary carbide Ti3SiC210.1016/j.mseb.2010.09.002 ↗
34. Fast joining SiC ceramics with Ti3SiC2 tape film by electric field-assisted sintering technology10.1016/j.jnucmat.2015.08.004 ↗
35. Thermal properties of Ti3SiC210.1016/S0022-3697(98)00313-8 ↗
36. Residual thermal stress of SiC/Ti3SiC2/SiC joints calculation and relaxed by post-annealing10.1111/ijac.12900 ↗
37. Fabrication of SiCw/Ti3SiC2 composites with improved thermal conductivity and mechanical properties using spark plasma sintering10.1007/s40145-020-0389-2 ↗
38. Reactions between Ti and Ti3SiC2 in temperature range of 1273-1573K
39. Thermal expansion anisotropy of ternary titanium silicides based on Ti5Si310.1016/j.actamat.2004.04.033 ↗