Abstract The reliable brazing of the ZTA ceramic joints was successfully obtained using Ni-Ti filler metal. The microstructure and mechanical properties of the joints brazed at different temperatures were investigated. During the process of brazing, both Al2O3 and ZrO2 in the ZTA reacted with the Ni-Ti filler, resulting in the formation of the AlNi2Ti + Ni2Ti4O reaction layer adjacent to the ZTA substrate when brazed at 1350 °C for 30 min. NiTi and Ni3Ti compounds precipitated at the center of brazing seam. When the brazing temperature increased from 1320 °C to 1380 °C, the thickness of AlNi2Ti + Ni2Ti4O layer increased gradually. As the brazing temperature varied from 1400 °C to 1450 °C, TiO was formed adjacent to the ZTA substrate, along with the reduction of Ni2Ti4O. AlNi2Ti distributed at the interface and center of brazing seam. The maximum shear strength of 152 MPa was obtained when brazed at 1420 °C for 30 min.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Ferroelectric and Piezoelectric Materials · Dielectric materials and actuators

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (37)

Show source-provided references
1. Improving the hot corrosion resistance of plasma sprayed ceria-yttria stabilized zirconia thermal barrier coatings by laser surface treatment10.1016/j.matdes.2013.12.075 ↗
2. Microstructure and mechanical properties of ZTA/BN machinable ceramics fabricated by reactive hot pressing10.1016/j.jeurceramsoc.2014.09.002 ↗
3. Effect of Al2O3 particle size on preparation and properties of ZTA ceramics formed by gelcasting10.1016/j.ceramint.2013.10.111 ↗
4. In situ study on microwave sintering of ZTA ceramic: effect of ZrO2 content on densification, hardness, and toughness10.1111/jace.14658 ↗
5. Microstructural evolution and thermal stress relaxation of Al2O3/1Cr18Ni9Ti brazed joints with nickel foam10.1016/j.vacuum.2017.10.030 ↗
6. Reactive wetting and interfacial characterization of ZrO2 by SnAgCu-Ti alloy10.1016/j.ceramint.2018.12.163 ↗
7. Interfacial characterization of silicon nitride/silicon nitride joints brazed using Cu-base active metal interlayers10.1016/j.ceramint.2011.11.050 ↗
8. Microstructure evolution of Si3N4/Si3N4 joint brazed with Ag-Cu-Ti+SiCp composite filler10.1016/j.ceramint.2010.02.010 ↗
9. Microstructure and mechanical properties of Si3N4/42CrMo joints brazed with TiNp modified active filler10.1016/j.ceramint.2013.12.008 ↗
10. Microstructural evolution and characterisation of interfacial phases in Al2O3/Ag–Cu–Ti/Al2O3 braze joints10.1016/j.actamat.2015.05.048 ↗
11. Interfacial reactions between sapphire and Ag-Cu-Ti-based active braze alloys10.1016/j.actamat.2015.11.019 ↗
12. Effect of Cr on the wetting in Cu/graphite system10.1016/j.apsusc.2011.02.060 ↗
13. Wetting and interfacial reactivity in Ag–Zr/sintered AlN system10.1016/S1359-6462(02)00449-9 ↗
14. Liquid metal wettability and advanced ceramic brazing10.1016/j.jeurceramsoc.2007.07.021 ↗
15. Joining of Si3N4 to Si3N4 using a AuPd(Co, Ni)-V filler alloy and the interfacial reactions10.1016/j.ceramint.2013.08.069 ↗
16. Microstructure, residual stress and mechanical properties of Al2O3/Nb joints vacuum-brazed with two Ag-based active fillers10.1016/j.vacuum.2018.09.028 ↗
17. Interfacial microstructure and mechanical property of ZrC-SiC ceramic and Ti6Al4V joint brazed with AgCuTi alloy10.1016/j.jeurceramsoc.2017.02.056 ↗
18. Graphene nanoplatelets reinforced AgCuTi composite filler for brazing SiC ceramic10.1016/j.jeurceramsoc.2018.11.046 ↗
19. Microstructure of reaction layer and its effect on the joining strength of SiC/SiC joints brazed using Ag-Cu-In-Ti alloy10.1007/s40145-014-0095-z ↗
20. Characterization of silicon carbide joints fabricated using SiC particulate-reinforced Ag-Cu-Ti alloys10.1016/j.ceramint.2012.10.271 ↗
21. Wetting of AgCu-Ti filler on porous Si3N4 ceramic and brazing of the ceramic to TiAl alloy10.1016/j.ceramint.2017.11.212 ↗
22. Zirconia ceramic and Nb joints brazed with Mo-particle-reinforced Ag-Cu-Ti composite fillers: interfacial microstructure and formation mechanism10.1016/j.ceramint.2017.04.133 ↗
23. Interactions, joining and microstructure of Sn-Ti/ZrO2 system10.1016/j.jeurceramsoc.2018.12.010 ↗
24. Brazing of ZrO2 toughened Al2O3 to stainless steel10.1179/mst.1997.13.2.156 ↗
25. Brazing ZTA ceramic to TC4 alloy using the Cu foam as interlayer10.1016/j.vacuum.2018.05.038 ↗
26. Revealing the strengthening mechanism in Si3N4 ceramic joint by atomic force microscopy coupled with nanoindentation techniques10.1016/j.jeurceramsoc.2012.04.004 ↗
27. Enthalpy of formation in the Al-Ni-Ti system10.1007/s11669-009-9573-3 ↗
28. Reaction between titanium and zirconia powders during sintering at 1500 °C10.1111/j.1551-2916.2007.01708.x ↗
29. Doping behavior of Zr4+ ions in Zr4+-doped TiO2 nanoparticles10.1021/jp407662d ↗
30. Investigation of interaction of metal melts and zirconia10.1007/s10853-005-1928-5 ↗
31. Microstructure and strength of brazed joints of Ti3Al-base alloy with NiCrSiB10.1016/j.matchar.2004.06.005 ↗
32. Convergent-beam electron diffraction "fingerprinting" of M6X phases at brazed ceramic joints10.1016/0956-716X(91)90352-2 ↗
33. Brazing of alumina with Ti4Cu2O and Ti3Cu3O interlayers10.1016/S0167-577X(97)00098-0 ↗
34. First-principles investigations of the structural, anisotropic mechanical, thermodynamic and electronic properties of the AlNi2Ti compound10.3390/cryst8020093 ↗
35. The nickel-rich corner of the Ni-Al-Ti system10.1007/BF00544203 ↗
36. Microstructure evolution and bonding strength of the Al2O3/Al2O3 interface brazed via Ni-Ti intermetallic phases10.1016/j.jeurceramsoc.2019.11.066 ↗
37. Processing, microstructure and mechanical properties of vacuum-brazed Al2O3/Ti6Al4V joints10.1016/j.msea.2011.12.042 ↗